Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results 1 to 12 of 12 for “"crack length measurement"”

  1. An Experimental Investigation of Composite Sensors for Crack Length Measurement

    Structural defects such as cracks can cause catastrophic failure in engineering components or structures. There are many techniques to measure the crack growth in materials and are commercially available. In this thesis, bondable crack length measurement gages have been investigated and these gages …

    odu Repository record for An Experimental Investigation of Composite Sensors for Crack Length Measurement (opens in a new tab)

  2. Experimental crack length measurement under variable temperature using a thin film AC potential difference technique

    … drop (PD) method is developed for measuring crack length under combined thermal and mechanical loading. An insulated aluminum film deposited on the surface of center cracked 6061-T6 aluminum alloy test specimens provides a medium for the measurement of PD data used in calculating crack …

    manitoba Repository record for Experimental crack length measurement under variable temperature using a thin film AC potential difference technique (opens in a new tab)

  3. Electroless Nickel Plating and Spark Plasma Sintering of nano ZrO2 for Mechanical Property Enhancement

    … fracture toughness was calculated by indentation-crack-length measurement and three-point bend test of notched samples; flexural strength was measured by 3-point bend tests. The measured hardness is comparable to the results found in the literatures. The coated and uncoated zirconia show …

    wustl Repository record for Electroless Nickel Plating and Spark Plasma Sintering of nano ZrO2 for Mechanical Property Enhancement (opens in a new tab)

  4. Energy analysis of brittle fracture and its application to zirconium-oxide ceramics

    … of the strain energy release rate with the crack extension revealed that the subcritical crack growth in a CN specimen causes dependence of the measured fracture parameters on the experimental procedure (stressing rate, stiffness of the testing system, crack length). It appears that, as …

    mcmaster Repository record for Energy analysis of brittle fracture and its application to zirconium-oxide ceramics (opens in a new tab)

  5. Acoustic emission analysis for quality assessment of thermally sprayed coatings

    … Vickers indentation to assess the degree of cracking and hence the toughness of the coating. AE monitoring was also applied to an industrial process as a contribution to the possibility of quality assessment during the deposition process. AE data were acquired during indentation tests on …

    heriot-watt Repository record for Acoustic emission analysis for quality assessment of thermally sprayed coatings (opens in a new tab)

  6. An experimental method for developing J-R curves from load versus crack length records

    … from load versus displacement records without crack length measurement. This method uses a so-called LMN function to describe the plastic deformation curve, which gives an unique relationship between load, plastic displacement and crack length. It not only eliminates the need for crack length …

    ut-knoxville Repository record for An experimental method for developing J-R curves from load versus crack length records (opens in a new tab)

  7. Investigation of Mechanical Properties of Bulk and Additively Manufactured Ni-Mn-Ga Shape Memory Alloy using Nanoindentation and Microhardness Techniques

    … of model models based on Palmqvist and radial crack. There were three different models used based on radial crack length including, Laugier, Anstis and Niihara’s model, while there were two different models based on Palmqvist crack length suggested by Laugier and Niihara. Both crack length and …

    ohiolink Repository record for Investigation of Mechanical Properties of Bulk and Additively Manufactured Ni-Mn-Ga Shape Memory Alloy using Nanoindentation and Microhardness Techniques (opens in a new tab)

  8. On the Nature of Static and Cyclic Fracture Resistance of Ultra High Molecular Weight Polyethylenes Used in Total Joint Replacements

    … of a compliance based automated system for crack length measurement during fatigue crack propagation (FCP) tests was demonstrated for UHMWPE materials. The Standard compliance calibration coefficients were found to accurately predict the fatigue crack growth only in the low da/dN regime …

    ohiolink Repository record for On the Nature of Static and Cyclic Fracture Resistance of Ultra High Molecular Weight Polyethylenes Used in Total Joint Replacements (opens in a new tab)

  9. Fracture Toughness Testing with Notched Round Bars

    … and the single edge bend SE(B) specimen. The crack front in a planar specimen has a constraint condition which varies through the thickness from plane stress on the lateral surfaces to plane strain in the middle of the specimen. This change in constraint makes the geometry of planar specimens …

    utk-theses Repository record for Fracture Toughness Testing with Notched Round Bars (opens in a new tab)

  10. Optické měření délky trhliny s využitím metody DIC

    Diplomová práce se zabývá měřením délky trhliny pomocí digitální korelace obrazu. V teoretické části práce je představena metoda digitální korelace obrazu, problematika trhliny a také jsou představeny konvenční metody pro měření délky trhliny. V oblasti měření délky trhliny pomocí DIC v této chvíli …

    brno-tech Repository record for Optické měření délky trhliny s využitím metody DIC (opens in a new tab)

  11. Srovnání metod pro vyhodnocení délky trhliny s využitím digitální korelace obrazu

    Diplomová práce se zabývá měřením délky trhliny pomocí digitální korelace obrazu. V teoretické části práce je představena metoda digitální korelace obrazu, problematika trhliny a také jsou představeny konvenční metody pro měření délky trhliny. V oblasti měření délky trhliny pomocí DIC v této chvíli …

    brno-tech Repository record for Srovnání metod pro vyhodnocení délky trhliny s využitím digitální korelace obrazu (opens in a new tab)

  12. Vývoj metodiky pro stanovení délky únavové trhliny pomocí korelace digitálních obrazů

    Zastavování únavových zkoušek kvůli vizuálním odečtům je pracné a je v rozporu s nepřetržitým snímáním doporučovaným normami pro stanovení rychlosti růstu únavových trhlin. Měření délky únavové trhliny v průběhu zkoušky navíc snižuje zátěž obsluhy a umožňuje automatizaci. Tato práce rozvíjí …

    brno-tech Repository record for Vývoj metodiky pro stanovení délky únavové trhliny pomocí korelace digitálních obrazů (opens in a new tab)