  1. The Effect of Testing Direction on DHC Growth Rate Using Zr-2.5Nb Plate

    Delayed Hydride Cracking (DHC) is a fracture mechanism responsible for several failures of Zr-2.5Nb CANDU pressure tubes. The crack velocity is directionally dependant. Disk-shaped hydrides preferentially form on certain crystallographic planes that are hypothesized to be responsible for the …

    carleton Repository record for The Effect of Testing Direction on DHC Growth Rate Using Zr-2.5Nb Plate (opens in a new tab)

  2. The fracture mechanics of lithium disilicate glass and glass-ceramics

    … under stress. Hence the study of subcritical crack growth is important in predicting the life expectancy of a material when it is subjected to a stress. Subcritical crack growth of glass and glass-ceramics, at room temperature and in two different environments (toluene and water) was studied. …

    ubc Repository record for The fracture mechanics of lithium disilicate glass and glass-ceramics (opens in a new tab)

  3. Time-Dependent Crack Growth in Brittle Rocks and Field Applications to Geologic Hazards

    … this research is to evaluate the time-dependent crack growth in rocks using lab tests and numerical modeling and its application to geologic hazard problems. This research utilized Coconino sandstone and Columbia granite as the study materials and produced the subcritical crack growth parameters …

    arizona-thes Repository record for Time-Dependent Crack Growth in Brittle Rocks and Field Applications to Geologic Hazards (opens in a new tab)

  4. Magnetic and Elastic Interactions at Cracks and Interfaces in Ferromagnetic Materials

    … the interaction of a magnetic field with several crack geometries. The influence of crack velocity and a realistic (nonlinear) magnetic susceptibility were included into a model of this type for the first time and shown to introduce unexpected trends in the magneto-elastic stress intensity. …

    vt Repository record for Magnetic and Elastic Interactions at Cracks and Interfaces in Ferromagnetic Materials (opens in a new tab)

  5. Investigation of the dynamic fracture behavior of concrete

    … erroneous results, which was detected by the crack gauge employed in this study. When using the analog filter, the event time increased and the peak signal value decreased considerably, relative to the unfiltered or true values. The inertial loads associated with the specimen during the impact …

    ubc Repository record for Investigation of the dynamic fracture behavior of concrete (opens in a new tab)

  6. Viscoelastic fracture characterization of a solid propellant.

    … studies were conducted on a propagating crack in a viscoelastic material. By applying an extension of the "correspondence principle" the stress and displacement at the crack tip were found as functions of the crack tip stress intensity factor. An energy balance was made for the specimen …

    nps Repository record for Viscoelastic fracture characterization of a solid propellant. (opens in a new tab)

  7. Evaluation of the fracture postulate for viscoelastic materials.

    … the fracture postulate which states that crack velocity is a unique function of stress intensity factor. To do this, fracture characterization tests were conducted for constant load, constant displacement, and constant displacement rate histories. A cyclic study, a more sophisticated …

    nps Repository record for Evaluation of the fracture postulate for viscoelastic materials. (opens in a new tab)

  8. A study of the stress corrosion cracking of mild steel in alkaline and alkaline sulphide solutions

    The stress corrosion cracking (SCC) of an At ST C-1018 mild steel was investigated in three solutions, composed of 12.5 mol/kg NaOH, 3.35 mol/kg NaOH and 2.5 mol/kg NaOH + 0.42 mol/kg Na₂S, respectively. The potential of maximum susceptibility to SCC of steel in the latter two solutions was …

    ubc Repository record for A study of the stress corrosion cracking of mild steel in alkaline and alkaline sulphide solutions (opens in a new tab)

  9. Simulations of Ductile Fracture in Pipeline Steels Under Quasi-Static and Dynamic Loading Conditions

    … A relation between the cohesive energy and crack velocity is developed to provide insight into the effect of loading rate on the CZM based on a constant CTOA model. Lastly, this study provided data which supports the notion that the upswing in the two curve method (TCM) is due to the effect …

    carleton Repository record for Simulations of Ductile Fracture in Pipeline Steels Under Quasi-Static and Dynamic Loading Conditions (opens in a new tab)

  10. Caustic cracking susceptibility of SAE A 516 Gr. 70 steel in alkaline sulphide solutions

    The stress corrosion cracking (SCC) of A516 Gr. 70 steel was investigated in three solution composed of 3.35 m NaOH, 2.5 m NaOH + 0.42 m Na₂S, and 3.35 m NaOH + 0.02 m Na₂S. The electrochemical potential for maximum susceptibility was assessed by the slow strain rate testing technique (SSRT), and …

    ubc Repository record for Caustic cracking susceptibility of SAE A 516 Gr. 70 steel in alkaline sulphide solutions (opens in a new tab)

  11. Fracture Toughness in Rate-Dependent Solids Based on Viod Growth and Coalescence Mechanism

    … widely used in many engineering applications. Crack growth and delamination are frequently observed failure models. The viscoelastic characteristic of polymeric materials can give rise to rate dependent crack growth; time dependent inelastic deformation of metals and alloys at high temperature …

    nus Repository record for Fracture Toughness in Rate-Dependent Solids Based on Viod Growth and Coalescence Mechanism (opens in a new tab)

  12. Evaluación experimental y modelado de propagación de grietas en un acero de fase dual

    … on properties like fracture toughness or the crack propagation resistance haven´t had a large develop. Thus is convenient continue studying these properties, which allow estimate the final limit of use of a piece through structural integrity analysis. This document presents the study of …

    un-colombia Repository record for Evaluación experimental y modelado de propagación de grietas en un acero de fase dual (opens in a new tab)

  13. Manufacturing Processes Leading to Improved High pH SCC Resistance in Pipes

    Stress Corrosion Cracking (SCC) is a damaging form of environmental corrosion found in pipeline steels that forms in the presence of a high pH environment. SCC forms at the surface of gas pipes under damaged coatings and propagates towards the inner wall of the pipe until a critical depth is …

    adelaide Repository record for Manufacturing Processes Leading to Improved High pH SCC Resistance in Pipes (opens in a new tab)

  14. The Effect of Including Pressure within Cracks on Failure Times of Cylinders Subjected to Internal Air Blast Loading

    The importance of internal crack pressure on the extent of crack propagation is studied using both numerical and experimental results. Experimental data were obtained from shock tube testing of internally pressurized quasi-brittle hollow cylinders loaded to failure. Half of the samples were tested …

    unm Repository record for The Effect of Including Pressure within Cracks on Failure Times of Cylinders Subjected to Internal Air Blast Loading (opens in a new tab)

  15. Fatigue crack growth in polycrystalline alumina at high temperatures

    High temperature crack growth behavior in a commercial and a hot-pressed polycrystalline Al$\sb2$O$\sb3$ was examined under monotonic tensile loading (static fatigue) and under Mode-I tension-tension cyclic loading (cyclic fatigue). The investigation of fatigue crack growth in polycrystalline …

    uiuc Repository record for Fatigue crack growth in polycrystalline alumina at high temperatures (opens in a new tab)

  16. Static fatigue of graphite

    Subcritical crack growth has been studied in two different grades of a fine-grained isotropic graphite and in pyrolytic graphite. The double torsion technique was used. Room temperature tests revealed a stress intensity-crack velocity behaviour similar to the third stage of crack growth in …

    ubc Repository record for Static fatigue of graphite (opens in a new tab)

  17. Magneto-Elastic Interactions in a Cracked Ferromagnetic Body

    … state of ferromagnetic plane with a moving crack has been investigated in this study. The model considers a soft magnetic ferroelastic body and incorporates a realistic (nonlinear) susceptibility. A moving crack is present in the body and is propagating in a direction perpendicular to the …

    vt Repository record for Magneto-Elastic Interactions in a Cracked Ferromagnetic Body (opens in a new tab)

  18. From Stress Corrosion to Catastrophic Fracture Mechanisms in Molecular Dynamics Models of Brittle Materials

    … going<br/>from the lowest possible velocity for a crack growing in subcritical loading<br/>conditions, to the highest velocity computed for very cold cracks. The<br/>study has been carried out in two prototypical models of brittle fracture:<br/>silicon and amorphous silica. Aiming to …

    kings Repository record for From Stress Corrosion to Catastrophic Fracture Mechanisms in Molecular Dynamics Models of Brittle Materials (opens in a new tab)

  19. Properties of concrete subjected to explosively generated impact and impulse loading.

    … electrical resistance strain gauges, crack velocity detection devices and a projectile velocity measurement system. Other measurements of post test damage have utilised stereoscopic photography, coloured particles of soil in the foundations of the concrete slabs and a scanning electron …

    whiterose Repository record for Properties of concrete subjected to explosively generated impact and impulse loading. (opens in a new tab)