Global ETD Search
Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.
Results 1 to 9 of 9 for “"cracking propensity"”
-
Assessing the autogenous shrinkage cracking propensity of concrete by means of the restrained ring test
… from very early age. The resultant risk of cracking presently cannot be adequately investigated. Parameters that are particularly difficult to capture experimentally are the concrete temperature and the viscoelasticity. The primary objective of this work was to assess as precise as possible …
-
Evaluation of cracking potential of superpave mixtures with high reclaimed asphalt pavement content
… mixtures that are susceptible to premature cracking. In this research, laboratory-produced Superpave HMA mixtures containing increased percentages (20, 30, and 40%) of RAP materials from three RAP sources (Shilling Construction Co., Konza Co., and the Kansas Department of Transportation’s …
-
AN INVESTIGATION OF DISTORTION-INDUCED FATIGUE CRACKS IN STEEL HIGHWAY BRIDGES: FROM CRACK DETECTION TO FATIGUE RETROFIT
Distortion-induced fatigue (DIF) cracking is the primary maintenance and structural safety concern in steel bridges built before the 1980s in the United States, requiring frequent inspections and costly repairs. Human visual inspections to characterize fatigue cracks have many drawbacks, including …
-
Minimum virgin binder limits in recycled Superpave (SR) mixes in Kansas
… susceptibility, rutting resistance, and fatigue cracking propensity using modified Lottman, Hamburg Wheel Tracking Device, flow number, Dynamic Modulus, and S-VECD direct tension fatigue tests. Results confirmed the effect of NMAS and material source on mixture performance. For SR-9.5A, the …
-
Evaluation of cracking resistance of Superpave mixtures in Kansas
… drier mixes that are often susceptible to early cracking. In this study, cracking resistance of Superpave mixtures with varying asphalt and RAP contents were investigated. HMA specimens were prepared based on Superpave mix design criteria for 12.5-mm (1/2-inch) nominal maximum aggregate size …
-
EFFECT OF FLUSHING PRESSURE ON ELECTRO-DISCHARGE MACHINING AND RESULTANT SURFACE CHARACTERISTICS
… performance, recast layer morphology and cracking propensity. AISI 01 tool steel and a high-energy machining condition were used in the present work. The flushing pressure was varied from 10 to 110 kPa in steps of 10kPa. The results show the flushing pressure effort can be divided into …
-
Pragmatic models for predicting material properties in laser powder bed fusion
… model was developed to predict solidification cracking in crack-susceptible aluminium alloys. This model incorporated calibrated melt pool profiles to accurately represent melt pool geometry and employed normal vector intersections to estimate misorientation angles. Coupling this with a …
-
Solid-liquid interdiffusion bonding for MEMS device integration
… of voiding level in the Cu3Sn phase on the cracking propensity is reported, and the voiding level is observed to link to copper electroplating bath condition. Zinc-aluminum based alloys are examined as a cost-effective material system for metal bonding. Interfacial reactions between these …
-
Fabrication of Hard-to-Process Ni-Based Superalloy Thin-Wall Parts Made by Laser Powder Bed Fusion
… However, build challenges, such as micro-cracking and in-process failure, inherent in LPBF, limit processability and affect final part quality. Micro-cracking is especially important for high γ’ Ni-based superalloys, which are used in serpentine-shaped components such as fuel nozzles and …