Global ETD Search
Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.
Results
Showing 1 to 5 of 5 for “"cyclic deformation response"”.
-
Investigation of Cyclic Deformation and Fatigue of Polycrystalline Cu under Pure Compression Cyclic Loading Conditions
… very limited or non-existent knowledge pool on cyclic deformation response under pure compressive fatigue condition. Our recent work verified that fatigue cracks may nucleate from stress concentration sites under pure compression fatigue, but whether or not a form of stress concentration is …
-
Cyclic Deformation Behaviour and the Related Micro-mechanisms of F.C.C. Metals Processed by Accumulative Roll-bonding
… metals, however there are few, if any, on the cyclic deformation behavior of such metals. The primary objective of this study is to investigate the cyclic deformation behaviour and the related micro-mechanisms of ARBed metals from a fundamental perspective. To achieve this, the microstructure …
-
ACTUATION FATIGUE PROPERTIES OF NITI-BASED HIGH TEMPERATURE SHAPE MEMORY ALLOYS
… the matrix by acting as barriers against plastic deformation [2-6].The increase in strength due to precipitation also permits reversible martensitic transformation at higher stress levels [2, 3, 7, 8].Furthermore, nano-precipitation in Ni-rich NiTiHf and NiTiZr alloys allows for precise control of …
-
Influence of notches due to laser beam cutting on the fatigue behavior of plate-like shaped parts made of metastable austenitic stainless steel
… effect sensitivity for different amounts of deformation-induced α'-martensite induced before cyclic tests was evaluated using a specific notch geometry. Furthermore, based on the fact that high frequency testing is performed in the present investigation, the likely influences of test …
-
Únavové charakteristiky hořčíkové slitiny AZ31 po korozní degradaci
Předmětem této diplomové práce je hodnocení cyklické odezvy a únavového chování hořčíkové slitiny AZ31 v základním stavu a po korozní degradaci v mlze neutrálního 5% roztoku NaCl po dobu 480 a 1000 hodin. V práci je hodnocena mikrostruktura, základní mechanické vlastnosti a únavové chování …