Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results 1 to 7 of 7 for “"cyclic nanoindentation"”

  1. Deformation mechanisms of metastable stainless steels accessed locally by monotonic and cyclic nanoindentation

    … individuels par des tests mécaniques de nanoindentation monotoniques et cycliques. Les courbes correspondantes au chargement-déchargement révèlent des informations détaillées sur les propriétés mécaniques sous-jacentes qui pourraient être liées à une étude complète de la structure de …

    star-france Repository record for Deformation mechanisms of metastable stainless steels accessed locally by monotonic and cyclic nanoindentation (opens in a new tab)

  2. Deformation mechanisms of metastable stainless steels accessed locally by monotonic and cyclic nanoindentation

    … of individual austenite grains via monotonic and cyclic nanoindentation. The corresponding loading–unloading curves have given extensive information about underlying mechanical properties, which could be related to an exhaustive reconstruction of the deformation substructure, both in surface and …

    barcelona Repository record for Deformation mechanisms of metastable stainless steels accessed locally by monotonic and cyclic nanoindentation (opens in a new tab)

  3. Numerical analysis of plastic deformation in metal-ceramic nanolayers during cyclic indentation

    … finite element method. Attention is devoted to cyclic response under fixed maximum and minimum loads, with the primary objective of examining the evolving plastic deformation in the ductile metal constrained by the hard ceramic layers. An axisymmetric model consisting of alternating aluminum …

    unm Repository record for Numerical analysis of plastic deformation in metal-ceramic nanolayers during cyclic indentation (opens in a new tab)

  4. In-situ Micro and Nanomechanical Characterization and Ultrasonic Machining of Zirconia Ceramics

    … mechanics in dental abrasive machining. In-situ nanoindentation tests combined with an in-situ technique were also conducted on pre-sintered and sintered zirconia materials. The nanoindentation revealed quasi-brittle behavior for both zirconia materials but at the microstructural level different …

    adelaide Repository record for In-situ Micro and Nanomechanical Characterization and Ultrasonic Machining of Zirconia Ceramics (opens in a new tab)

  5. Molecular Dynamics Study of Radiation and Creep Response of Nanotwinned FCC Metals

    … damage. We also perform atomistic simulations of cyclic nanoindentation to complement experimental studies of cyclic nano- and micro-indentation, along with indentation creep, on nanotwinned Cu and Ag. Taken together, the studies provide evidence that nanotwinned fcc structures are more stable …

    houston Repository record for Molecular Dynamics Study of Radiation and Creep Response of Nanotwinned FCC Metals (opens in a new tab)

  6. Πειραματική και θεωρητική μελέτη μηχανικών ιδιοτήτων και φαινομένων μεγέθους σε νανοδομές και λεπτά υμένια

    … the samples were studied by nanoindentation experiments with a wide range of loads between 1 to 500mN in order to be able to calculate the nano-mechanical properties (elastic modulus and hardness) of the two different types of systems. The results for the two different types …

    greece Repository record for Πειραματική και θεωρητική μελέτη μηχανικών ιδιοτήτων και φαινομένων μεγέθους σε νανοδομές και λεπτά υμένια (opens in a new tab)

  7. Studium povrchů tenkovrstvých materiálů

    Disertační práce se zabývá studiem povrchových vlastností jedno a vícevrstvých filmů deponovaných z vinyltriethoxysilanových a tetravinylsilanových monomerů. Zabývá se také charakterizací adheze jednovrstvých filmů z tetravinylsilanu. Plazmaticky polymerizované tenké vrstvy byly připraveny na …

    brno-tech Repository record for Studium povrchů tenkovrstvých materiálů (opens in a new tab)