  1. Damp-Heat-Induced Degradation in TOPCon and Heterojunction Solar Cells: Mechanisms, Materials, and Mitigation

    … In particular, their performance stability under damp-heat (DH) conditions and susceptibility to manufacturing-induced contamination pose significant concerns, as both factors can deteriorate interfacial passivation quality and metallisation durability. This thesis investigates the degradation …

    unsw Repository record for Damp-Heat-Induced Degradation in TOPCon and Heterojunction Solar Cells: Mechanisms, Materials, and Mitigation (opens in a new tab)

  2. Degradation of Photovoltaic Packaging Materials and Power Output of Photovoltaic Systems: Scaling up Materials Science with Data Science

    … by humidity and UV. This testing included damp heat (DH) exposure (85 C, 85 % relative humidity) and QUV exposure (1.55 W/m<sup>2</sup> at 340 nm, black panel temperature 70 C). In DH testing, yellowing induced by antioxidant hydrolysis and additive migration can be observed. Hydrolysis is …

    ohiolink Repository record for Degradation of Photovoltaic Packaging Materials and Power Output of Photovoltaic Systems: Scaling up Materials Science with Data Science (opens in a new tab)

  3. Evaluation of the Effect of Backsheet Properties on PV Encapsulant Degradation under Ultraviolet-Damp-Heat Conditions

    … in accelerated aging tests (up to 4000 h for Damp-Heat (DH) and up to 480 kWh/m² for Ultraviolet (UV) and UV-DH combined). Firstly, by using samples with different backsheets, the effects of different material combinations on the EVA degradation mechanisms (chemical changes) were investigated. …

    epfl Repository record for Evaluation of the Effect of Backsheet Properties on PV Encapsulant Degradation under Ultraviolet-Damp-Heat Conditions (opens in a new tab)

  4. Investigation and Mitigation of Moisture- and Potential-Induced Degradation Mechanisms of Silicon Heterojunction Solar Cells and Modules

    … is sensitive to three factors: moisture (i.e. damp heat (DH)-induced degradation), high voltages (i.e. potential-induced degradation (PID)) and UV exposure. We nonetheless established that with the right module configuration, SHJ solar cells can reach service lifetimes of 35+ years. Next, we …

    epfl Repository record for Investigation and Mitigation of Moisture- and Potential-Induced Degradation Mechanisms of Silicon Heterojunction Solar Cells and Modules (opens in a new tab)