Global ETD Search
Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.
Results 1 to 20 of 43 for “"damp-heat"”
-
Stability of silicon surface passivation under damp heat and light soaking
… stability of silicon surface passivation under damp heat and light soaking as well as potential mechanisms behind the resulting degradation. Particularly, the influence of the spatial atomic layer deposition (SALD) mode, the passivation layer thickness, the properties of the interface between …
-
Investigating Damp-Heat Degradation and Mitigation Strategies for Industrial N-Type Silicon Solar Cells
… these solar modules and cells, especially under damp-heat conditions. Furthermore, the industry urgently requires accelerated testing methods to cost-effectively evaluate different process and cell technology routes. This thesis aims to elucidate the potential degradation mechanisms of TOPCon and …
-
Damp-Heat-Induced Degradation in TOPCon and Heterojunction Solar Cells: Mechanisms, Materials, and Mitigation
… In particular, their performance stability under damp-heat (DH) conditions and susceptibility to manufacturing-induced contamination pose significant concerns, as both factors can deteriorate interfacial passivation quality and metallisation durability. This thesis investigates the degradation …
-
Evaluation of the Effect of Backsheet Properties on PV Encapsulant Degradation under Ultraviolet-Damp-Heat Conditions
… in accelerated aging tests (up to 4000 h for Damp-Heat (DH) and up to 480 kWh/m² for Ultraviolet (UV) and UV-DH combined). Firstly, by using samples with different backsheets, the effects of different material combinations on the EVA degradation mechanisms (chemical changes) were investigated. …
-
Defect spectroscopy on Cu(In,Ga)(S,Se) 2 -based heterojunction solar cells: role of the damp-heat treatment
… test cells are reduced after prolonged damp-heat treatment in the laboratory, leading to a reduced energy conversion efficiency. We subject non-encapsulated test cells to damp-heat exposure at 85C ambient temperature and 85% relative humidity for various time periods (6h-438h). We apply …
-
MATERIAL PROPERTY STUDY ON DYE SENSITIZED SOLAR CELLS AND CU(GA,IN)SE2 SOLAR CELLS
… 3) We studied the degradation mechanism using damp heat based on ZnO and Al:ZnO. We found that the Al dopant would enhance the moisture capture ability in ZnO, causing degradation under damp heat and annealing treatment.4) we have compared the differences between Zn1-xMgxO and Al: Zn1-xMgxO and …
-
Identification and Mitigation of Degradation Mechanisms Induced by Heat and Light in NiOx-based Perovskite Solar Cells
… solar cells demands rigorous testing, including damp heat and light soaking tests. However, PSCs are susceptible to various degradation mechanisms when exposed to elevated temperatures, light, or humidity. This thesis aims to investigate these degradation mechanisms and propose some mitigation …
-
Modeling Degradation of Photovoltaic Modules using Machine Learning of Electroluminescent Images
… been studied and quantified for five brands of damp-heat exposed commercial modules. Using supervised machine learning, three degradation features were classified to greater than 95% accuracy by training a scalable classification pipeline which can now be used by PV researchers for unbiased, …
-
Investigation of the Performance and Stability of TOPCon Solar Cells from a Metallization Perspective
… metallization-related reliability issue is damp-heat degradation. Accelerated cell-level damp-heat testing shows that contaminants could penetrate through the porous screen-printed contacts, leading to rapid deterioration of the metal-Si interface. To mitigate this degradation, copper …
-
Lifetime and Degradation Science of Polymeric Encapsulant in Photovoltaic Systems: Investigating the Role of Ethylene Vinyl Acetate in Photovoltaic Module Performance Loss with Semi-gSEM Analytics
… the degradation of mini-module samples under damp heat accelerated stress conditions. Mini-module samples featured two construction geometries that differed in the thicknesses of screen-printed silver conductive lines (SP-Ag) to assess the impact of gridline size on damp heat induced …
-
New materials for chalcogenide based solar cells
… for replacing CdS and ZnO films to improve the damp-heat stability of the solar cells and for minimizing the use of Cd. Specifically, I demonstrate a new CIGS solar cell with better damp heat stability wherein the ZnO layer is replaced with SnO2. The efficiency of solar cells made with SnO2 …
-
Long-term stability of organic solar cells
… temperature, continuous illumination, UV stress, damp heat and outdoor exposure. In the second part, detailed investigations of degradation mechanisms under different aging conditions (mainly under UV-stress and damp heat) and strategies how to minimize the degradation are presented.<br><br>A …
-
Usage of Highly Accelerated Stress Test (HAST) in Solar Module Ageing Procedures
… are established. The concept is to carry out the Damp Heat test and the Highly Accelerated Stress Test in order to accelerate the time of testing for solar module production. The choice of materials fell on four types of mini modules to be tested, three with standard embedding materials and one …
-
Degradation of Photovoltaic Packaging Materials and Power Output of Photovoltaic Systems: Scaling up Materials Science with Data Science
… by humidity and UV. This testing included damp heat (DH) exposure (85 C, 85 % relative humidity) and QUV exposure (1.55 W/m<sup>2</sup> at 340 nm, black panel temperature 70 C). In DH testing, yellowing induced by antioxidant hydrolysis and additive migration can be observed. Hydrolysis is …
-
Characterization of encapsulant and edge seal materials for flexible solar cell packaging
… accomplished using ultra-violet, thermal, and damp heat exposure to simulate actual weathering conditions. The impact of these aging conditions on material adhesion was evaluated and analyzed.
-
Degradation of Bifacial & Monofacial, Double Glass & Glass-backsheet, Photovoltaic Modules with Multiple Packaging Combinations
… indoor accelerated exposures included modified damp heat (80 ℃, 85% relative humidity) and modified damp heat with full-spectrum light, for up to 2,520 hours. The EVA+GB modules with opaque rear encapsulant exhibited a significantly greater power loss, and the dominant degradation mechanism was …
-
Data-Driven Degradation Study of Interfacial Adhesion Under Accelerated Aging: Adhesively Bonded Cu and Polyimide in Flexible Printed Circuit Boards (PCBs)
… and copper, were subjected to 1000 h of damp heat exposure (85 ◦C/85 %RH). The degradation pathway was modeled in a < Stressor|Mechanism|Response > framework using network structural equation modeling (netSEM). netSEM degradation modeling was used to visualize and predict the extent of …
-
Degradation of Transparent Conductive Oxides: Mechanistic Insights and Interfacial Engineering
… environmental stressors such as irradiance, heat and humidity. Electrical and optical properties and surface energies were measured. Yellowness, haze, water contact angle and resistivity of different materials trended differently with exposure time and type, indicating different degradation …
-
Encapsulation and design of scalable packaging materials for thin film perovskite solar cell applications
… and their adhesion profiles were studied upon damp-heat exposure on these samples. Second, thorough XPS analysis was conducted on the delaminated PET surface from the PET/EVA/PET encapsulation architecture upon the UV, thermal, and moisture aging to understand the degradation mechanism at the …
-
The role of Encapsulants in the long-term performance of advanced Crystalline Silicon Glass-Glass PV modules
… and Silicon Heterojunction (SHJ)) exposed to damp-heat, where we highlight the good stability of the EVA, and the sensitivity to moisture of the SHJ solar cells. 2. We propose a detailed microscopical model explaining the problematic of the SHJ to water. In reality, the presence of moisture …