Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results

Showing 1 to 20 of 52 for “"debinding"”.

  1. Failure analysis of green ceramic bodies during thermal debinding

    In industry, thermal debinding is the traditional mode of binder removal from multilayer ceramic capacitors (MLCs). Binder removal from ceramics takes as long as 50-150 h, thereby contributing significantly to the manufacturing costs and also controlling the production rate. Increasing energy costs …

    missouri Repository record for Failure analysis of green ceramic bodies during thermal debinding (opens in a new tab)

  2. Magnesium Polyolefin Interactions during Thermal Debinding in the MIMProcess of Magnesium

    … the mechanisms taking place during the thermal debinding of PE and PP based polymers in combination with magnesium powder is developed by using literature and different experimental setups.

    cau-kiel Repository record for Magnesium Polyolefin Interactions during Thermal Debinding in the MIMProcess of Magnesium (opens in a new tab)

  3. An Experimental Investigation of Debinding and Sintering Parameters for Copper Powder Material Extrusion

    This study investigated the debinding and sintering parameter effects using Powder Metal Extrusion (PME). Specifically, a Polylactic Acid (PLA) - Copper filament was used with a traditional Fused Filament Fabrication (FFF) printer to produce parts consisting of copper particles and a PLA binder. …

    tamu Repository record for An Experimental Investigation of Debinding and Sintering Parameters for Copper Powder Material Extrusion (opens in a new tab) Embargoed until 2026-12-01

  4. DEVELOPMENT AND TESTING OF ADDITIVELY MANUFACTURED COPPER MIXTURES FOR WARHEAD APPLICATIONS

    … how Cu particle morphology, binder ratios, debinding conditions, and sintering parameters affect densification and microstructural evolution. More than one hundred pressed samples were fabricated using different formulations and thermal cycles. Thermogravimetric analysis (TGA) was used to …

    nps Repository record for DEVELOPMENT AND TESTING OF ADDITIVELY MANUFACTURED COPPER MIXTURES FOR WARHEAD APPLICATIONS (opens in a new tab)

  5. Producing near-net shape titanium alloy parts by metal injection moulding

    … injection moulding, removing the binder (debinding) and sintering. The binder affects feedstock rheology, allowing the required shape to be moulded. It then needs to be removed so the object can be sintered to consolidate into a near-net shaped part. As MIM has many advantages, including …

    waikato-masters Repository record for Producing near-net shape titanium alloy parts by metal injection moulding (opens in a new tab) Download file for Producing near-net shape titanium alloy parts by metal injection moulding (opens in a new tab)

  6. Fabrication and Characterization of Miniaturized Components Based on Extruded Ceramic-Filled Polymer Blends

    … can be sintered to full density. A two-step debinding is introduced to eliminate debinding defects that are commonly observed in thermal debinding (TD). Cracking is a major issue due to a lack of pore spaces for outgassing of pyrolysis products in traditional TD. In two-step debinding, a …

    lsu-thes Repository record for Fabrication and Characterization of Miniaturized Components Based on Extruded Ceramic-Filled Polymer Blends (opens in a new tab)

  7. The Formulation of Titanium - based Metal Feedstocks and the Fabrication of Parts using the Powder Injection Moulding Process

    … based metal powder feedstock followed by a debinding process and subsequent sintering. The fabrication process in its entirety was investigated in four distinct steps. Feedstock formulation involved combining the metal powders with various carrier components. Injection moulding enabled the …

    waikato-masters Repository record for The Formulation of Titanium - based Metal Feedstocks and the Fabrication of Parts using the Powder Injection Moulding Process (opens in a new tab) Download file for The Formulation of Titanium - based Metal Feedstocks and the Fabrication of Parts using the Powder Injection Moulding Process (opens in a new tab)

  8. Metal Injection Moulding of Inconel 718 using a Water Soluble Binder System

    … calorimetry (DSC) characteristics as well as debinding behaviour were all carried out. Parts were sintered and heat treated with density and dimensional measurements taken throughout, in order to identify the effect of PEG molecular weight on the different processing steps. Metallography and …

    whiterose Download PDF for Metal Injection Moulding of Inconel 718 using a Water Soluble Binder System (opens in a new tab)

  9. Development of PEG based binders for metal injection moulding with special focus on titanium

    … easily be contaminated by the binders during the debinding and sintering stages. The lack of industrial confidence in the Ti-MIM is likely due to the limited understanding of binder chemistry. As the same binder systems are often used for different powders in MIM, a poor binder may still lead to …

    auckland-ms Repository record for Development of PEG based binders for metal injection moulding with special focus on titanium (opens in a new tab)

  10. Compounding and processing of a water soluble binder for powder injection moulding

    … moulding (PIM) process. Consequently, water debinding was a requirement once it is a lower environmental impact technology, economically attractive and less hazardous than the conventional catalytic, thermal or solvent debinding. Furthermore, the understanding of the influence of the binder …

    minho-thes Repository record for Compounding and processing of a water soluble binder for powder injection moulding (opens in a new tab)

  11. Study of rheological and sintering behavior of iron-based feedstock used in low-pressure metal injection molding

    … %) of this powder. Furthermore, to design the debinding cycle (i.e., wick thermal debinding) and define the presintering temperature (i.e., 600ºC), the same powder with optimal binder formulation (i.e., 1 vol. % stearic acid as a surfactant, 2 vol. % ethylene-vinyl acetate as a thickening …

    ets-quebec Download PDF for Study of rheological and sintering behavior of iron-based feedstock used in low-pressure metal injection molding (opens in a new tab)

  12. Material development and process optimisation for Digital Light Processing of translucent alumina

    … were employed to determine the optimal thermal debinding parameters. Upon examination of various debinding regimes, the debinding heat rate of 0.2 °C/min and increased dwell times contributed to reducing defects and enhancing densification. Samples exhibiting a relative density higher than 99.0% …

    birmingham Download PDF for Material development and process optimisation for Digital Light Processing of translucent alumina (opens in a new tab)

  13. Characterization and Optimization of Process Parameters for Controlling Extrudate Morphology and Laser-Matter Interactions in Metal Additive Manufacturing

    … content introduces the need for specialized debinding equipment, prolongs manufacturing time, and limits geometrical capabilities. A MEX framework was investigated to address these limitations. The framework involved (1) synthesis of a 316L stainless steel paste with just 3.2 vol% binder, (2) …

    tamu Repository record for Characterization and Optimization of Process Parameters for Controlling Extrudate Morphology and Laser-Matter Interactions in Metal Additive Manufacturing (opens in a new tab)

  14. Characterization and Optimization of Process Parameters for Controlling Extrudate Morphology and Laser-Matter Interactions in Metal Additive Manufacturing

    … content introduces the need for specialized debinding equipment, prolongs manufacturing time, and limits geometrical capabilities. A MEX framework was investigated to address these limitations. The framework involved (1) synthesis of a 316L stainless steel paste with just 3.2 vol% binder, (2) …

    tamu Repository record for Characterization and Optimization of Process Parameters for Controlling Extrudate Morphology and Laser-Matter Interactions in Metal Additive Manufacturing (opens in a new tab)

  15. Modelling material behavior for additively manufactured metals and polymers produced by fused filament fabrication

    … process involves three key stages: printing, debinding, and sintering. Despite its numerous benefits, MFFF confronts particular challenges during printing and sintering. Additionally, the layer-wise nature of the FFF process leads to anisotropic mechanical characteristics in printed parts. …

    uoit Repository record for Modelling material behavior for additively manufactured metals and polymers produced by fused filament fabrication (opens in a new tab)

  16. Additive manufacturing of aluminum alloy by metal fused filament fabrication (MF3).

    … green parts that were involved in a two-step debinding process combining solvent and thermal extraction of the polymer binder, then sintered in a partial vacuum. Resulting grain structure, sintered density, and mechanical properties will be characterized and compared to metal injection molded …

    louisville Repository record for Additive manufacturing of aluminum alloy by metal fused filament fabrication (MF3). (opens in a new tab)

  17. Material properties design using simulations and experiments for powder injection molding of lead zirconate titanate (PZT).

    … were performed to understand the defects after debinding and sintering. As the approach is to develop feedstock without measurement of feedstock properties, it is expected that the results from current work will help in reducing the number of experiments needed to obtain a defect free PIM …

    louisville Repository record for Material properties design using simulations and experiments for powder injection molding of lead zirconate titanate (PZT). (opens in a new tab)

  18. Material and process development for material extrusion metal additive manufacturing using recycled nickel

    … to achieve successful sintering. 3D-printing, debinding, and sintering were evaluated and optimized using rheology, thermal, and microstructural analysis leading to the production of parts with 91% relative density and 340 MPa tensile strength.

    uoit Repository record for Material and process development for material extrusion metal additive manufacturing using recycled nickel (opens in a new tab)

  19. PHYSICAL PROPERTY STUDIES OF FUSED DEPOSITION MODELING SHAPED CHARGE LINERS

    … this study variations in 3D printing, chemical debinding methods, and sintering to enable near theoretical maximum density to enable production of shaped charge liners in theater. Initial studies investigated 3D printed copper discs to optimize density using a commercial off-the-shelf (COTS) …

    nps Repository record for PHYSICAL PROPERTY STUDIES OF FUSED DEPOSITION MODELING SHAPED CHARGE LINERS (opens in a new tab)

Page 1 of 3