Development and Testing of a Debond-on-Demand Polyurethane Adhesive Through Induction Heating
… systems.<br/>The research begins by developing a debond-on-demand methodology using a hot melt adhesive (HMA) as a prototype controlled by induction heating. Followed by exploring various adhesive formulations, initially considering epoxy, and polyurethane systems. The epoxy uses a disulfide-based …
-
Debond Buckling of Woven E-glass/Balsa Sandwich Composites Exposed to One-sided Heating
… structures exposed to one-sided heating where a debond exists between the unexposed facesheet and core material. Sandwich composites of plain weave E-glass/epoxy facesheets and an end-grain balsa wood core manufactured using the Vacuum Assisted Resin Transfer Molding (VARTM) technique were the …
-
Changes in Occlusal Contact Area Following Orthodontic Treatment: At Time of Debond and Into Retention
… treatment characteristics, time since debond and retention types on occlusal contact changes were analyzed. Methods: Patients treated in the University of Washington Orthodontics clinic who obtained an intra-oral scan for the fabrication of new retainers were screened. Inclusion …
-
A randomised controlled trial to assess the pain associated with the debond of orthodontic fixed appliances
… fixed appliances, expectations of pain during debond and whether biting on a soft acrylic wafer during debond decreases the pain experienced. Method: Ethical approval was gained. Subjects were randomly allocated to the control or wafer group. A visual analogue scale (VAS) based questionnaire …
-
Effect of refrigerant spray on orthodontic composite resin-bracket debond strength and associated adhesive remnant index
… speed on orthodontic composite resin shear debond strength and Adhesive Remnant Index (ARI) after bond failure. Orthodontic brackets were bonded to forty paired extracted mandibular third molars. Pairs were divided into experimental and control groups, with and without refrigerant spray …
-
Large Deflection Effects on the ERR and Mode Partitioning of the Single and Double Cantilever Beam Sandwich Debond Configurations
… release rate and mode partitioning of face/core debonds for the Single and Double Cantilever Beam Sandwich Composite testing configurations, which are loaded with an applied shear force and/or bending moment. Studies on this topic have been done by employing geometrically linear theories (either …
-
The Application of Debond Length Measurements to Examine the Accuracy of Composite Interface Properties Derived From Fiber Pushout Testing
… 400$\sp\circ$C, indicating that the fibers were debonded by the fatigue load. The identification of progressive debonding in metal matrix composites is also discussed.
-
Nondestructive and destructive evaluation of FRP composite wrapped concrete cylinders with embedded debonds
… compressive strength and ductility. Presence of debonds between the FRP wrap and the underlying column surface inhibits the proper confinement of the column by the composite wrap.;The objectives of this research are: (a) to evaluate the feasibility of using Active Infrared Thermography for …
-
Shear bond strength of a single use self-etching primer used multiple times over 24 hours
… hours-, and 24 hours after opening. Samples were debonded with a universal testing machine after 24 hours to assess short term SBS, and after 2 months to assess bond maturation. Results: No statistically significant difference in SBS was found in the 24-hour debond group between the different time …
-
Finite Element Analysis of Probe Induced Delamination of a Thin Film at an Edge Interface
… crack closure method. Having assumed a circular debond as observed experimentally, energy release rates are determined by a step-wise approach around the circumference. The progression of debond is simulated in multiple analyses by altering the boundary conditions associated with increasing the …
-
COMPARISON OF SHEAR BOND STRENGTH OF NEW AND REBONDED SYMETRI™ CLEAR CERAMIC BRACKETS
… An additional aim was to see how a generic debond pliers compares to the Symetri™ Debonding pliers in terms of shear bond strength and bracket morphology after debond. Methods: Sixty extracted premolars and nine extracted canines were collected and stored in 1% Chloramine T solution. The …
-
Failure Mechanisms in Unidirectional Composites Under Transverse and Longitudinal Tension
… what is the process by which fiber/matrix debond cracks link up to form transverse cracks, and 2) under longitudinal tension, how does a fracture plane form? In the study, related to transverse tension, plausible mechanisms for transverse crack formation are considered in two scenarios: …
-
Comparison of Finished Case Quality Between Invisalign vs. Traditional Fixed Appliances – A Randomized Control Trial
… and the ABO Objective Grading System, both at debond and 6 month retention. This randomized controlled trial included 80 patients, recruited from the Texas A&M College of Dentistry orthodontic clinic, who were randomly assigned to either the aligner or the braces group. Three time points were …
-
Crack Propagation in Aluminum Sheets Reinforced With Boron-Epoxy
… to the metal sheet. However, cyclic debonding typically occurs over a localized area near the crack. Herein, an analysis was developed to predict both the crack growth and debond growth in a reinforced system. The analysis was based on the use of complex variable Green's functions for …
-
Quantitative evaluation of thin film adhesion using the probe test
… to lift-up from the surface of the substrate. A debond is thus initiated at the loading point and propagates as a semi-circular crack at the interface as the probe slides under the coating. A standard test procedure has been developed for testing thin adhesive coating/substrate systems. The …
-
An interdisciplinary study of cathodic debonding in elastomer/metal adhesive bonds
… activated complex at the degraded crack tip. Debond, or loss of adhesion, can exist in two modes. Weakening denotes debond growth which takes place undetected to the naked eye, and is governed by a diffusion-control degradation process that gives a straight line when plotted against the square …
-
Effect of Pad Design and Bracket Manufacturing Method on Bracket Bond Strength
… difference in shear bond strength and debonding characteristics between one-piece metal brackets made by metal injection molding (MIM) and multi-piece metal brackets made by machining then soldering/brazing with differing pad designs. Methods: A total of thirteen metal orthodontic …
-
Analysis of matrix damage in single fiber composites
… strains or the fiber/matrix interface w ill debond depending on the interfacial strength. This damage of the fiber or the matrix would eventually lead to the ultimate failure of the composite. Hence it is essential to analyze the stresses and energies associated with an unidirectional …
-
The notched coating adhesion specimen: a fracture test for coatings and accelerated screening test for adhesion
… method is proposed to provide estimates of the debond toughness of adhesive bonds. Notched coating adhesion (NCA) specimens consist of single substrates coated with thin layers of adhesive. The coating is notched to induce initial debonds, and the specimen is then loaded in a manner to produce …