Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results

Showing 1 to 20 of 54 for “"fractographic analysis"”.

  1. Analysis of Strength Variation in Glass Due to Ion Exchange

    … resulting Modulus of Rupture (MOR). Statistical analysis techniques and Weibull analysis were used to study the variations which occur within and between strength distributions of each sample group. A smaller sampling of test groups was subjected to fractographic analysis to study the effect of …

    vt Repository record for Analysis of Strength Variation in Glass Due to Ion Exchange (opens in a new tab)

  2. Microstructural and environmental effects on fretting fatigue

    … of stress/life data, crack growth data, and fractographic analysis of two microstructures. The effect of environment is analyzed through data from these two microstructures being tested in lab air and vacuum. The hypothesis developed is that the microstructure plays an important part in the …

    missouri Repository record for Microstructural and environmental effects on fretting fatigue (opens in a new tab)

  3. Combined torsional and cyclic fatigue resistance of rotary endodontic files

    … at the tip of a rotary file on resistance. Fractographic analysis was performed on the fractured files to further understand the mode of failure. Size F2 ProTaper Ultimate (PTU) and ProTaper Gold (PTG) files from Dentsply Sirona were rotated with either a 30° or 60° curvature angle and 5mm …

    ubc Repository record for Combined torsional and cyclic fatigue resistance of rotary endodontic files (opens in a new tab) Download PDF for Combined torsional and cyclic fatigue resistance of rotary endodontic files (opens in a new tab)

  4. An in vitro study of the failure of short-fibre reinforced composite post and core restoration of endodontically treated teeth

    … by conducting the following investigations: (1) analysis of the internal structures of SFRC posts and cores using micro-CT; (2) evaluation of failure load and failure mode of ETT restored with SFRC as a post and core after subjecting the teeth to fracture resistance testing and (3) analysis of …

    adelaide Repository record for An in vitro study of the failure of short-fibre reinforced composite post and core restoration of endodontically treated teeth (opens in a new tab)

  5. The Effect of Cracks and Geo-Morphology on Evaporation from Clay Soils.

    … using a laser scanner, as well as by pixel analysis of surface photographs. The drying test has shown that crack surfaces contributed at most to 6% of total evaporation before de-saturation and up to 63.4% after de-saturation. Results have also shown that Chertkov's model could model crack …

    carleton Repository record for The Effect of Cracks and Geo-Morphology on Evaporation from Clay Soils. (opens in a new tab)

  6. Analysis of Microstructure Evolution and Mechanical Properties of Linear Friction Welded Titanium Alloys

    … as-welded and stress relieved conditions. The fractographic analysis performed on both the tensile and fatigue samples using electron microscope showed the characteristic features of ductile fracture.

    carleton Repository record for Analysis of Microstructure Evolution and Mechanical Properties of Linear Friction Welded Titanium Alloys (opens in a new tab)

  7. Examination of the effect of tin particles and grain size on the charpy impact transition temperature in steels

    … carried out. Scanning electron microscopy (SEM) analysis was used to measure the grain boundary carbide thickness and for fractographic analysis to determine if the coarse TiN particles are acting as cleavage initiation sites. The Charpy ductile-brittle transition temperatures (DBTT) have been …

    birmingham Download PDF for Examination of the effect of tin particles and grain size on the charpy impact transition temperature in steels (opens in a new tab)

  8. Elucidating the Effect of Sintering Time on the Process-Structure-Property Relationship of Inconel 625 Produced by Metal Extrusion Additive Manufacturing

    … in improved tensile strength and elongation. Fractographic analysis confirmed ductile failure via microvoid coalescence in both cases. These findings underscore the critical role of sintering duration in optimising density; despite developing microstructure characteristics that should degrade …

    waterloo Repository record for Elucidating the Effect of Sintering Time on the Process-Structure-Property Relationship of Inconel 625 Produced by Metal Extrusion Additive Manufacturing (opens in a new tab)

  9. Experimental study of the through-thickness strength of laminated composites

    … understanding is the most important. Moreover, fractographic analysis by SEM has also been conducted to support the test results.</p> <p>Finally the Weibull statistics method has been used to treat the stress gradient effect in the different test geometries while establishing the failure map. It …

    oxford Repository record for Experimental study of the through-thickness strength of laminated composites (opens in a new tab)

  10. Toughness-strength relationships in high strength 7xxx aluminium alloys

    … (Al<sub>2</sub>CuMg), was studied via image analysis. The grain structure and grain boundary characteristics (precipitate free zone (PZF) and grain boundary precipitates) were also assessed. Standard <i>K<sub>Ic</sub></i> tests were performed in accordance with ASTM E399. Several failure …

    soton Download PDF for Toughness-strength relationships in high strength 7xxx aluminium alloys (opens in a new tab)

  11. ELEVATED TEMPERATURE DEFORMATION AND FORMING BEHAVIOUR OF AA7075 ALUMINUM SHEET MATERIAL

    … studies for voidinduced damage and fractographic analysis as well as X-Ray diffraction (XRD) studies for analyzing undeformed and deformed grain orientation distribution (bulk texture) are carried out for different AA7075 sheet metal tempers. In addition, a study of development of …

    mcmaster Repository record for ELEVATED TEMPERATURE DEFORMATION AND FORMING BEHAVIOUR OF AA7075 ALUMINUM SHEET MATERIAL (opens in a new tab)

  12. Συγκριτική μελέτη μηχανικών ιδιοτήτων σύνθετων ρητινών και τεχνικών ελέγχου τους

    … Toughness employing SENB and Brazilian tests. Fractographic analysis was carried out in an SEM to determine the origin of fracture for specimens subjected to SENB, Brazilian and Impact Strength testing. The results were statistically analyzed employing ANOVA and Tukey post hoc test (a=0.05) …

    greece Repository record for Συγκριτική μελέτη μηχανικών ιδιοτήτων σύνθετων ρητινών και τεχνικών ελέγχου τους (opens in a new tab)

  13. Mechanical behavior of additively manufactured TI-6AL-4V ELI parts: Effects of laser parameter selection

    … higher stress levels produced increased scatter. Fractographic analysis confirmed surface‑initiated fatigue cracking associated with surface‑connected lack‑of‑fusion defects in both conditions, with reduced defect severity observed for optimized specimens. The experimentally observed crack …

    unf Repository record for Mechanical behavior of additively manufactured TI-6AL-4V ELI parts: Effects of laser parameter selection (opens in a new tab) Download PDF for Mechanical behavior of additively manufactured TI-6AL-4V ELI parts: Effects of laser parameter selection (opens in a new tab)

  14. Design of Surface-Engineered Polymer Fibers as Strength Reinforcements for Cementitious Hybrid Composites

    … and significant flexural modulus enhancement. Fractographic analysis reveals toughening mechanisms such as fiber bridging and pullout that promote effective crack control. The second study introduces a simple and eco-friendly method using metakaolin-coated high-density polyethylene (HDPE) …

    toronto-retro Repository record for Design of Surface-Engineered Polymer Fibers as Strength Reinforcements for Cementitious Hybrid Composites (opens in a new tab)

  15. Effects of thermal processing variations on microstructure and high cycle fatigue of beta-STOA Ti-6Al-4V

    … short and long quench delay times. Post-mortem fractographic analysis and electron back scattered diffraction aided in determining the microstructural influence on fatigue crack initiation and propagation, indicating that long, planar basal slip lengths contribute to crack nucleation. Based upon …

    colo-mines Repository record for Effects of thermal processing variations on microstructure and high cycle fatigue of beta-STOA Ti-6Al-4V (opens in a new tab)

  16. Efeito de um vidro de borossilicato e diferentes tratamentos de superfície na resistência à flexão biaxial de zircônias 4y-psz e multicamada submetidas à fadiga mecânica

    … testing (Instron 3365, 1 mm/min, 5,000 kgf), fractographic analysis via SEM, and chemical characterization via EDS and XRD were subsequently performed. Data were analyzed by two-way ANOVA and Tukey’s test (5%). Results: All studied factors showed statistically significant effects (p < 0.05). …

    brazil-ufrn Repository record for Efeito de um vidro de borossilicato e diferentes tratamentos de superfície na resistência à flexão biaxial de zircônias 4y-psz e multicamada submetidas à fadiga mecânica (opens in a new tab)

  17. The Fatigue Properties Of Spring Steel

    … modelling in coil springs; fatigue and failure analysis, an investigation into measurement of residual stresses and the relation to fatigue life. The operation of springs is directly concerned with the theories of torsion and bending which makes the better understanding of these theories …

    plymouth Repository record for The Fatigue Properties Of Spring Steel (opens in a new tab)

  18. Structure and properties of carbon fibre reinforced aromatic thermoplastics

    … particle size over the size range examined. Fractographic analysis of this phenomenon revealed several toughening mechanisms: Polyetheretherketone (PEEK) rich zones act as crack arresters; fibre bundle and particle bridging of the crack increase the work to fracture. Impact toughness is …

    sheffield-hallam Download PDF for Structure and properties of carbon fibre reinforced aromatic thermoplastics (opens in a new tab)

Page 1 of 3