Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results

Showing 1 to 20 of 218 for “"fractography"”.

  1. Fractography of fresh vs. dry bones

    Limited experimentation has been conducted on fractography of fresh versus dry bones. The present project examined the presence of select fractographic features on wet and dry bone specimens over a time interval of 15 months. The experimental remains consisted of a total of 81 white-tailed deer …

    bu Repository record for Fractography of fresh vs. dry bones (opens in a new tab)

  2. Fractography and crack propagation in functional crystals

    … is the acquisition of fundamental knowledge in fractography to understand the morphology of fracture surfaces and relate them to the applied mechanical stresses. The project integrates the development of innovative methods and procedures for estimating the mechanical properties of GaAs and Si …

    ets-quebec Download PDF for Fractography and crack propagation in functional crystals (opens in a new tab)

  3. Fractography and Mechanical Properties of Laminated Alumina and Yttria Stabilized Zirconia

    … toughening occurring during impact. The fractography and mechanical properties of laminated alumina and YSZ were studied in this thesis. Five sample types were studied in this thesis: (5:5) Al2O3/YSZ (a sequence of 5 alumina tapes stacked on 5 YSZ tapes), (5:5) Al2O3/YSZ (1 wt.% Pure …

    unt Repository record for Fractography and Mechanical Properties of Laminated Alumina and Yttria Stabilized Zirconia (opens in a new tab)

  4. A Study of Decarburization in SAE 1042 Steel: Its Effect on Fatigue Life, Tensile Properties, and Fatigue Fractography

    <p>The R. R. Moore rotating-beam fatigue test was used to determine the effects of-increased surface decarburization on the fatigue life of SAE 1042 steel. This test was conducted on three series of test specimens: (1) specimens having no surface decarburization (series D-1), (2) specimens having a …

    ut-knoxville Repository record for A Study of Decarburization in SAE 1042 Steel: Its Effect on Fatigue Life, Tensile Properties, and Fatigue Fractography (opens in a new tab)

  5. An electron fractography (SEM)investigation of heat-affected zone in the newly developed Climax low-carbon Mn-Mo-Nb Steel

    <p>Recent oil and gas discoveries in the Arctic regions of the United States and Canada have necessitated development of new grades of high strength low alloy steels to meet the stringent toughness specifications for this critical application. The Climax low carbon Mn-Mo-Nb steel was recently …

    ut-knoxville Repository record for An electron fractography (SEM)investigation of heat-affected zone in the newly developed Climax low-carbon Mn-Mo-Nb Steel (opens in a new tab)

  6. FRACTOGRAPHY OF AS-CAST DUCTILE IRON SAMPLES AND ANALYZING THE EFFECT OF SKIN ROUGHNESS ON ITS FATIGUE PROPERTIES USING FRACTURE MECHANICS APPROACH

    … chemically bonded samples are discussed. Fractography provided significant information regarding mode of failure, crack initiation sites and crack propagation path. Quantification of surface profile was done by performing surface profilometer tests. Profilometer tests gave a detailed …

    mtu Repository record for FRACTOGRAPHY OF AS-CAST DUCTILE IRON SAMPLES AND ANALYZING THE EFFECT OF SKIN ROUGHNESS ON ITS FATIGUE PROPERTIES USING FRACTURE MECHANICS APPROACH (opens in a new tab)

  7. Defect imaging and analysis for predicting the reliability of ceramics

    … Subsequently, fracture models plus the fractography were used to predict strength and compared with the results of mechanical testing. Applying high-throughput microscopy and image analysis on the same materials enables prediction of defect populations, their size and nature. Based on …

    unsw Repository record for Defect imaging and analysis for predicting the reliability of ceramics (opens in a new tab)

  8. Fatigue Crack Growth Behavior of CoCrFeNi

    … surface roughness found by post-mortem fractography, and roughness-induced crack closure is supported by opening load data for the load ratio R = 0.05. Fractography also showed step features and surface cracking symptomatic of quasi-cleavage fracture, indicative of limited slip system …

    clemson Repository record for Fatigue Crack Growth Behavior of CoCrFeNi (opens in a new tab)

  9. Bending fatigue of cancellous bone screws used in anterior spine surgery.

    … (3.2mm inside diameter) cancellous bone screws. Fractography was used to qualify and quantify the failure mode. Fracture mechanics was used to determine the load level from the fractographic findings. These results were used in a test program to reproduce the fatigue failures seen in-vivo. The …

    ottawa-retro Repository record for Bending fatigue of cancellous bone screws used in anterior spine surgery. (opens in a new tab)

  10. Microstructure and Mechanical Properties of a Dual Phase Transformation Induced Plasticity Fe-Mn-Co-Cr High Entropy Alloy

    … analysis, mechanical testing, and fractography were performed on the DP-HEA. The microstructural state of the alloy was analyzed by optical microscope, scanning electron microscope (SEM), energy dispersive spectroscopy, and electron backscatter diffraction (EBSD). The plastic …

    alabama Repository record for Microstructure and Mechanical Properties of a Dual Phase Transformation Induced Plasticity Fe-Mn-Co-Cr High Entropy Alloy (opens in a new tab)

  11. Influence of Grain Size and Widmanstätten Colonies on Variability of Tensile Properties of Forged Ti-6Al-4V

    … tensile testing, quantitative metallography and fractography were conducted to identify aspects of the microstructure and fracture surfaces that may have caused the variability. Three aspects of the microstructure that were identified as characteristics that may affect the mechanical properties …

    calpoly Repository record for Influence of Grain Size and Widmanstätten Colonies on Variability of Tensile Properties of Forged Ti-6Al-4V (opens in a new tab)

  12. A study of the stress corrosion cracking of mild steel in alkaline and alkaline sulphide solutions

    … mol/kg NaOH were of the order of 10⁻⁸ m/s. The fractography of the cracks was transgranular in 12.5 mol/kg NaOH at Ecorr. A mixed intergranular-transgranular fractography was observed at the active-passive transition in all three solutions. The results of the two techniques were compared and …

    ubc Repository record for A study of the stress corrosion cracking of mild steel in alkaline and alkaline sulphide solutions (opens in a new tab) Download PDF for A study of the stress corrosion cracking of mild steel in alkaline and alkaline sulphide solutions (opens in a new tab)

  13. Simulating heat affected zone microstructures in high strength low alloy pipeline steels for systematic study of hydrogen susceptibility

    … diffraction (EBSD) analysis. Multi-scale fractography utilized LOM screening, topographic scanning, and SEM for microstructural fracture feature identification. Optical analysis used Nital and selective MA constituent etching with image thresholding for size/shape metrics. EBSD provided …

    colo-mines Repository record for Simulating heat affected zone microstructures in high strength low alloy pipeline steels for systematic study of hydrogen susceptibility (opens in a new tab)

  14. The edge flaking of tungsten carbide hardmetal cermets under repetitive impact loading

    … cone cracking dominates in the cermets. The fractography of the crack surfaces and crack paths, occurring in the cermets, have been studied in order to explain the edge flaking performance. Contiguity and mean-free path are found to have important influences on the edge flaking performance. …

    cape-town Repository record for The edge flaking of tungsten carbide hardmetal cermets under repetitive impact loading (opens in a new tab)

  15. Micromechanisms of cleavage fracture at cryogenic temperatures of SA-738 Gr. B steel and 7% nickel steel

    … test temperature of −120℃ respectively. Detailed fractography of fracture toughness specimens tested at −196 and −170℃ showed that all specimens failed with transgranular cleavage, and eight out of ten cleavage cracks were inclusion-initiated. Nine out of ten specimens had the local fracture …

    birmingham Download PDF for Micromechanisms of cleavage fracture at cryogenic temperatures of SA-738 Gr. B steel and 7% nickel steel (opens in a new tab)

  16. High frequency near-threshhold corrosion fatigue of AISI 316L stainless steel

    … intensity level near the applied values. Crack fractography was studied by scanning electron microscopy. It showed that the fractography generally consisted of three regions; a crystallographic cleavage-like near-threshold region, a feathery and fibrous transition region, and a striated region. …

    ubc Repository record for High frequency near-threshhold corrosion fatigue of AISI 316L stainless steel (opens in a new tab) Download PDF for High frequency near-threshhold corrosion fatigue of AISI 316L stainless steel (opens in a new tab)

  17. Cracking of zirconium alloys at constant load with and without applied potentials

    … technique. Metallurgical microstructures and fractography were analyzed by optical microscopy and scanning electron microscopy (SEM), respectively. The results obtained from this study indicate that no failures were observed under constant loading with smooth specimens. However, the notched …

    unlv Repository record for Cracking of zirconium alloys at constant load with and without applied potentials (opens in a new tab) Download PDF for Cracking of zirconium alloys at constant load with and without applied potentials (opens in a new tab)

  18. Characterization and Simulated Analysis of Carbon Fiber with Nanomaterials and Additive Manufacturing

    … within the nylon filament, as well as the fractography of tested samples. Experimental testing shows that compressive strength increased by 28%, and the average SBS samples increased by 8% with minimal impacts on the tensile strength. The simulated results for Nylon/CF tensile samples were …

    iupui Repository record for Characterization and Simulated Analysis of Carbon Fiber with Nanomaterials and Additive Manufacturing (opens in a new tab)

Page 1 of 11