Global ETD Search
Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.
Results 1 to 20 of 23 for “"fully lamellar"”
-
Fatigue crack threshold and growth behaviour in a near fully-lamellar gamma based titanium aluminides
… and fatigue crack growth of a near fully-lamellar \(y\)-TiAl alloy (Ti-4522XD alloy) have been investigated in air at room temperature, 400, 650, 700 and 750 oC and at three R ratios (0.1, 0.5 and 0.8). Studies were carried out on both corner-cracked specimens and smooth specimens. A …
-
An Experimental and Computational Study of High-Temperature Creep Behavior in Fully Lamellar Titanium Aluminide Alloys
… can exhibit high creep resistance due to their fully lamellar microstructure. These mechanical properties are desirable for components like turbine blades, where tight tolerances must be maintained for optimal performance. This research examines the high-temperature creep behavior of a fully …
-
Modeling and simulation of deformation and fracture behavior of components made of fully lamellar gamma-TiAl alloy
… of deformation and fracture behavior of fully lamellar gamma-TiAl alloy, focusing on understanding the variability of local material properties and their influences on translamellar fracture. A fracture model has been presented that takes the inhomogeneity of the local deformation …
-
Study of the Nucleation Mechanism of a-Ti in Bimodal and Fully Lamellar Microstructures Developed in the High-Strength, Near-Beta Titanium Alloy, TIMETAL®18
… of this alloy in both the bimodal and fully lamellar microstructures. Microstructural characterization was carried out using an FEI Sirion scanning electron microscope and custom stereological routines developed at the Center for the Accelerated Maturation of Materials (CAMM). …
-
Engineering the Alpha Two Phase Morphology in Gamma TiAl Based Alloys
Conventionally processed, fully lamellar, TiAl Based alloys ordinarily possess alpha2 laths having a thickness on the order of hundreds of nanometers. Polycrystalline samples, having compositions between Ti-42Al and Ti-46Al, can be solution heat treated in the alpha phase field, and then rapidly …
-
Mechanisms and Effect of Microstructure on High Temperature Deformation of Gamma-TiAl Based Alloys
… second part of this study creep behavior of the fully lamellar TiAl alloys is investigated. Dislocation structures similar to those observed in the equiaxed alloys suggests that the jogged-screw model can be adapted for lamellar alloys. The aim of the model is to predict the unique creep …
-
Joining of Powder Metallurgy Beta Gamma Titanium Aluminide Through Diffusion Brazing
… post bond heat treatment parameters to achieve a fully lamellar microstructure. Experimental results indicate that diffusion brazing beta gamma alloy below the eutectoid temperature of the substrate results in an α2 reaction layer at the solid/liquid interface that retards diffusion of the melting …
-
Controlling microstructure in nickel 200, titanium grade 2, and titanium grade 5 for the calibration of ultrasonic microstructure characterization
… treatments and hot compression further produced fully lamellar, duplex, and equiaxed (globular) microstructure forms in the TiGr5 material. The theory of ultrasonic signals interacting with grain boundaries and grain/phase interfaces will be discussed in light of the microstructures produced …
-
Directional Solidification, Microstructures and Mechanical Properties of Cr-Cr3Si Eutectic Alloys
… microstructure of the Cr-16.05 at.% Si alloy is fully lamellar and devoid of any pro-eutectic phases suggesting that the best composition for obtaining a fully lamellar structure is Cr-16.05 at.% Si, rather than the eutectic composition (Cr-15 at.% Si) indicated in the phase diagram. The eutectic …
-
Optimization Studies on the Secondary Treatments and Mechanical Behavior of Ti48Al2Cr2Nb Alloy Produced By Electron Beam Melting (EBM) Method
… HT2 transformed the duplex microstructure into a fully lamellar morphology with the highest texture. Room and high temperature tensile tests demonstrated that HIP, HT1, and HT2 treatments effectively mitigated brittleness. HIP reduced anisotropy at room temperature, with a 9.53 MPa difference in …
-
Development of alternative thermomechanical processing techniques to improve forging outcomes of cast peritectic TiAl alloys
… casting segregation or the anisotropic behavinglamellar content that hinders secondary processing; alternative processes are required.For 45XD, this study found that integrating HIP and homogenisation stages into one step, using HIPequipment, proved beneficial to the forging outcome in …
-
Effect of thermomechanical processing on the mechanical properties of cost-effective powder metallurgy titanium-based materials
… strongly dependent on the processing conditions. Fully lamellar microstructures (from processing in the β phase) showed similar strength levels but considerably lower ductility compared to alloys with bimodal microstructures and stronger texture (from processing in the α+β phase). In the case of …
-
Texture evolution of niobium, aluminum, and titanium in Ti-Al-Nb composites processed by accumulative roll bonding
… achieved. The as-received Nb sheet exhibited a fully lamellar structure and had a strong cold rolling texture. After subjecting to ARB, slight grain refining was observed and the high angle grain boundary (HAGB) fraction was increased. The intensity of the α-fiber texture was weakened while that …
-
Microstructural Evolution in Friction Stir Welding of Ti-5111
… the base metal. The weld microstructures show a fully lamellar colony structure with peak welding temperatures exceeding beta transformation temperature. The friction stir weld shows material texture strengthening of the BCC F fiber component before transformation to D2 shear texture in the stir …
-
Microstructure Evolution of EBM Fabricated Ti-6Al-4V
… of the post-processed component. Besides the fully lamellar structure consisting of Widmannstetten a- and b-phase, martensite has been observed in the as-built state. A few additional features are detected in all specimen such as large feature-less regions consisting of a-phase. In all …
-
Verhalten und Lebensdauer einer intermetallischen Legierung auf Basis von gamma-TiAl unter thermomechanischer Beanspruchung
… vergleichbare Lebensdauern, während das Fully-Lamellar-Gefüge tendenziell etwas höhere Lebensdauern aufweist. Weiterhin stellen die gewonnenen Ergebnisse eine wertvolle Datenbasis für die Auslegung von thermomechanisch beanspruchten Komponenten im Turbinen- und Motorenbau dar.
-
The effect of friction stir processing on the microstructure, mechanical properties and fracture behavior of investment cast Ti-6Al-4V
… of the detailed results obtained for the fully lamellar material. The results show that fracture topography depends strongly on the stress intensity range and microstructural length scale. In addition, many of the features observed on the fracture surface were directly related to the …
-
Water Droplet Erosion Resistant Materials and Surface Treatments
… In the first stage of this study, WDE of nearly fully lamellar TiAl alloy was directly compared to Ti6Al4V at relatively wide ranges of impact speed (i.e. 275m/s, 300m/s, 325m/s and 350m/s) and droplet size (i.e. 464µm and 603µm). TiAl demonstrated superior erosion performance (i.e. longer …
-
Innovative materials for high temperature structural applications: 3rd Generation γ-TiAl fabricated by Electron Beam Melting
… 2nd generation γ-TiAl alloys have been successfully fabricated by EBM. To increase the material’s potential, the production of 3rd generation γ-TiAl alloys Ti-(45-46)Al-2Cr-8Nb was therefore studied. The optimization of the EBM parameters led to high homogeneity and very low post-processing …
-
In-situ fabrication of laser additive manufactured titanium-aluminide based alloys doped with niobium-chromium for high performance engineering application.
… with precipitates of β-phase along the lamellar boundaries with hardness of 621.01HV. The β-precipitants helped induced grain boundary pinning and dislocation resistance. The in-house DED printed GE sample and the commercial cast GE had microhardness values of 500.79HV and 401.02HV, …
Page 1 of 2