Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results

Showing 1 to 6 of 6 for “"hot cracks"”.

  1. Influence of microstructure on susceptibility to weld defects in two high strength low alloy steels

    Hot cracking root causes in two HSLA welded steels were investigated and remedies were proposed to avoid hot cracking at centerline of the weld. The specimens were welded in Tjoint configuration keeping the constant welding parameters for both investigated alloys: Gr.50 (with lower content of …

    ets-quebec Download PDF for Influence of microstructure on susceptibility to weld defects in two high strength low alloy steels (opens in a new tab)

  2. The effects of microstructural features and process parameters on the hottearing in direct chill cast aluminum alloys

    Hot tearing is an irreversible failure that occurs above the the solidus temperature of an alloy during casting, in the presence of a liquid phase. These cracks possess serious quality implications in industrial direct chill (DC) casting process. During solidification, thermal stresses are induced …

    ubc Repository record for The effects of microstructural features and process parameters on the hottearing in direct chill cast aluminum alloys (opens in a new tab) Download PDF for The effects of microstructural features and process parameters on the hottearing in direct chill cast aluminum alloys (opens in a new tab)

  3. Avaliação das ligas Al-5%Cu e Al-4%Cu-1%Ni tratadas por refusão à laser para aplicação em manufatura aditiva

    … are susceptible to the formation of pores, cracks, distortions and roughness, which impair high performance applications. The addition of Ni in Al-Cu alloys system makes it possible to improve the mechanical properties at high temperatures and favors the reduction of the solidification …

    brazil-ufrn Repository record for Avaliação das ligas Al-5%Cu e Al-4%Cu-1%Ni tratadas por refusão à laser para aplicação em manufatura aditiva (opens in a new tab)

  4. Non-Newtonian effects in silicate liquids and crystal bearing melts

    … of shear banding and the apparition of 'hot cracks'. Crystal bearing melts exhibit two more Non-Newtonian eects. The first one, the shear thinning, is typical of that observed in previous experiments on crystal-bearing melts. On crystal free melts, this viscosity decrease is observed at …

    lmu-germany Repository record for Non-Newtonian effects in silicate liquids and crystal bearing melts (opens in a new tab)

  5. Laser Powder Bed Fusion of Scalmalloy (Al-4.6Mg-0.6Sc-0.3Zr): Formation Mechanism of Bimodal Grain Structure and Fatigue Behaviour of the Alloy

    … the alloy to be 3D printable, without forming hot cracks. Hot cracking during LPBF of the traditional high strength aluminium alloys largely prevents these alloys from being 3D printable. However, the mechanism of the bimodal grain structure of Scalmalloy during LPBF has not been fully …

    auckland-tech Repository record for Laser Powder Bed Fusion of Scalmalloy (Al-4.6Mg-0.6Sc-0.3Zr): Formation Mechanism of Bimodal Grain Structure and Fatigue Behaviour of the Alloy (opens in a new tab)

  6. Obloukové svařování korozivzdorných ocelí pro náročné pracovní podmínky

    Předložená bakalářská práce se zabývá obloukovým svařováním korozivzdorných ocelí. Pomocí svařovací technologie u státního podniku DIAMO jsou spojovány trubky, příruby a plechy k vedení roztoku síranu sodného, který je získáván jako doprovodný produkt při výrobě uranu. Vlivem chemické reakce …

    brno-tech Repository record for Obloukové svařování korozivzdorných ocelí pro náročné pracovní podmínky (opens in a new tab)