Global ETD Search
Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.
Results
Showing 1 to 6 of 6 for “"hot tensile testing"”.
-
Investigation of Liquid Metal Embrittlement in Advanced High Strength Steels
… and provides a viable solution to suppress LME. Hot tensile testing was first used to evalute the LME susceptiblility of the studied steels. It was discovered that the austenite content of the steels’ microstructure, Si content in the steels’ chemistry and the type of Zn coating all influence the …
-
Effect of Microstructure and Chemical Composition on the Liquid Metal Embrittlement of Advanced High Strength Steels
… (LME) during resistance spot welding (RSW) and hot tensile testing, focusing on the effects of Si and Mo. RSW trials on electrogalvanized sheets showed that a 1.5Si alloy exhibited longer cracks than a 0.6Si alloy due to Si’s role in inhibitinh Fe-Zn reactions and prolonging grain boundaries’ …
-
Fenômeno de fratura intergranular assistida por oxidação em superligas de níquel 718
… Because of this, we have characterized OAIC by hot tensile testing at different strain rates and scanning and transmission electron microscopies, with the alloy in the solutionized condition. In this study, the phenomenon had different onset temperatures for each deformation rate, indicated by …
-
The influence of prior creep damage on the fracture localisation in X20 CrMoV12-1 cross-weld creep tests
… for prolonged periods of time. Non-destructive testing (NDT) methods are utilised extensively on Eskom power plants to determine the remaining life and replacement strategies for critical components. Surface replication is used as a life assessment tool for creep damage quantification of main …
-
Characterizing the Constitutive Behaviour and Austenite Decomposition of an 1,800 MPa Press Hardenable Boron Steel
… designated PHS 1800, was investigated under hot stamping conditions. Prior to mechanical testing, a novel heat treatment technique was developed to pre-alloy the Al-Si coating thereby preventing it from melting during austenitization. The alloy was held at 700°C for 7 – 10 minutes and then …
-
Linear friction welding of AD730™ Ni-based superalloy to additively manufactured Inconel 718
… to 3.5 mm were free from oxides and microcracks. Hot ductility of the forged polycrystalline Ni-based superalloy, AD730TM was investigated in the temperature interval 1050–1240 °C. The nil strength (NST) and nil ductility temperatures (NDT) were determined by hot tensile testing using the …