Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results 1 to 20 of 28 for “"hydrogen cracking"”

  1. Hydrogen cracking and stress corrosion of pressure vessel steel ASTM A543

    … Low Alloy (Q&T HSLA) steel, regarding the cracking behavior and susceptibility to environmental cracking in the base metal and in the heat affected zone (HAZ) when welded. A number of leaking cracks developed in the girth welds of the pressure vessel after a short time of upgrading the …

    colo-mines Repository record for Hydrogen cracking and stress corrosion of pressure vessel steel ASTM A543 (opens in a new tab)

  2. Phase Transformation Behavior and Hydrogen Cracking Susceptibility in Grade T23 and T24 Steel Welds

    Cracking in water walls of newly built fossil power plants using Grade T23 and T24 steels has halted service. The cause for this cracking is still undetermined, and one possible mechanism is hydrogen assisted cracking (HAC). The goal of this research was to compare the susceptibility to HAC in …

    ohiolink Repository record for Phase Transformation Behavior and Hydrogen Cracking Susceptibility in Grade T23 and T24 Steel Welds (opens in a new tab)

  3. Effect of welding parameters on the susceptibility to hydrogen cracking in line pipe steels in sour environments

    In this study, hydrogen induced cracking (HIC) behavior of welded steels used in petroleum lines under sour petroleum environments was investigated. The testing environment in NACE TM0284-2003 standard was used in order to simulate sour petroleum environment. In order to investigate behavior of …

    metu Repository record for Effect of welding parameters on the susceptibility to hydrogen cracking in line pipe steels in sour environments (opens in a new tab)

  4. Development of a test geometry for evaluating the hydrogen cracking susceptibility of high strength GMA welding consumables

    … University through a research programme on the hydrogen cracking susceptibility of multipass girth welds of X-100 steel pipeline produced by the gas metal arc welding process (GMAW). The work aimed to develop a test geometry able to test very low hydrogen content GMAW consumables available in …

    cranfield Repository record for Development of a test geometry for evaluating the hydrogen cracking susceptibility of high strength GMA welding consumables (opens in a new tab)

  5. Soldabilidade do aço USISAC350 na construção metálica

    … welding (SMAW) to compare the susceptibility to hydrogen cracking of the base metals. Tekken test results indicated that only the lower thickness USISAC350 steel did not require preheating to avoid the hydrogen cracking. The heat affect zone of all studied steel grades presented hardness values …

    brazil-ufmg Repository record for Soldabilidade do aço USISAC350 na construção metálica (opens in a new tab)

  6. Hydrogen distribution and redistribution in the weld zone of constructional steels

    … major cause of brittle failure was identi ed as hydrogen embrittlement of the weld zone, although a comprehensive understanding of this phenomenon is not, even now, available. Hydrogen in solution in the weld zone is found in arc welds, due to the intense conditions in the welding arc. There is …

    brunel Repository record for Hydrogen distribution and redistribution in the weld zone of constructional steels (opens in a new tab)

  7. Hydrogen Assisted Crack in Dissimilar Metal Welds for Subsea Service under Cathodic Protection

    … at the weld fusion boundary region. This type of cracking is known as hydrogen assisted cracking (HAC) and it is influenced by base/filler metal combination, and welding and PWHT procedures.DMWs of two material combinations (8630 steel – Alloy 625 and F22 steel – Alloy 625), produced with two …

    ohiolink Repository record for Hydrogen Assisted Crack in Dissimilar Metal Welds for Subsea Service under Cathodic Protection (opens in a new tab)

  8. Development and modelling of weld cooling time equations.

    … susceptibility of a weld's heat affected zone to hydrogen cracking is largely governed by the severity of the cooling portion of the weld's thermal cycle. The 800 to 500 °C cooling time is particularly critical. A model to link the weld bead geometry to the 8OO to 500 °C cooling time for submerged …

    rgu Repository record for Development and modelling of weld cooling time equations. (opens in a new tab)

  9. Variable amplitude corrosion fatigue and fracture mechanics of weldable high strength jack-up steels

    … in the late 80s and early 90s, of extensive cracking around the spud can regions of several Jack-ups operating in the North Sea. It was thought that these steels may be more susceptible to hydrogen cracking and embrittlement. There was the additional requirement to study their behaviour under …

    ucl Repository record for Variable amplitude corrosion fatigue and fracture mechanics of weldable high strength jack-up steels (opens in a new tab)

  10. Effect of Microstructure on Hydrogen Assisted Cracking in Dissimilar Welds of Low Alloy Steel Pipes Joined with Nickel Based Filler Metals

    … protection. These failures were attributed to hydrogen assisted cracking (HAC) along brittle carbides that precipitate in the nickel alloy during onshore PWHT. In response to the field failures, the oil and gas industry began using low alloy steel (LAS) or C-Mn steel overlays in place of nickel …

    ohiolink Repository record for Effect of Microstructure on Hydrogen Assisted Cracking in Dissimilar Welds of Low Alloy Steel Pipes Joined with Nickel Based Filler Metals (opens in a new tab)

  11. Seed-free short time synthesis of zincosilicate zeolite VPI-8 and its catalysis of methane dehydroaromatization reaction

    … sensors, agriculture, medicine, veterinary, hydrogen storage, fuel cells, microreactors, membrane reactors, and racemic separations. Today, zeolite is not limited to aluminosilicate. Researchers are attempting to use other species (such as B, Ga, Ge, Ti, and Zn) to replace aluminum in …

    ksu Repository record for Seed-free short time synthesis of zincosilicate zeolite VPI-8 and its catalysis of methane dehydroaromatization reaction (opens in a new tab)

  12. Caracterização avançada de aços microligados de baixo Mn e alto Nb aplicados em tubos sour service visando aumento do desempenho de tenacidade

    … gas in sour environments, where the presence of hydrogen leads to premature failures of these structures. On the other hand, the low carbon equivalent value, usually found in this type of steel, demands that the hot rolling and accelerated cooling process must be carefully selected in order to …

    brazil-ufmg Repository record for Caracterização avançada de aços microligados de baixo Mn e alto Nb aplicados em tubos sour service visando aumento do desempenho de tenacidade (opens in a new tab)

  13. Cracking in Hot-dip Galvanized Welded Joints of Steel Platform Structures

    … had undergone the same processing with no cracking. This research project began by investigating the metallurgy and microstructure of the base material, the welds, and of the crack sites. Two key features that were noted were the thicker and inclusion-rich grain boundaries in the base …

    alberta Repository record for Cracking in Hot-dip Galvanized Welded Joints of Steel Platform Structures (opens in a new tab)

  14. Fabricação de eletrodo arame tubular auto protegido composto por tubo de aço carbono e fluxo contendo Fe-Cr-Ni para a formação de aço inoxidável como metal de solda na soldagem subaquática de aço carbono A36

    … aqueous environment in which the process occurs. Hydrogen cracking, for example, is a common defect of welded joints under these conditions and leads to reduced mechanical strength and service life of welded components. Given the above, this work investigated the formation of a duplex stainless …

    brazil-ufmg Repository record for Fabricação de eletrodo arame tubular auto protegido composto por tubo de aço carbono e fluxo contendo Fe-Cr-Ni para a formação de aço inoxidável como metal de solda na soldagem subaquática de aço carbono A36 (opens in a new tab)

  15. Evaluation of the Susceptibility of Duplex Stainless Steel 2205 to Hydrogen Assisted Cracking in REAC System

    … crevice/pitting corrosion and stress corrosion cracking. Given the condition of hydrogen-rich environment, high-pressure process fluid, and service temperature, this type of cracking is most likely a form of hydrogen assisted cracking (HAC). It is highly influenced by phase balance …

    ohiolink Repository record for Evaluation of the Susceptibility of Duplex Stainless Steel 2205 to Hydrogen Assisted Cracking in REAC System (opens in a new tab)

  16. Quantification of the Local Mechanical Behavior in Dissimilar Metal Welds and its Effect on Hydrogen Assisted Cracking

    … is a continuation of previous works related to hydrogen assisted cracking susceptibility testing using the delayed hydrogen cracking test (DHCT). DHCT was developed in house within the welding engineering program to study fusion boundary failure of Alloy 625 filler metal to steel Dissimilar …

    ohiolink Repository record for Quantification of the Local Mechanical Behavior in Dissimilar Metal Welds and its Effect on Hydrogen Assisted Cracking (opens in a new tab)

  17. Effect of Postweld Heat Treatment on the Properties of Steel Clad with Alloy 625 for Petrochemical Applications

    … fusion boundary and is possibly susceptible to hydrogen assisted cracking (HAC) and sulfide stress cracking (SSC). National Association of Corrosion Engineers (NACE) standard MR0175/International Standard Organization (ISO) 15156 requires that HAZ hardness should be less than 22 HRC or 250 VHN. …

    ohiolink Repository record for Effect of Postweld Heat Treatment on the Properties of Steel Clad with Alloy 625 for Petrochemical Applications (opens in a new tab)

  18. Thermomechanical factors influencing weld metal hydrogen assisted cold cracking

    Hydrogen Assisted Cold Cracking is a phenomena that manifests itself in weldments when a critical hydrogen concentration is trapped within a susceptible microstructure and subjected to a threshold level of stress and poses a significant threat to pipeline girth weld integrity, in particular the …

    adelaide Repository record for Thermomechanical factors influencing weld metal hydrogen assisted cold cracking (opens in a new tab)

Page 1 of 2