Global ETD Search
Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.
Results
Showing 1 to 20 of 26 for “"iron silicate"”.
-
Interactions of dolomitic lime with iron silicate melts.
… made of the dissolution of dolomitic lime in iron silicate (fayalite) melts at temperatures corresponding to those obtained during the early stages of an LD blow (1300°C). The melts were contained in iron crucibles and held in a furnace under an argon atmosphere. Cylinders of dolomitic …
-
The dissolution of lime in iron silicate melts.
… has been made of the dissolution of lime in iron silicate melts. The experiments were carried out under an inert atmosphere of argon at 1300°C in a vertical tube furnace. A small cylindrical pellet of lime was preheated to the melt temperature before being immersed in the melt contained …
-
Iron Silicate Nano-Crystals as Potential Catalysts or Adsorbents for Heavy Hydrocarbons Upgrading
… however, the necessity for a reduction in the environmental footprint of upgrading processes is a must. This gives rise to produce research on alternate ways for bitumen recovery and upgrading in the reservoir to increase the sustainability of heavy oil and bitumen exploitation. One possible way …
-
Experimental investigation of fundamental viscosity, density, and leaching characteristics of sodium-iron-silicate slags
Environmental regulations govern the emission of sulfur dioxide for lead smelters. Because of this, some have adopted a hydrometallurgical desulfurization step, which results in a sodium-iron-silicate slag being generated in their furnaces. This slag must be disposed of, but the behavior of …
-
Nanostructured Lithium Iron Silicate/carbon Composites As Cathode Material For Next Generation Of Lithium-Ion Batteries
Lithium iron silicate (Li2FeSiO4) has the potential as cathode material for next generation lithium ion batteries because of its high specific theoretical capacity (330 mA h g-1), low cost, environmental benignity, and improved safety. However, itsintrinsically poor electronic conductivity and slow …
-
Quantitative Analysis of Iron Silicate Mineral Composition, Crystal Size, and Volume in the Bald Eagle Intrusion and Contact Metamorphosed Biwabik Iron Formation, Minnesota, USA
… interaction in systems with significant ferrous iron content (Mayhew et al., 2018; Ellison et al., 2021; Geymond et al., 2022; 2023; 2025; Templeton et al., 2024). As olivine is a key mineral of interest for hydrogen generation either through natural water-rock interaction, or engineered …
-
Growth and structure of ultrathin silicates and germanates containing iron oxide
… a detailed study of ultrathin films of FeO, iron silicate, and iron germanate on Ru(0001). These two-dimensional structures are suitable model systems for catalytically active structures, such as zeolites, which are known for their good catalytic properties, for instance as molecular sieves …
-
Development of Techniques for Plasma Membrane and Cell Surface Enrichment
… technique. The pellicle is constructed with iron silicate or silica core nanowires to observe the effects of wire density upon enrichment success. Comparison of these two wire pellicles reveals a two-fold enrichment of transmembrane proteins, over a multiple myeloma whole cell lysate, in both …
-
Selective Reduction of Laterite Ore
… and rate of reduction of nickel, cobalt and iron oxides under different conditions, reduction mechanisms, and optimum conditions for selective reduction of nickel and cobalt oxides. Ore reduction with the size 53-200 μm and size < 53 μm was studied at 700-1000 ℃ in the CO-CO2 gas mixture …
-
The partitioning of iron during the combustion of pulverized coal.
… been found that the amount of chemically bound iron greatly influences the slag contact angle and stickiness on steel heat transfer tubes. The goal of this research, which is part of a larger project headed by the PSI Technology Company to study mineral matter transformations during combustion, …
-
The Densities of Liquid Silicates Containing Iron Oxide at 1410°C.
… the density-composition relationship of iron silicates in contact with solid iron at 1410°C has been determined. The "iron oxide" in an iron silicate has been replaced by calcium oxide, manganous oxide, cobaltous oxide, nickel oxide and calcium fluoride and the density-composition …
-
Electron donor contributions to denitrification in the Elk Valley Aquifer, North Dakota
… organic carbon (OC), pyrite (FeS2), and ferrous iron silicate minerals. In the EVA tracer tests, increases in sulfate indicated that the oxidation of pyrite explained a significant of the denitrification. The contributions of the three electron donors varied between tests and from test to test …
-
A Large-Scale Survey of Brown Dwarf Atmospheres
… shown to exhibit interesting properties such as iron, silicate, and salt clouds. Theoretical atmospheric models based on known physics and chemistry can be used as tools to interpret and understand our observations of brown dwarfs. I have fit archival and new infrared spectra of over 300 brown …
-
Behaviour of trace elements in copper smelting processes - LA-ICP-MS as a tool for sample characterisation
… and lanthanum between copper sulphide mattes and iron silicate slags, no previous data was found in the literature. This also applies to the experimentally verified distribution coefficients of lithium and lanthanum between copper-rich alloy and high-alumina iron silicate slags. Regarding …
-
A study of photo anodes and oxygen evolution
… photoelectrochemical behaviour of flame oxidised iron has been investigated. The transient photo current behaviour has been explained in terms of the creation and subsequent reduction of an oxy-hydroxy intermediate on the electrode’s surface. This has been supported by the results gained by …
-
Dissolution of Valuable Metals from Nickel Smelter Slags by Means of High Pressure Oxidative Acid Leaching
… of sulphide ore concentrates, large amounts of iron are rejected with iron silicate slags. These slags contain Ni, Cu and Co in concentrations up to several percent units. Extraction of the entrapped base metals using high pressure oxidative acid leaching (HPOXAL) was investigated in this work. …
-
The Study of Ultra-Clean Coal
… matter in coal. The efficiency of extraction of iron varied between 60 and 99 percent; of the different forms of iron present in the mineral matter, both the iron silicate and the dilute hydrochloric acid soluble iron were almost completely extracted; the overall efficiency of extraction of iron …
-
An experimental study of the system FeO-Fe2O3-SiO2 at high pressures and temperatures : Garnet, perovskite and post-perovskite phases
… lower mantle conditions, garnets transform into silicate perovskite (bridgmanite) and eventually into post-perovskite (CaIrO3-structured) silicate. Incorporation of iron into the structures of these phases can strongly affect chemical and physical properties of the Earth’s mantle, as well as its …
-
Phase equilibria and precious or high-tech metal distributions in copper smelting systems
… matte/copper and silica/spinel/wüstite-saturated iron silicate slags as well as the distribution equilibria of precious (Au, Ag, Pt, and Pd) and high-tech (Ni, Co, and Sn) metals in the equilibrium systems were investigated using an advanced high-temperature isothermal equilibration/quenching …
Page 1 of 2