  1. Improving the delamination bridging behaviour of z-pins through material solutions

    … fracture toughness of the order of 40 kJ/m2, compared to the 28 kJ/m2 yielded by commercial CF/BMI Z-pins. Moreover, the transition from full pull-out to rupture occurs at a mode-mixity of 0.55, whereas BMI Z-pins start failing at a mode-mixity of 0.19.<br/>The effect of the fibre …

    bristol Repository record for Improving the delamination bridging behaviour of z-pins through material solutions (opens in a new tab)

  2. Structure et mécanismes de microdéformation de polymethylmethacrylates renforcés au choc

    … impact toughness, which does not exceed 5.5 kJ/m2 in any of the RTPMMA. There may be scope for further optimizing the particle size at high EA contents owing to an observed decrease in entanglement molar mass, as demonstrated in previous work by Béguelin et al., but this is not thought to be …

    epfl Repository record for Structure et mécanismes de microdéformation de polymethylmethacrylates renforcés au choc (opens in a new tab)

  3. Fracture toughness of conventional, milled and printed denture bases

    … significantly larger work of fracture values (~8 KJ/m2 vs ~3 KJ/m2). Conclusion: The tested 3D-printed denture base material had significantly higher KIC, exhibited crazing, had a higher absorbed energy before fracture and was stable under ageing conditions, suggesting that it could be more …

    ubc Repository record for Fracture toughness of conventional, milled and printed denture bases (opens in a new tab)

  4. Experimental and Micromechanical Analysis of Flax and Glass Reinforced Bio-Based Composites

    … resin reinforced with E-glass fibers was 237 kJ/m2, whereas that of the vinyl ester resin reinforced with same E-glass fiber was 191 kJ/m2. Results of SEM images along with flexural strength, interlaminar shear strength and impact tests revealed better wetting of fibers by matrix, stronger …

    ndsu Repository record for Experimental and Micromechanical Analysis of Flax and Glass Reinforced Bio-Based Composites (opens in a new tab)

  5. Phase morphology and fracture toughness of CNT/polytherimide modified epoxy polymer nanocomposites as matrices for advanced CFPR composites

    … for the even lowered fracture toughness (0.90 kJ/m2 ) compared to the corresponding CNT-free systems (0.85 kJ/m2 ). This is not the case for the FRP composites based on the tetrafunctional epoxy resin where the resulting uniform phase morphology contributes to further improvements in fracture …

    qu-belfast Repository record for Phase morphology and fracture toughness of CNT/polytherimide modified epoxy polymer nanocomposites as matrices for advanced CFPR composites (opens in a new tab)

  6. The use of advanced oxidation processes in the degradation of the pesticide chlorpyrifos and reduction of microbial contamination on apples

    … achieved through an AOP treatment applying 68.4 kJ/m2 UV dose and 1.22% v/v H2O2 at 66°C that resulted in a 47% reduction (92µg) of the pesticide with < 0.004 µg accumulation of chlorpyrifos-oxon. The same treatment supported a >6.56 log CFU reduction in E. coli O157:H7 and >6.56 log CFU …

    guelph Repository record for The use of advanced oxidation processes in the degradation of the pesticide chlorpyrifos and reduction of microbial contamination on apples (opens in a new tab)

  7. Developing Short Milled Carbon Fibre Modified Toughened Epoxy Matrix for Superior and Inexpensive infrastructural CFRP Laminates

    … MPam1/2 whereas GICMat was increased from 0.26 kJ/m2 to 2.06 kJ/m2, which is believed to result from the combined effect of fibre stereology and the debonding/pull-out mechanisms observed under Scanning Electron Microscope (SEM) images of fracture surfaces. In addition, the flexural modulus of …

    unsw Repository record for Developing Short Milled Carbon Fibre Modified Toughened Epoxy Matrix for Superior and Inexpensive infrastructural CFRP Laminates (opens in a new tab)

  8. Stimuler les défenses des plantes contre botrytis cinerea par des rayonnements UV-C

    … faibles et répétées d’UV-C (inférieur à 1,70 kJ/m2). Cette stimulation est associée au renforcement de la paroi cellulaire, à l’augmentation des composés phénoliques et à l’augmentation de l’activité de certaines enzymes antioxydantes. Lorsque le traitement par les rayonnements UV-C est …

    star-france Repository record for Stimuler les défenses des plantes contre botrytis cinerea par des rayonnements UV-C (opens in a new tab)

  9. Design of Sintered, Tough, Oxide Laminate and Fibrous Monolithic Composites

    … and a work of fracture of 142 MPa and 0.51 KJ/m2, respectively. Fibrous monolithic composites with different interphase thickness and interphase composition were fabricated. 2-, 3- and mixed-layer fibrous monolithic composites were made.

    uiuc Repository record for Design of Sintered, Tough, Oxide Laminate and Fibrous Monolithic Composites (opens in a new tab)

  10. Photo-sensitive Natural Rubber Applied for Utilization in Stereolithography 3D Printing

    … augmentation de la résistance à l’impact (6,1 kJ/m2) et de l’étirement (4,0 %) par rapport à la résine commerciale pure (2,4 kJ/m2 de résistance à l’impact et 2,2 % d’allongement à la rupture) sans pour autant avoir une diminution simultanée du module d’Young et de la résistance mécanique. La …

    star-france Repository record for Photo-sensitive Natural Rubber Applied for Utilization in Stereolithography 3D Printing (opens in a new tab) Restricted access

  11. Desarrollo y optimización de wood plastic composites con matriz biopolimérica y fibras naturales

    … BioHDPE, obteniendo valores de 5275 MPa y 3,6 kJ/m2, respectivamente, en comparación con el bioHDPE puro de 826 MPa y 2,0 kJ/m2. En cuanto al cambio de color de las muestras inyectadas, se observó que el aumento de fibra generó una clara modificación en las tonalidades finales de las piezas, …

    upv Repository record for Desarrollo y optimización de wood plastic composites con matriz biopolimérica y fibras naturales (opens in a new tab)

  12. Mechanical and electrical properties of micro-architectured carbon nanotube sheet

    … The highest tearing energy measured is 11.6 kJ/m2 indicating the promise to use these materials in load bearing applications.

    uiuc Repository record for Mechanical and electrical properties of micro-architectured carbon nanotube sheet (opens in a new tab)

  13. Machine-learning Assisted Process Optimization for Laser Powder Bed Fusion

    … - 10.3%), and fracture toughness (9.9 - 12.7 kJ/m2). The underlying reason was attributed to the subtle microstructural differences that were further revealed using two newly defined morphology indices (i.e., dimensional-scale index Id and shape index Is) based on several key microstructural …

    unsw Repository record for Machine-learning Assisted Process Optimization for Laser Powder Bed Fusion (opens in a new tab)

  14. ENHANCEMENT OF A COPOLYESTER’S IMPACT RESISTANCE VIA INORGANIC REINFORCEMENT

    … achieved an impact resistance of 553 kJ/m2 and a flexural modulus of 244 MPa, representing increases of approximately 54% and 28%, respectively, compared with neat Hytrel. Functionalized nanocomposites also exhibited excellent property retention after hydrothermal aging. These results …

    fau Repository record for ENHANCEMENT OF A COPOLYESTER’S IMPACT RESISTANCE VIA INORGANIC REINFORCEMENT (opens in a new tab)

  15. Augalų atsparumas abiotiniams veiksniams /

    … after treating the plants with UV-B (2, 4, 8 kJ/m2) and ozone (40 ir 80 ppb) doses. Test data shows, that morphometrical parameters such as fresh and dry weight along with leaf area and count are very sensitive to stress factors. Biochemical parameters such as soluble protein content and the …

    vilnius Repository record for Augalų atsparumas abiotiniams veiksniams / (opens in a new tab)

  16. High stiffness, high strength and high toughness green composites based on poly(hydroxybutyrate-co-valerate) (PHBV)

    … with values of 16.9 GPa, 183 MPa and 42 kJ/m2, respectively, being obtained. The inclusion of PBAT did not affect the mechanical properties except for some reduction in flexural strength. The inclusion of ENR produced significant increases in impact resistance but reductions in tensile …

    unsw Repository record for High stiffness, high strength and high toughness green composites based on poly(hydroxybutyrate-co-valerate) (PHBV) (opens in a new tab)

  17. INNOVATIVE APPROACHES TO PLANT PROTECTION AND PRODUCE SAFETY THROUGH HIGH-PRECISION PLANT MANAGEMENT SYSTEMS

    … short-term exposure to UV-B radiation (43.2 kJ m−2) induced only moderate physiological stress and shifts in the composition of epiphytic and endophytic bacterial communities. 16S rDNA profiling through Nanopore sequencing of both DNA (epiphytic part) and cDNA (endophytic part) templates …

    milano Repository record for INNOVATIVE APPROACHES TO PLANT PROTECTION AND PRODUCE SAFETY THROUGH HIGH-PRECISION PLANT MANAGEMENT SYSTEMS (opens in a new tab) Embargoed

  18. Biomimetism of Brazil nutshell (Bertholletia excelsa)

    … modulus of 2.52 GPa, and impact strength of 1.8 kJ/m2. However, adjustments and improvements in the syntactic foam are still required.

    brazil-ufscar Repository record for Biomimetism of Brazil nutshell (Bertholletia excelsa) (opens in a new tab)

  19. Estudo das propriedades mecânicas, térmicas e de transporte do compósito com carbonato de cálcio nano e microparticulado em polipropileno

    … of nanoparticulate increased from 4.60 to 4.96 KJ/m2 concentration of 7.87% of CaCO3. As for the Tensile strength, only 0.48% of nanoparticulate CaCO3 increased from 32.8 MPa to 35.2 MPa. HDT in the gain was 12ºC with respect to the homopolymer PP and a 2.9 ºC on the microparticulate composite. …

    brazil-ufscar Repository record for Estudo das propriedades mecânicas, térmicas e de transporte do compósito com carbonato de cálcio nano e microparticulado em polipropileno (opens in a new tab)

  20. Uso de luz UV-C en mango “Tommy Atkins” y su efecto en los atributos de calidad e inocuidad: Estudio matemático basado en CFD

    … se evaluó el efecto de la dosis óptima de 6 kJ/m2 en los atributos de calidad del mango mínimamente procesado almacenado por 12 días a 5 °C. Los resultados mostraron que la aplicación de esta dosis permitió asegurar la inocuidad y preservar la mayoría de los atributos de calidad del mango …

    un-colombia Repository record for Uso de luz UV-C en mango “Tommy Atkins” y su efecto en los atributos de calidad e inocuidad: Estudio matemático basado en CFD (opens in a new tab)

Page 1 of 3