  1. Thermo-Oxidative Degradation of HDPE Geomembranes: Effect of Phenolic Antioxidant and Hindered Amine Light Stabilizer Concentrations

    … of phenolic antioxidant and hindered amine light stabilizer (HALS) with under the six months of the thermal-oxidative degradation. The interactions between phenolic antioxidant, HALS and carbon black can affect the mechanical, physical and chemical properties. To monitor these properties, …

    usf Repository record for Thermo-Oxidative Degradation of HDPE Geomembranes: Effect of Phenolic Antioxidant and Hindered Amine Light Stabilizer Concentrations (opens in a new tab)

  2. Untersuchungen zum Einfluss von Additiven auf die Langzeitstabilität von Polyethylenvinylacetatfolie bei Einsatz als Einbettmaterial in Photovoltaik-Modulen

    … das sogenannte HALS (hindered amine light stabilizer). Im Rahmen der Arbeit ist es gelungen Ursache-Wirkungs-Zusammenhänge zwischen der Folienadditivierung und dem Auftreten verschiedener Fehlerbilder zu identifizieren. Darüber hinaus war es möglich eine Folienzusammensetzung zu …

    qucosa-diss

  3. Estabilização radiolítica do Poli(metacrilato de metila) industrial

    … PMMA. O aditivo é do tipo HALS (Hindered Amine Light Stabilizer) que tem como ação básica a captura de radicais e, mesmo não tendo aplicação para proteção radiolítica, demonstrou uma boa radioproteção ao PMMA. A avaliação das cisões na cadeia principal induzida pela radiação foi realizada usando …

    brazil-ufpe Repository record for Estabilização radiolítica do Poli(metacrilato de metila) industrial (opens in a new tab)

  4. High performance clear-coat systems for wood used outdoors

    … acid, and a PF-resin containing a hindered amine light stabilizer. The solvent based polyurethane was more compatible than the water-based acrylic and alkyd coatings with treated wood surfaces. Wood treatments had no effect on coating adhesion, but coating adhesion was highest for the …

    ubc Repository record for High performance clear-coat systems for wood used outdoors (opens in a new tab) Download PDF for High performance clear-coat systems for wood used outdoors (opens in a new tab)

  5. Photodegradation of adhesives used in wood composite materials

    … photodegradation. The effectiveness of a UV light absorber and hindered amine light stabilizer (UVA and HALS) at protecting adhesives from photodegradation was also investigated. First, the effect of adhesive type (melamine formaldehyde, epoxide, and emulsion polymer isocyanate), stabilizer …

    ubc Repository record for Photodegradation of adhesives used in wood composite materials (opens in a new tab) Download PDF for Photodegradation of adhesives used in wood composite materials (opens in a new tab)

  6. Investigations of catalyst behaviour in the formation of polyurethanes

    … addition of UV absorber and HALS (Hindered Amine Light Stabilizer) overcame the sensitivity of the titanium chelate catalyzed coating when exposed to UV radiation and performed better than the control catalysed with the organotin carboxylate catalyst. The titanium chelate catalyst system was …

    auckland-ms Repository record for Investigations of catalyst behaviour in the formation of polyurethanes (opens in a new tab)

  7. Hodnocení degradace inkoustového tisku

    Tato diplomová práce se zabývá studiem degradace inkoustového tisku na ručním papíru, který je upraven polymerní vrstvou s obsahem světelného stabilizátoru a anorganického plniva. Polymerní vrstva natíraná na médium byla tvořena polyvinylalkoholem, oxidem titaničitým a přídavkem světelného …

    brno-tech Repository record for Hodnocení degradace inkoustového tisku (opens in a new tab)

  8. Photodegradation and photostabilization of weathered wood flour filled polyethylene composites

    … fade, and loss of flexural properties. The final lightness of the composites was not dependent upon the manufacturing method. However the mechanical property loss was dependent upon manufacturing method. The samples with more wood component at the surface (planed samples) experienced a larger …

    mtu Repository record for Photodegradation and photostabilization of weathered wood flour filled polyethylene composites (opens in a new tab)

  9. Vinyl methyl oxazolidinone as a styrene substitute for unsaturated polyester resins

    … and Irganox® 1330, as well as hindered amine light stabilizer Tinuvin® 765 during the resin preparation, turned out to be not ineffective for UP-FI-based resin. However, a slight extension of the resin storage stability time was observed after the addition of 500 to 2000 ppm of Irganox® 1330. …

    qucosa-diss