Effect of composition variation and service environment on the long term ageing of 316H austenitic stainless steel
… creep performance. The microstructures after long term ageing were characterised, and it was demonstrated that certain chemical elements, notably Si and P, have a role in the formation of precipitates, and the partitioning or segregation of elements to these phases at grain boundaries. …
-
Long-term ageing of concrete structures in Finnish rock caverns as application facilities for low- and intermediate-level nuclear waste
… barriers ensuring the safety of low- and intermediate-level waste repositories in rock caverns are designed to remain serviceable for hundreds of years. With regard to the ageing of the concrete, the lifetime of the disposal facilities will be divided into the periods before and after the …
-
Probabilistic models for reliability assessment of ageing equipment and maintenance optimization
… maintenance models for reliability assessment of ageing equipment and maintenance optimization. The proposed Markov models can represent non-periodic inspection and maintenance better than the existing models in the literature. Sensitivity analyses are performed on both models to investigate the …
-
On the puncture strength of rubber
… The energy beneath the indentor was determined using a model experiment based on the biaxial stretching of rubber by inflation. The energy stored in the rubber surrounding the indentor was calculated. The contribution of these energies was shown to be small. The puncture test was used …
-
Performance evaluation of carbon-dioxide sensors used in building HVAC applications
… sensors were tested and evaluated to determine the accuracy, linearity, repeatability, hysteresis, humidity sensitivity, temperature sensitivity, and pressure sensitivity of each sensor as well as effect of long-term ageing on sensor performance. All tests were conducted in a chamber …
-
Optimising calcium phosphate cement formulations to widen clinical applications
… solubility to overcome the problems faced by long term stability of hydroxyapatite (HA) cements; (2) manipulating the cement formulation to produce a cement that can set on a change in temperature, upon implantation, increasing handling time during surgeries; (3) incorporating therapeutic …
-
Fundamental Characterisation of Asphalt Overlaid Rigid Pavements
… connectivity and sustainable movement, yet its long-term performance is often compromised by ageing, environmental stresses and increasing traffic loads. Among the key factors influencing pavement durability are thermal properties, which directly affect mechanical behaviour, heat distribution in …
-
Development of Polymer Modified Pelletised Bitumin for Utility Reinstatements and Emergency Pothole Repair
… binder PPMB on the asphalt has been evaluated in terms of stiffness, permanent deformation (wheel track test, creep test and indentation test) and fatigue life test, durability (water sensitivity and freeze-thaw cycle) in comparison with the conventional patching materials. The results showed that …
-
Multiphysics Modelling and Mitigation of Ageing in Asphalt Pavements
Bitumen binders oxidise with air and cause ageing deterioration of asphalt pavements in the form of hardening, cracking and an overall decline in the mechanical performance. The degree of oxidative ageing is governed by many coupled internal and external physics and variables, making it difficult …
-
Investigation of Different Factors Affecting Asphalt Cement Ageing and Durability
… and its performance period is called ageing. The severity of the age-hardening significantly depends on environmental factors such as temperature, latitude (which affects the angle of sunshine radiation), humidity, ultraviolet, etcetera, as well as mixture properties (such as aggregate …
-
Mechanical Properties of INCONEL 740H at 725°C
… material (as manufactured) and after stress-free long-term ageing at 725°C for up to 20,000 hours. The temperature of 725°C was selected based on the literature review, and discussion with the material provider. At the time of the study there was very sporadic date points at 725°C for the …
-
Characterisation of lead-free solder pastes and their correlation with the stencil printing process performance
… part of the study concerns the influence of long-term ageing on the rheology and print quality of lead-free solder pastes used for flip-chip assembly, and the main focus of the work was to develop methodologies for benchmarking new formulations in terms of shelf life, rheological …
-
Monitoring and modelling the long-term performance of Dublin Port Tunnel
… even endanger tunnel integrity and safety in the long term. To better the understanding of the structural health condition of this critical underground infrastructure, this thesis specifically investigates the long-term ageing performance of a cross passage twin tunnel section of Dublin Port …
-
Bio-inspired nacre-like ceramic/polymer composites for dentistry
… due to its high hardness, and potential <br/>long-term ageing and aesthetics issues. Recent advances in the manufacture of polymerinfiltrated ceramic network (PICN) materials, which combine the benefits of both ceramic <br/>and polymer to achieve tooth-matching mechanical properties, present a …
-
Fuel parameter testing, quality assessment and engine emissions evaluation of biodiesel (B100), diesel (D100) and its 20% blend (B20) under long term storage conditions
… and cause changes in its fuel properties. The long-term ageing under real-time conditions of two different biodiesel (B100) fuels (from soybean oil and waste vegetable oils), two petroleum derived diesel (D100) fuels and their 20% vol. or B20 fuel blend was studied by storing these blends under …
-
Experimental and modelling studies of electronic packaging interconnections formed with lead-free materials
… carried out and the growth behaviours of the intermetallic compounds (IMCs) during wetting, solidification and isothermal ageing have been investigated. It has been found that the addition of Bi into the Sn-Ag-Cu solder reduces the consumptions of the substrates and suppresses the growth of IMCs …
-
Development of a New High Performance Cold Mix Asphalt
… This aim has been achieved by i) addressing the longstanding problems associated with conventional bitumen emulsions, namely large and non-uniform distribution of bitumen droplets within the emulsion, and ii) reducing the long curing time of CBEMs by replacing conventional limestone filler (LF) …
-
Možnosti hodnocení a predikce trvanlivosti betonu
Diplomová práce se zabývá problematikou trvanlivosti betonu se zaměřením na karbonataci betonu a cyklické zmrazování a rozmrazování. V rámci práce byly provedeny dva experimenty. První experiment byl zaměřen na hodnocení dlouhodobého vývoje mechanických vlastností betonu, posouzení kvality …
-
SURFACE TAILORING OF OXIDE-BASED NANOSYSTEMS FOR THE DESIGN OF ADVANCED COMPOSITE MATERIALS AND SMART DEVICES
… exposes aluminium hydroxyl groups, while the outermost layer is silica[1]. Among its many potential applications, its tubular dual structure has sparked interest in the field of nanomedicine and polymer nanocomposites[2]. However, only few reports investigated the possibility of a selective …