Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results

Showing 1 to 20 of 24 for “"melt fracture"”.

  1. Melt Fracture of Polystyrene

    … viscometer has been used to study the melt fracture of polystyrene. The polystyrene samples used differed in molecular weight and molecular weight distribution. The weight average molecular weight (Mw) ranged from 97,200 to 1.8 x 10^6 and the distribution breadth (Mw/Mn) from 1.06 to …

    mcmaster Repository record for Melt Fracture of Polystyrene (opens in a new tab)

  2. Melt fracture behaviour of molten polypropylenes

    … for the onset of slip, surface and gross melt fracture. It was found that there was no distinction between surface and gross melt fracture, which is commonly observed in the case of polyethylenes. Furthermore, the flow curves determined by using capillaries having various diameters are …

    ubc Repository record for Melt fracture behaviour of molten polypropylenes (opens in a new tab) Download PDF for Melt fracture behaviour of molten polypropylenes (opens in a new tab)

  3. Critical Stress and Recoverable Shear for Polymer Melt Fracture

    … used in this study. The behaviour of the melts at the onset of instabiIity was explained by using Graessley's correlation between "true" and Rouse shear compliance in Hooke's law. It was found that the critical stress increases linearly as the weight average molecular weight decreases, …

    mcmaster Repository record for Critical Stress and Recoverable Shear for Polymer Melt Fracture (opens in a new tab)

  4. The role of surface energy of boron nitride on gross melt fracture elimination of polymers

    … with the critical shear rate for the onset of melt fracture, indicating the importance of surface energy in the procedure of selecting an effective processing aid. In addition, experiments were carried out in both an Instron capillary rheometer equipped with a special annular die (Nokia …

    ubc Repository record for The role of surface energy of boron nitride on gross melt fracture elimination of polymers (opens in a new tab) Download PDF for The role of surface energy of boron nitride on gross melt fracture elimination of polymers (opens in a new tab)

  5. The effect of surface properties of Boron Nitride on polymer processability

    … as distortions on the extrudate surface (melt fracture), usually observed at high production rates. Fluoropolymers have long been used as processing aids for surface melt fracture treatment of polyolefin extrudates. Recent developments have shown that a small amount of Boron Nitride (BN) …

    ubc Repository record for The effect of surface properties of Boron Nitride on polymer processability (opens in a new tab) Download PDF for The effect of surface properties of Boron Nitride on polymer processability (opens in a new tab)

  6. Boron nitride and its combinations as processing aids in the extrusion of Ziegler-Natta polyethylenes

    … on the extrudate surface (sharkskin or surface melt fracture) or in the form of irregular helix distortions (gross melt fracture) at higher shear rates. Usually, polymer processing aids are used to postpone/eliminate these melt fractures. Fluoropolymer has been found to be effective in …

    ubc Repository record for Boron nitride and its combinations as processing aids in the extrusion of Ziegler-Natta polyethylenes (opens in a new tab) Download PDF for Boron nitride and its combinations as processing aids in the extrusion of Ziegler-Natta polyethylenes (opens in a new tab)

  7. The flow stability of linear low-density polyethlene at polymer and metal interfaces

    … of the single component instability of surface melt fracture on the interface behavior in stratified bicomponent flow has been examined. First, the factors and conditions leading to the onset of surface melt fracture in linear low-density polyethylene (LLDPE) were identified using …

    vt Repository record for The flow stability of linear low-density polyethlene at polymer and metal interfaces (opens in a new tab)

  8. Rheology and processing of molten poly(methyl methacrylate) resins

    … on the extrudate surface (sharkskin or surface melt fracture) or in the form of helix and/or chaotic distortions (gross melt fracture). To postpone such phenomena to higher shear rates processing aids are used. External processing aids, such as fluoropolymers and waxes, have been found to be …

    ubc Repository record for Rheology and processing of molten poly(methyl methacrylate) resins (opens in a new tab) Download PDF for Rheology and processing of molten poly(methyl methacrylate) resins (opens in a new tab)

  9. The effect of boron nitride on the rheology and processability of molten polymers

    … or not, the critical conditions for the onset of melt fracture is determined. The influence of the average size of boron nitride particles, its agglomeration if present, its concentration in the resins and the quality of the attained dispersion on the melt fracture of the metallocene polyethylene …

    ubc Repository record for The effect of boron nitride on the rheology and processability of molten polymers (opens in a new tab) Download PDF for The effect of boron nitride on the rheology and processability of molten polymers (opens in a new tab)

  10. Flow instabilities of PP filled with crosslinked EPDM rubber : using rheology to understand and control its occurrence

    … particles which make flow instability such as melt fracture intense and complicated. In this study a comprehensive rheological analysis is performed to gain a deep understanding of TPVs’ flow instabilities and identify the key parameters that control them. First, a thorough linear viscoelastic …

    ubc Repository record for Flow instabilities of PP filled with crosslinked EPDM rubber : using rheology to understand and control its occurrence (opens in a new tab) Download PDF for Flow instabilities of PP filled with crosslinked EPDM rubber : using rheology to understand and control its occurrence (opens in a new tab)

  11. Influence of molecular structure on rheological and processing behaviour of molten polymers

    … and processing behaviour. In particular, the melt fracture and wall slip phenomena have been extensively studied using various rheological tools and techniques. In order to study the effects of the two key molecular characteristics, the weight average molecular weight and the molecular weight …

    ubc Repository record for Influence of molecular structure on rheological and processing behaviour of molten polymers (opens in a new tab) Download PDF for Influence of molecular structure on rheological and processing behaviour of molten polymers (opens in a new tab)

  12. Rheology and processability of teflon FEP resins for wire coating

    … The critical conditions for the onset of melt fracture and the influence of temperature, molecular weight, and composition of the resins are determined. The critical molecular weight for the onset of entanglements was found to be about 100,000, a value much higher than those previously …

    ubc Repository record for Rheology and processability of teflon FEP resins for wire coating (opens in a new tab) Download PDF for Rheology and processability of teflon FEP resins for wire coating (opens in a new tab)

  13. Rheology and capillary flow of sodium and zinc ionomers

    … in terms of instabilities such as wall slip and melt fracture. It was found that the no-slip boundary condition is a valid assumption for these polymers due to the strong ionic associations and strong interactions with the capillary wall. All ionomers were found to exhibit gross melt fracture and …

    ubc Repository record for Rheology and capillary flow of sodium and zinc ionomers (opens in a new tab) Download PDF for Rheology and capillary flow of sodium and zinc ionomers (opens in a new tab)

  14. Rheology and processing of biodegradable poly(epsilon -caprolactone) polyesters and their blends with polylactides

    The solution rheological properties and melt viscoelastic behaviour of a number of commercial and newly synthesized PCLs with different molecular characteristics was investigated using both rotational and extensional rheometry. The variation of zero-shear viscosity and relaxation spectrum with …

    ubc Repository record for Rheology and processing of biodegradable poly(epsilon -caprolactone) polyesters and their blends with polylactides (opens in a new tab) Download PDF for Rheology and processing of biodegradable poly(epsilon -caprolactone) polyesters and their blends with polylactides (opens in a new tab)

  15. Rheology and processing of high-density polyethylenes (HDPEs) : effects of molecular characteristics

    … of both series of HDPEs was investigated. Their melt fracture behaviour was studied primarily as a function of Mw and MWD, and operating conditions i.e. temperature and geometrical details and type of die (capillary, slit and annular). It is found that sharkskin and other melt fracture phenomena …

    ubc Repository record for Rheology and processing of high-density polyethylenes (HDPEs) : effects of molecular characteristics (opens in a new tab) Download PDF for Rheology and processing of high-density polyethylenes (HDPEs) : effects of molecular characteristics (opens in a new tab)

  16. Rheology and processing of poly(lactides) and their enantiomeric copolymers and blends

    … different ratios of lactides) on solution and melt rheological properties under shear and extension were studied. The solution properties and linear viscoelasticity (LVE) of melts indicated linear structure behavior. The zero-shear viscosity and relaxation time of PLAs showed a power law …

    ubc Repository record for Rheology and processing of poly(lactides) and their enantiomeric copolymers and blends (opens in a new tab) Download PDF for Rheology and processing of poly(lactides) and their enantiomeric copolymers and blends (opens in a new tab)

  17. Flow Behavior of Sparsely Branched Metallocene-Catalyzed Polyethylenes

    … and extensional rheological properties, the melt fracture behavior, and the ability to accurately predict the flow through an abrupt 4:1 contraction geometry. The effects that sparse long-chain branching (M<sub>branch</sub> > M<sub>c</sub>) has on the shear and extensional rheological …

    vt Repository record for Flow Behavior of Sparsely Branched Metallocene-Catalyzed Polyethylenes (opens in a new tab)

  18. Capillary rheometry of soy isolate dough

    … doughs are discussed including yield stresses, melt fracture and sample reservoir pressure losses.

    vt Repository record for Capillary rheometry of soy isolate dough (opens in a new tab)

  19. Thermorheology and processing of polyethylene blends : macromolecular structure effects

    … weights. At high LDPE weight fractions, DSC melting thermograms have shown three different polymer phases; two for the pure components and a third melting peak of co-crystals. Different rheological techniques were used to check the thermo rheological behavior of all blends in the melt state …

    ubc Repository record for Thermorheology and processing of polyethylene blends : macromolecular structure effects (opens in a new tab) Download PDF for Thermorheology and processing of polyethylene blends : macromolecular structure effects (opens in a new tab)

  20. Arborescent Polystyrene-graft-Polyisoprene Copolymers as Polymer Processing Additives

    … low density polyethylene (LLDPE) suffer from melt defects including sharkskin, cyclic melt fracture, and gross melt fracture during processing. The occurrence of these defects sets an upper limit to the rate at which these polymers can be processed, thus increasing production costs. One method …

    waterloo Repository record for Arborescent Polystyrene-graft-Polyisoprene Copolymers as Polymer Processing Additives (opens in a new tab)

Page 1 of 2