Global ETD Search
Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.
Results
Showing 1 to 5 of 5 for “"mold thickness"”.
-
Thermal Management and Solidification Characteristics in High Performance Aluminum Casting
… this objective. In this technique a water jet demolds the water soluble sand mold and subsequently impinges upon the solidifying metal, thereby producing high cooling rates in the casting which in turn leads to microstructural refinement and higher mechanical properties. The objective of this …
-
Development of a photonic band gap structure through titania sol-gel coating of polystyrene spheres
… in a high humidity atmosphere, decreased sample mold thickness, and a sol-gel precursor with large R groups aided in improving the short-range periodicity. dip-coating. Areas of ordered holes separated by thick titania sections were created using dip-coating. The best order was obtained by …
-
Heat transfer and microstructure during the early stages of solidification of metals
… compared with experimental measurements of shell thickness and secondary dendrite arm spacing from this work as well as results reported in the literature. The effects of superheat, alloy composition, chill material, surface roughness and surface film (oil) were investigated. The results indicate …
-
In situ composites of compatibilized polypropylene/liquid crystalline polymer blends
… obtain high mechanical properties from injection molded samples were investigated in this dissertation. Three liquid crystalline polymers (LCPs), two liquid crystalline (LC) copolyesters and one LC poly(ester-amide), were used. The PP/LCP blends were compatibilized with a maleic anhydride grafted …
-
Supramolecular polymer additives to improve the crystallization behavior and optical properties of polybutylene terephthalate and polyamides
… as well as the laser transparency, in injection molded samples. This is the first time semi crystalline polyamides were clarified. The most efficient clarifiers for PA6 were found to decrease the values for haze from nearly 100 % (1.1 mm thick samples) for neat PA6 to 19 % and 11 % at a …