Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results 1 to 2 of 2 for “"nanoindenta-tion"”

  1. High resolution characterisation of H on stress corrosion cracking in nuclear materials

    … under pressurised water reactors (PWR) condi- tions. As the primary method of material degradation, SCC has been studied extensively for several decades, and many factors have been shown to affect SCC susceptibility, these include cold-work, tempera- ture and water chemistry. To develop a …

    oxford Repository record for High resolution characterisation of H on stress corrosion cracking in nuclear materials (opens in a new tab)

  2. Mikrostrukturorientierte Charakterisierung mechanischer Eigenschaften von AlSi10 gelöteten CrNi Stahl/Aluminium Mischverbunden

    … dicken intermetallischen Schichten in der Reaktionszone, welche die mechanischen Eigenschaften der resultierenden Lötverbindungen verschlechtern. Dementsprechend wird ausgehend vom Stand der Technik ein Konzept zur vollständigen Untersuchung der Mikrostruktur-Eigenschafts-Beziehungen der …

    qucosa-diss Repository record for Mikrostrukturorientierte Charakterisierung mechanischer Eigenschaften von AlSi10 gelöteten CrNi Stahl/Aluminium Mischverbunden (opens in a new tab)