Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results 1 to 20 of 70 for “"nickel-base superalloy"”

  1. Thermal Aging Effects on IN718 Plus Nickel-base Superalloy

    Precipitation behavior in IN718Plus superalloy has been studied after heat treatment between 923K to 1123K upto 1000h. Spherical gamma prime (γ’) precipitates transform to plate shaped eta phase (η) upon aging which is important for fatigue design of this alloy. The as received microstructure shows …

    ohiolink Repository record for Thermal Aging Effects on IN718 Plus Nickel-base Superalloy (opens in a new tab)

  2. Hot forging of the nickel-base superalloy ATI 718Plus

    Nickel-base superalloys are widely applied in the hot section of aero engines due to their high temperature capabilities and excellent mechanical properties. For turbine discs, polycrystalline nickel-base superalloys are used where they experience temperatures up to 700ºC and stresses as high as …

    cambridge Repository record for Hot forging of the nickel-base superalloy ATI 718Plus (opens in a new tab)

  3. Life modeling of notched CM247LC DS nickel-base superalloy

    Directionally solidified (DS) nickel-base superalloys are used in high temperature gas turbine engines because of their high yield strength at extreme temperatures and strong low cycle fatigue (LCF) and creep resistance. Costly inspecting, servicing, and replacing of damaged components has …

    gatech Repository record for Life modeling of notched CM247LC DS nickel-base superalloy (opens in a new tab)

  4. On the mesoscale plasticity of nickel-base superalloy single crystals

    … of aeroengines, namely, the so-called Ni-base superalloys. The complex hierarchical structure of these materials means that their macroscopic response is controlled to a great extent by the phenomena that play out on very fine scales, from angstroms (lattice spacing dimension) to …

    oxford Repository record for On the mesoscale plasticity of nickel-base superalloy single crystals (opens in a new tab)

  5. Creep and fatigue of a single crystal nickel base superalloy

    … has led to the development of existing nickel-base superalloys to produce materials with optimum mechanical properties in the single crystal condition. As single crystals are known to be anisotropic, a study is needed to determine the general mechanical properties of these materials, and …

    aston Repository record for Creep and fatigue of a single crystal nickel base superalloy (opens in a new tab)

  6. Fatigue Initiation Fail Mode Classifiation of a Nickel-base Superalloy

    Inconel-718 is a nickel-base superalloy frequently used in aircraft engines and land-based turbines for its high-temperature and corrosion resistance. In this work a large number of fracture surfaces from fatigue specimens of Inconel-718 have been studied with the main purpose to identify and learn …

    chalmers Repository record for Fatigue Initiation Fail Mode Classifiation of a Nickel-base Superalloy (opens in a new tab)

  7. Thermomechanical fatigue behavior of the directionally-solidified nickel-base superalloy CM247LC

    … high temperatures, directionally-solidified (DS) nickel-base superalloys have been used extensively. Complex thermomechanical loading histories makes life prediction for such components difficult and subjective. Costly product inspection and refurbishment, as well as capital expense required in …

    gatech Repository record for Thermomechanical fatigue behavior of the directionally-solidified nickel-base superalloy CM247LC (opens in a new tab)

  8. Reduced order constitutive modeling of a directionally-solidified nickel-base superalloy

    Hot section components of land-based gas turbines are subject to extremely harsh, high temperature environments and require the use of advanced materials. Directionally solidified Ni-base superalloys are often chosen as materials for these hot section components due to their excellent creep …

    gatech Repository record for Reduced order constitutive modeling of a directionally-solidified nickel-base superalloy (opens in a new tab)

  9. Directional Recrystallization of an Additively Manufactured Oxide Dispersion-Strengthened Nickel-Base Superalloy

    This thesis investigates the recrystallization behaviors of an additively manufactured (AM) oxide dispersion-strengthened (ODS) NiCoCr medium entropy alloy, focusing specifically on the effects of a liquid phase, annealing twins, and aluminum microalloying additions on recrystallization kinetics. …

    mit Repository record for Directional Recrystallization of an Additively Manufactured Oxide Dispersion-Strengthened Nickel-Base Superalloy (opens in a new tab)

  10. Transient Liquid Phase bonding in the nickel base superalloy CM 247 LC

    … Phase bonds in the directionally solidified superalloy CM 247 LC with a commercial braze filler material MBF-80 (Ni-Cr-B-C). Specimens were bonded at 1070°C, 1125°C and 1170°C for durations of 15 minutes, 1 hour and 4 hours. The resultant microstructures were then examined metallographically …

    ubc Repository record for Transient Liquid Phase bonding in the nickel base superalloy CM 247 LC (opens in a new tab)

  11. Process development and characterization of an oxide dispersion stabilized nickel base superalloy

    Thesis (Ph.D.)--Massachusetts Institute of Technology, Dept. of Materials Science and Engineering, 1982.

    mit Repository record for Process development and characterization of an oxide dispersion stabilized nickel base superalloy (opens in a new tab)

  12. Micro chip formation mechanism in grinding of Nickel-base superalloy-Inconel 718

    Nickelbasis Superlegierungen werden aufgrund ihrer hervorragenden Eigenschaften in Hochtemperatur- und korrosiven Umgebungen und in der Luftfahrt- und Raumfahrtindustrie als strategische Werkstoffe angesehen. Ihre hervorragenden mechanischen Eigenschaften hingegen reduzieren ihre Schleifbarkeit …

    freiburg-diss Repository record for Micro chip formation mechanism in grinding of Nickel-base superalloy-Inconel 718 (opens in a new tab)

  13. High Performance Thermal Barrier Coatings on Additively Manufactured Nickel Base Superalloy Substrates

    … in thermal barrier coating deposited on AM’ed superalloys. The APS method is used to deposit 7YSZ as the topcoat and NiCrAlY as the bond coat on TruForm 718 substrates fabricated using the direct metal laser sintering (DMLS) method. For comparison, another TBC system with the same topcoat and …

    iupui Repository record for High Performance Thermal Barrier Coatings on Additively Manufactured Nickel Base Superalloy Substrates (opens in a new tab)

  14. Modelling (D022) Precipitate Nucleation, Growth and Coarsening in the Nickel-base Superalloy 625

    … and allowing for them to be shape changing. Based on the Svoboda-Fischer-Fratzl-Kozeschnik (SFFK) framework, the model is calibrated with respect to experimental measurements of aspect ratio evolution at 650°C, with the statistics were acquired through a novel analysis methodology. The …

    whiterose Repository record for Modelling (D022) Precipitate Nucleation, Growth and Coarsening in the Nickel-base Superalloy 625 (opens in a new tab)

  15. Additive Manufacturing of Nickel-Base Superalloy IN939 by Powder Bed Fusion-Laser Beam

    IN939 is a precipitation-hardenable Ni-base superalloy. It has been widely used for blades and vanes in gas turbines, and aircraft engines due to its outstanding properties such as high microstructural stability up to 850 oC, high corrosion, oxidation and creep resistance. Recently, a growing …

    dcu Repository record for Additive Manufacturing of Nickel-Base Superalloy IN939 by Powder Bed Fusion-Laser Beam (opens in a new tab)

Page 1 of 4