Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results 1 to 14 of 14 for “"peeling test"”

  1. Analytical Study on Adhesively Bonded Joints Using Peeling Test and Symmetric Composite Models Based on Bernoulli-Euler and Timoshenko Beam Theories for Elastic and Viscoelastic Materials

    … for viscoelastic materials. One model is for the peeling test of an adhesively bonded joint, which is described using a Timoshenko beam on an elastic foundation. The adherend is considered as a Timoshenko beam, while the adhesive is taken to be a linearly elastic foundation. Three cases are …

    tamu Repository record for Analytical Study on Adhesively Bonded Joints Using Peeling Test and Symmetric Composite Models Based on Bernoulli-Euler and Timoshenko Beam Theories for Elastic and Viscoelastic Materials (opens in a new tab)

  2. Experimental and numerical study of solder ball joints' reliability at package level & board level

    … chip and a PCB. To mimic the real dropping, drop tests are usually used to study the dynamic response of Printed Circuit Board (PCB) as well as the reliability of the solder ball joints in laboratory. In the present thesis, the dynamic responses of the PCB and solder joints are studied by both …

    hkust Repository record for Experimental and numerical study of solder ball joints' reliability at package level & board level (opens in a new tab)

  3. Investigation of Nanomaterial Based Photovoltaic Panel Packaging Materials

    … coating passed the MIL-STD-810G felt abrasion test, 100 cycles of temperature cycling test (-45°C-120°C), heat endurance test (200°C for 500 hours), and UV test (2.7mW/cm2 UVA radiation for 1000 hours). The second PV packaging material investigated is the nano-particle embedded EVA …

    arkansas Repository record for Investigation of Nanomaterial Based Photovoltaic Panel Packaging Materials (opens in a new tab)

  4. The role of surfaces in reprography: the study of toner fixing

    … observation of the fixing states and the tape peeling test failure states showed the direct relation between the fuse quality and the toner fixing states. A physical fusing model was employed to explain the change in the shape of toner particles during the fixing process. The non-uniform fixing …

    vt Repository record for The role of surfaces in reprography: the study of toner fixing (opens in a new tab)

  5. Remoistenable temporary supports for facing of canvas paintings

    … se realizaron pruebas de desprendimiento (peeling test) en diferentes condiciones ambientales para estudiar la fuerza adhesiva de los RTS seleccionados.

    upv Repository record for Remoistenable temporary supports for facing of canvas paintings (opens in a new tab)

  6. Investigation of Magnetic Pulse Welding on Lap Joint of Similar and Dissimilar Materials

    … material joints were examined by lap shearing test, peeling test and microhardness test, and the similar materials joint was also tested by nanoindentation. The joint strength was greater than that of the base metals and the welded region was hardened by high velocity impact. The tensile …

    ohiolink Repository record for Investigation of Magnetic Pulse Welding on Lap Joint of Similar and Dissimilar Materials (opens in a new tab)

  7. Wet Adhesion of Polyvinylamine-Phenylboronic Acid to Cellulose Hydrogel

    … structure and application conditions. The greatest wet adhesion was obtained with 150 kDa PVAm with 16% of the amines bearing phenylboronic moieties. The pH at which the PVAm-PBA was adsorbed onto the cellulose was the dominant process parameter. The specific role of the phenyl boronic groups …

    mcmaster Repository record for Wet Adhesion of Polyvinylamine-Phenylboronic Acid to Cellulose Hydrogel (opens in a new tab)

  8. Delaminační pevnost aortální stěny

    … zde provedeny delaminační experimenty pomocí peelingového testu a jejich výsledky jsou zde porovnány s výsledky známými z literatury.

    cz-tech Repository record for Delaminační pevnost aortální stěny (opens in a new tab)

  9. A Novel Quantitative Mechanical Test of Atherosclerotic Plaque Stability

    … in human atherosclerosis, we also applied peeling tests on human Left Anterior Descending (LAD) coronary arteries to investigate interlaminar adhesive strength of vessels. Our results indicate a significant effect of genotype on measured G values for plaques in apoE knockout (KO) and apoE …

    south-carolina Repository record for A Novel Quantitative Mechanical Test of Atherosclerotic Plaque Stability (opens in a new tab)

  10. Determination of the mechanical properties of the porcine thoracic aorta and an analysis of the stress concentration in fiber reinforced nonlinear solids

    … in two-fiber reinforced materials. We performed peeling experiments on the ascending and the descending segments of the porcine thoracic aorta to evaluate its tearing characteristics. The stretch experienced by the peeled halves, peel force per unit width and peeling energy per unit area reveal …

    tamu Repository record for Determination of the mechanical properties of the porcine thoracic aorta and an analysis of the stress concentration in fiber reinforced nonlinear solids (opens in a new tab)

  11. Study Of The Effect Of The Environmental Relative Humidity On The Angle Dependent Peeling Strength Of Pressure Sensitive Adhesives (PSA)

    … PSA by quantifying material properties, such as peeling strength. The peeling strength is dependent on the composition, viscoelastic properties of the adhesive, and its measurement provides information regarding stickiness and reversibility on different substrates.The work of Kendall and Gent …

    ohiolink Repository record for Study Of The Effect Of The Environmental Relative Humidity On The Angle Dependent Peeling Strength Of Pressure Sensitive Adhesives (PSA) (opens in a new tab)

  12. Delaminační vlastnosti cévní stěny

    … o zdrojích kolísání delaminační síly při peelingovém experimentu. První hypotézou je závislost delaminační síly na šířce čela trhliny a druhou je kolísající složení po délce tepny.

    cz-tech Repository record for Delaminační vlastnosti cévní stěny (opens in a new tab)

  13. Analýza delaminačních testů aorty

    … práce se zabývá analýzou delaminačních testů lidské aorty. Nejprve je v ní popsána disekce aorty jako onemocnění, následně jsou představeny metody zkoumání koheze tepenné stěny. Součástí práce je také popis modelu zákona trakce a separace, na který byla aplikována data získaná z …

    cz-tech Repository record for Analýza delaminačních testů aorty (opens in a new tab)

  14. Fabrication of durable self-healing superhydrophobic coating to improve the performance of high voltage insulators during winter conditions

    … in mechanical properties via tensile and tear tests. The composites containing microcapsules depicted self-healing efficiencies of 67% and 55% calculated based on the recovered toughness and tearing energy of the healed samples. Secondly, a silicone-based superhydrophobic (SHP) coating was …

    uqac