  1. Fatigue Study of Pipeline Steels

    <p>Two types of pipeline steels, Alloy B [Fe-0.05C-1.52Mn-0.12Si-0.092Nb, weight percent (wt.%)] and Alloy C [Fe-0.04C-1.61Mn-0.14Si-0.096Nb, wt.%)], were tested. Vickers hardness and nanoindentation tests were used to obtain the hardness and elastic modulus. Compact-tension (CT) specimens were …

    ut-knoxville Repository record for Fatigue Study of Pipeline Steels (opens in a new tab)

  2. Hydrogen induced damage in pipeline steels

    … (HIC) resistance of several grades of plate steels was investigated using electrolytic hydrogen charging. HIC generated by electrolytic charging was also compared to the industrial standard test for HIC, the NACE standard TM0284. The electrolytic charging (EC) apparatus was designed to …

    colo-mines Repository record for Hydrogen induced damage in pipeline steels (opens in a new tab)

  3. Fatigue crack growth in hydrogen pipeline steels

    Pipeline hydrogen transport and distribution are contemplated for hydrogen applications. Hydrogen introduction in the natural gas pipeline systems is also considered in the power to gas (P2G) approach to utilizing excess renewable energy when the supply exceeds the demand. It is well known that …

    uiuc Repository record for Fatigue crack growth in hydrogen pipeline steels (opens in a new tab)

  4. Inclusion morphology and fracture : toughness of pipeline steels

    … microstructural measurements. Two types of X-70 pipeline steel, one a semi-killed conventional (CON) steel, the other a fully killed and calcium treated for inclusion shape control (CAT) steel were examined in this research. Four stages of hot reduction of the CON steel viz. S2 (38% reduced), S3 …

    ubc Repository record for Inclusion morphology and fracture : toughness of pipeline steels (opens in a new tab) Download PDF for Inclusion morphology and fracture : toughness of pipeline steels (opens in a new tab)

  5. Hydrogen in pipeline steels under electrochemical and gaseous environments

    … compromises the structural integrity of pipeline steels in aqueous and gaseous environments, posing significant challenges to the oil and gas industry. The transition toward a hydrogen economy, driven by global warming concerns, has also highlighted the importance of developing …

    sask Repository record for Hydrogen in pipeline steels under electrochemical and gaseous environments (opens in a new tab) Embargoed until 2027-07-08

  6. TEXTURE CONTROL FOR OPTIMIZING PROPERTIES IN X70 PIPELINE STEELS

    Most pipelines are often designed to serve in rigorous environments for several decades. Failure in pipelines can lead to environmental catastrophe and substantial economic losses. The importance of various microstructural characteristics of pipeline has rarely been considered, and these …

    sask Repository record for TEXTURE CONTROL FOR OPTIMIZING PROPERTIES IN X70 PIPELINE STEELS (opens in a new tab)

  7. Studies of Anisotropic Ductile Fracture Behaviour in Pipeline Steels

    Pipeline steels exhibit various anisotropic properties, which are induced during the metal forming process. These anisotropies can have significant effect on the ductile fracture behavior of the steels. Although, these anisotropic effects are considerable, most damage assessment methodologies adopt …

    carleton Repository record for Studies of Anisotropic Ductile Fracture Behaviour in Pipeline Steels (opens in a new tab)

  8. Advanced hybrid laser welding of pipeline steels using novel technologies

    … weld metal brittleness in more hardenable carbon steels. These limitations can be overcome by adding a filler wire into the weld pool. Meanwhile, novel technologies including beam wobbling and hot-wire feeding have shown the potential to improve the mechanical properties of laser welds. The aim of …

    waterloo Repository record for Advanced hybrid laser welding of pipeline steels using novel technologies (opens in a new tab)

  9. Mechanism of failure by hydrogen-induced cracking in pipeline steels

    Pipeline steels that carry oil and natural gas in severe environments suffer from two important modes of failure: stress corrosion cracking (SCC) and hydrogen-induced cracking (HIC). The SCC has been studied extensively in the literature; however, HIC phenomenon in pipeline steels is less …

    sask Repository record for Mechanism of failure by hydrogen-induced cracking in pipeline steels (opens in a new tab)

  10. Toughness and separation improvement of thick plate X70 pipeline steels

    The effects of microstructure, texture, and material constraint for four American Petroleum Institute (API) X70 grade steel plates of varying thickness (13.5, 15.5, 22, and 32 mm) on separations and the subsequent effects of separations on toughness and toughness anisotropy were evaluated. The …

    colo-mines Repository record for Toughness and separation improvement of thick plate X70 pipeline steels (opens in a new tab)

  11. Mechanical Behavior of Pipeline Steels and an Al0.1CoCrFeNi High-Entropy Alloy

    … part focuses on the mechanical behavior study on pipelines steels. More specifically, the effect of hydrogen on the deformation behavior of the crack tip of an X52 pipeline steel specimen, and the overload effects on the fatigue crack growth of an x70 pipeline weld metal are discussed. For the …

    utk-theses Repository record for Mechanical Behavior of Pipeline Steels and an Al0.1CoCrFeNi High-Entropy Alloy (opens in a new tab)

  12. Hydrogen dissociative adsorption on pipeline steels in high-pressure gaseous environments

    … the pursuit of achieving the net-zero target. Pipeline can serve as an ideal transportation method for H2 due to its high efficiency, large capacity, and relatively low cost. However, H2 pipelines are facing the problem of Hydrogen Embrittlement (HE), which might cause catastrophic failure. …

    calgary Repository record for Hydrogen dissociative adsorption on pipeline steels in high-pressure gaseous environments (opens in a new tab)

  13. Assessment of Tensile Strain Capacity in X70 and X100 Pipeline Steels

    … Tensile Strain Capacities (TSCs) of API 5L steel pipelines, focusing on X70 and X100 grades. It evaluates X70 base metal pipelines with internal or external semi-elliptical cracks and extends to X70 and X100 girth weld pipes under tension and bending conditions. FEA incorporates initiation and …

    carleton Repository record for Assessment of Tensile Strain Capacity in X70 and X100 Pipeline Steels (opens in a new tab)

  14. Simulation of Ductile Fracture in Pipeline Steels Under Varying Constraint Conditions

    … variations on crack tip opening angle (CTOA) of pipeline steels using modified boundary layer (MBL), and (2) to simulate ductile crack propagation in pipeline steels using drop weight tear test (DWTT) and comparing these FE simulations with experimental results. The calibration of various CZM was …

    carleton Repository record for Simulation of Ductile Fracture in Pipeline Steels Under Varying Constraint Conditions (opens in a new tab)

  15. Investigation of hydrogen induced cracking susceptibility of API 5L X65 pipeline steels

    The service environment of oil and gas pipelines often subject them to harsh conditions, such as, very low temperatures, microbial attack, acidic or sour environments etc. These conditions can trigger different failure mechanisms such as corrosion, embrittlement and cracking. The hydrogen induced …

    sask Repository record for Investigation of hydrogen induced cracking susceptibility of API 5L X65 pipeline steels (opens in a new tab)

  16. Effect of tempering on hydrogen induced cracking in accelerated cooled pipeline steels

    Hydrogen induced cracking (HIC) occurs in pipeline steels used in oil and gas applications rich in hydrogen sulfide gas. The presence of high amounts of H2S gas, also known as sour service, allows for ingress of hydrogen and internal cracking in the absence of an externally applied stress. It is …

    colo-mines Repository record for Effect of tempering on hydrogen induced cracking in accelerated cooled pipeline steels (opens in a new tab)

  17. Bauschinger effect in macro and micro sized high strength low alloy pipeline steels

    … in X70, X80 and X100 high strength low alloy pipeline steels were presented. The microstructure of the as-received alloys was characterized. A variety of microstructures was present across the different alloys, ranging from a refined granular ferrite with small amounts of perlite to a bainitic …

    birmingham Download PDF for Bauschinger effect in macro and micro sized high strength low alloy pipeline steels (opens in a new tab)

  18. Influence of crystallographic texture in X70 pipeline steels on toughness anisotropy and delamination

    … texture in four commercially-produced API X70 pipeline steels and their relation to planar anisotropy of toughness and delamination were evaluated. The experimental steels were processed through either a hot strip mill, a Steckel mill, or a compact strip mill. Different processing routes were …

    colo-mines Repository record for Influence of crystallographic texture in X70 pipeline steels on toughness anisotropy and delamination (opens in a new tab)