Global ETD Search
Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.
Results 1 to 20 of 363 for “"premature failure"”
-
Analysis of the premature failure of wind turbine gearbox bearings
… of operating wind turbines due to their high failure rates. Failures occur within 10 % of bearing design life, despite the fact that they are designed to the same bearing standards that satisfactorily predict bearing lifetime in many other industrial applications. No theory has yet been widely …
-
Investigation and analysis of premature failure of valve regulated lead acid batteries
… increase, although up to 40% of VRLA cells fail prematurely. This high failure rate compromises safety and it is also a substantial loss of revenue. The charging and discharging method on a battery is very crucial because it can affect the life span of a battery. When a lead-acid battery is …
-
Macro- and micro-scale modelling of material inhomogeneity for the premature failure of welded 9Cr steels in power plants
… A major global problem of such materials is the premature failure which commonly occurs in the weld regions at elevated temperature. The primary objective of this thesis is the development of a macro- and micro-mechanical framework to predict this premature failure in the 9Cr-1Mo weldments. At …
-
Characteristic influence of thermo-mechanical stresses leading to premature failure of compressor turbine blades of short-haul aircraft fleet
… investigate the life of CT blades only inform of failure after exposure to service with scanty information on the numerous prematurely occurring failures. Consequently, accounting for CT blade life still poses a great challenge to air operators. This research therefore probed characteristic …
-
Strengthening of reinforced concrete elements using carbon fibre
… research is to investigate the prediction of premature failure of RC beams strengthened using CFRP and to propose a reliable and practical design procedure. The premature failures include conventional “shear failure” and anchorage failures of the CFRP laminate. The research will progress based …
-
Stress and Damage Analyses of Thermal Barrier Coatings Under Cyclic Thermal Loading Conditions
The premature failure of the thermal barrier coatings (TBCs) system is a preliminary phenomenon that can significantly limit their applications in gas turbine engines. The delamination of TBCs occurs typically at interfaces between the top coat and bond coat due to thermal mismatch stress via both …
-
Wide bandgap inverter duty bearings : development and lifetime prediction of conductive grease bearings with integrated graphene nanoparticles.
… that lead to system degradation and costly premature failure. A significant application issue of WBG devices in motor drive systems is the premature failure of motor bearings due to an increase in vibration caused by electric discharge machining (EDM) resulting from inverter-induced, high …
-
Shear behavior of prestressed concrete U-beams
… shear capacity. During this phase of testing the premature failure mechanism was isolated as the breakdown of the web-to-flange interface in the end region of the girder. Therefore, the second phase of testing sought to prevent the breakdown of this boundary by three options: (1) increasing the …
-
Applied Statistical Microcontact Model for Prediction of Gear Power Loss
… operating temperatures which can lead to premature failure of components. While experimental data quantifying frictional loses at the gear tooth contact interface exists for varying tooth surface roughness profile combinations, there is poor correlation with existing parametrizations of …
-
Testing a wheeled landing gear system for the TH-57 helicopter.
… analyzed requires modification to eliminate premature failure of the nose wheel attachment tube. Helicopter wheeled landing gear systems
-
Examining the role of copper in electrofusion couplings : implication for PE100 pipe durability
… to catalyse oxidative reactions, leading to premature failure. This study assesses HDPE's thermal and UV degradation in pipelines, particularly examining copper's impact. Results reveal that research-grade HDPE is more susceptible to copper-catalysed degradation than commercial PE100, …
-
Axial Performance of Self-tapping Screws in Mass Timber Products Under Moisture Content Variation
… connections in timber structures. The premature failure of STS during the construction phase has been recently reported by structural engineers and contractors of several mass timber projects in North America due to the increase of the wood's surrounding moisture content. This type of …
-
Multi-hazard performance criteria for non-ductile reinforced concrete frame buildings retrofitted with an FRP column jacketing system
… have non-seismic detailing, which can lead to premature failure under natural and man-made disasters (e.g. earthquakes and blast events). The premature failure can potentially be prevented through the installation of a fiber-reinforced polymer (FRP) column jacketing system. This retrofit system …
-
The influence of cementation on liquefaction resistance of sands
Cohesionless sands are known to be susceptible to failure by liquefaction when they are saturated and subjected to earthquake shaking. Considerable study has been directed towards this subject over the past 20 years in recognition of the possibility of large-scale property damage or loss of life …
-
Development of CAC (Calcium aluminate cement) : GGBFS (Ground granulated blast-furnace slag) blended strain hardening cementitious composite (SHCC) - material behaviour and retrofitting performance
… to microbial induced corrosion which leads to premature failure. With the continued aging of existing concrete pipelines, the demand for rehabilitation of these valuable assets is increasing. In this thesis, an innovative cementitious lining material was developed. Composed of calcium aluminate …
-
Experimental Characterization of Slot Film Cooling Flows With Minimally Intrusive Diagnostics
… active cooling of critical components to prevent premature failure of the system. One such method is film cooling, in which a layer of relatively cool gas is injected near the surface to be protected. This work describes the use of minimally intrusive diagnostics to characterize the kinematics, …
-
Elastodynamic and finite element analysis of coupled lateral-axial vibration of a drillstring with a downhole vibration generator and shock sub
… unwanted vibrations of the drillstring, and thus premature failure of components. The only effective way to benefit from the positive consequences of these tools is to develop vibration models to predict the vibration pattern of the drillstring for any mode of interest, and implement suppression …
-
Investigation into the performance of outdoor insulators under high humidity conditions.
… on the insulator surface, often leading to premature failure. The finite element method program, Maxwcll, was used to simulate the outdoor insulators both under these polluted, wet conditions and under unpolluted conditions. Both cases were simulated for a silicone rubber, glass cap-and-pin …
Page 1 of 19