The Relationship of Microstructure to Fracture and Corrosion Behavior of a Directionally Solidified Superalloy
… microstructural features to these properties. Quantitative fractography was used to determine that the path of cracks during failure of tensile specimens is influenced by the presence of carbides, which are located in the interdendritic regions of the material as dictated by segregation. The …
-
Microstructural origins of variability in the tensile ductility of dual phase steels
Quantitative relationships among processing parameters, microstructure, and material properties are of considerable interest in the context of development of robust processing routes that optimize the required material properties. As a result, the scientific literature contains a large number of …
-
Creep fracture and some low-alloy steels.
… probably occurred by vacancy transport. Detailed quantitative fractography has yielded empirical laws governing the nucleation and growth of such cavities which show some similarities to those suggested for the phenomenon in single phase materials. It was demonstrated that remaining creep life was …
-
Effects of microstructure and strain rate on deformation behavior in advanced high strength steels
… of failure in these steels. However, very few quantitative studies have been done to understand these mechanisms of failure. Therefore, the objective of this study was to quantitatively understand the effects of microstructure and strain rate on the deformation behavior of three different …
-
Microstructure development and fatigue crack growth studies on high-carbon plate-martensite austenite microstructures
… grains size (PAGS), plate-martensite and RA was quantitatively characterized. Lower austenitizing temperatures and shorter hold times resulted in the greatest PAGS refinement as well as refinement in plate-martensite and RA constituent size. Multiple thermal cycling did not further refine the …
-
Effects of strain rate on mechanical properties and fracture mechanisms in dual phase steels
… the objective of this work is to investigate and quantitatively characterize the fracture surfaces of DP steels generated under a wide range of strain rates and gain an understanding on the microstructure-based fracture mechanisms. Four DP steels, of two nominal strength levels (590 MPa and 980 …
-
Šíření dlouhých únavových trhlin v austenitické oceli při smykových módech II a III
Práce je zaměřena na realizaci experimentu umožňujícího současné zatěžování vzorku kruhového průřezu ve smykových módech II a III. Postup experimentu byl navržen tak, aby byl co nejvíce potlačen vliv zavíraní trhliny při cyklickém zatěžování a získané prahové hodnoty rozkmitu faktoru intenzity …
-
Propagation of Fatigue Cracks under Shear Loading Modes II, III and II+III in the Near-Threshold Region
Práce je zaměřena na šíření únavových trhlin v módech II, III a II + III v prahové oblasti v kovových materiálech. Byly provedeny experimenty pro ARMCO železo, titan, nikl a austenitickou ocel na třech druzích vzorků pro zatěžování trhliny ve smykových módech. Byl použit zvláštní způsob vytváření …