Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results 1 to 13 of 13 for “"reheat cracking"”

  1. Reheat cracking susceptibility in welds of creep resistant alloys for power generation applications

    … may be susceptible to stress relaxation cracking (SRC) or strain age cracking (SAC) during post weld heat treatment (PWHT) or service. These reheat cracking (RC) phenomena are attributed to a combination of susceptible microstructures, sufficiently high tensile residual stress and …

    colo-mines Repository record for Reheat cracking susceptibility in welds of creep resistant alloys for power generation applications (opens in a new tab)

  2. An investigation of reheat cracking in the weld heat affected zone of type 347 stainless steel

    Reheat cracking has been a persistent problem for many alloys such as the stabilized stainless steels: Types 321 and 347 and Cr-Mo-V steels as well as Ni-base superalloys termed “strain-age cracking”. Cracking occurs during PWHT at the HAZ. Many investigations have been conducted on the RHC with …

    ohiolink Repository record for An investigation of reheat cracking in the weld heat affected zone of type 347 stainless steel (opens in a new tab)

  3. Fundamental studies of the metallurgical causes for reheat cracking in 1 1/4Cr-1/2Mo, 2 1/4Cr-1Mo and Cu precipitation hardenable steels and means of mitigating the potential problem

    … are considered to be susceptible to weld related reheat cracking. This study was instituted to determine the mechanisms for reheat cracking in these steels as well as to determine methods to successfully avoid reheat cracking. Two heats of 1 1/4Cr-1/2Mo, one being calcium treated: three heats of 2 …

    utk-theses Repository record for Fundamental studies of the metallurgical causes for reheat cracking in 1 1/4Cr-1/2Mo, 2 1/4Cr-1Mo and Cu precipitation hardenable steels and means of mitigating the potential problem (opens in a new tab)

  4. Development and Use of a Simple Test Method to Evaluate Reheat Cracking Sensitivity in the Weld Deposit Region of a Submerged Arc Weld

    … have recently noted the occurrence of reheat cracking in the weld deposits of 2¼[ two and one fourth]Cr‑1Mo‑¼[one fourth]V (22V) during the fabrication of pressure vessels used in the petrochemical industry. Due to increased oversight now required during fabrication of already expensive …

    ut-knoxville Repository record for Development and Use of a Simple Test Method to Evaluate Reheat Cracking Sensitivity in the Weld Deposit Region of a Submerged Arc Weld (opens in a new tab)

  5. Effect of PWHT and filler metal on stress relaxation cracking susceptibility in 347H stainless steel welds for elevated temperature service

    … reported to be susceptible to stress-relaxation cracking (SRC) within months or years of service. Without prior stress relief via post weld heat treatment (PWHT), stress relaxation cracking may occur. The welded heat-affected zone (HAZ) and fusion zone (FZ) of 347H SS, particularly in thick …

    colo-mines Repository record for Effect of PWHT and filler metal on stress relaxation cracking susceptibility in 347H stainless steel welds for elevated temperature service (opens in a new tab)

  6. The effect of welding conditions on the low temperature transformation and properties of the Weld HAZ of low alloy steels for use in light water reactors

    … used in Light Water Reactor construction, preheat for welding, and in some instances, the maintenance of preheat after welding, is employed to avoid fabrication problems. The employment of preheat is aimed primarily at the elimination of HAZ cracking, which is normally attributed to cold …

    ut-knoxville Repository record for The effect of welding conditions on the low temperature transformation and properties of the Weld HAZ of low alloy steels for use in light water reactors (opens in a new tab)

  7. Weldability Evaluation of Naval Steels

    … Temperature (DRT) of 1303°C. The 148°C Liquation Cracking Temperature Range (LCTR) indicated moderate HAZ liquation cracking susceptibility. This finding was attributed to microstructural evidence suggesting a fully austenitic phase transformation sequence at elevated temperatures, compositional …

    ohiolink Repository record for Weldability Evaluation of Naval Steels (opens in a new tab)

  8. Characterization of the Fine-Scale Weld Deposit Microstructure and its Influence on the Elevated Temperature Properties of 2.25Cr - 1Mo - 0.25V Weldments in Heavy Wall Pressure Vessels

    … of the microstructure on creep behavior and reheat cracking susceptibility. Scanning electron microscopy and transmission electron microscopy examinations concentrated on carbide morphology and evolution as a function of time and temperature, since the majority of properties that are …

    utk-theses Repository record for Characterization of the Fine-Scale Weld Deposit Microstructure and its Influence on the Elevated Temperature Properties of 2.25Cr - 1Mo - 0.25V Weldments in Heavy Wall Pressure Vessels (opens in a new tab)

  9. Temper-bead/half-bead/control deposition repair welding techniques used for low alloy and Cr-Mo steels

    … conducted using optical light microscopy. The reheat cracking tendency of the weld HAZ for each of the three heats of material was evaluated using spiral notched transverse weld specimens with both small (0.125" dia.) and large (0.350" dia.) diameter samples. Gleeble thermal simulation was …

    ut-knoxville Repository record for Temper-bead/half-bead/control deposition repair welding techniques used for low alloy and Cr-Mo steels (opens in a new tab)

  10. Stress Relief Cracking in Low Alloy Creep Resistant Steels

    Stress Relief Cracking (SRC) in low alloy steels was the core focus for this work. Stress relief cracking is an ongoing concern for thick-walled creep resistant steel welds during PWHT when high restraint and high residual stresses are present after welding. While much is already known about SRC, …

    ohiolink Repository record for Stress Relief Cracking in Low Alloy Creep Resistant Steels (opens in a new tab)

  11. Phase Transformation Behavior and Stress Relief Cracking Susceptibility in Creep Resistant Steels

    Cracking has been reported in newly constructed water wall panels of fossil power plants during startup testing. Both high hardness (exceeding 350 HV) and high levels of welding residual stress have been reported in welds of waterwall panels made of T23 and T24 steels. Stress-relief cracking (SRC) …

    ohiolink Repository record for Phase Transformation Behavior and Stress Relief Cracking Susceptibility in Creep Resistant Steels (opens in a new tab)