DEVELOPMENT OF PRECIPITATION HARDENABLE AL-SC-ZR-HF QUATERNARY ALLOYS THROUGH THERMODYNAMIC MODELING, AND ROOM-TEMPERATURE AND ELEVATED TEMPERATURE HARDNESS
… heat treatment, two compositions showed a secondary room-temperature hardness peak up to 700 MPa at 450°C. Elevated temperature hardness profiles also indicated an increase in hardness from 200-300°C, attributed to the precipitation of Al3Sc, however, no secondary hardness response was …
-
Microstructural investigation of D2 tool steel during rapid solidification
… increases. In the case of powders, the optimum hardness after heat treatment is achieved at different temperatures for constant periods of time. Higher supersaturation of austenite results in obtaining secondary hardness at higher annealing temperature. D2 steel ingots generated using spray …
-
A study of carbide reactions during the tempering of high speed steels
… compositions of extracted carbide residues, and hardness and metallographic constitution (particularly as revealed by selective carbide etchants) of the steel itself. Supplementary work is described regarding similar experiments carried out on hot die steel and on two special high vanadium …
-
Tepelné zpracování nástrojových ocelí ve vakuu
Bakalářská práce se zabývá studiem vlivu ochlazovacího prostředí na popouštěcí křivku nástrojové ledeburitické oceli pro práci za studena X210Cr12. Ocel byla tepelně zpracovávána ve vakuové peci s možností kalení do oleje. V rámci práce byly zkoumány vzorky kalené z teploty 1060 °C, popuštěné při …