The Electrical and Mechanical Properties of Electrographite-Metal Interfaces
… of the interface; frictional force, wear rate and contact resistance, were measured, and have been explained by physical changes occurring at the interface. Three wear regimes were encountered, mild wear, severe wear and catastrophic wear The wear mechanisms involved in these regimes …
-
Investigation on the mechanism of wear of single crystal diamond tool in nanometric cutting of iron using molecular dynamics (MD) and the development of generalized potential energy surfaces (GPES) base on ab initio calculations
… the hardest of all materials known, undergoes severe wear in the machining of iron. This is because of the strong chemical affinity of iron towards carbon. However, the micro-mechanisms of wear are not well understood. A review of literature indicates graphitization of diamond as the leading …
-
The effect of elevated temperature on the wear of stainless steel in contact with tungsten carbide
… The work described was initiated to isolate the wear mechanisms of two such steels in contact with tungsten carbide at temperatures up to 500° C. Experiments were carried out on angular contact bearings similar to these used in service, where both rolling and sliding is present and also for pure …
-
Oxidational and Tribological Studies of Austenitic Stainless steels under CO2-Based Environments
… and environments of air and CO,. The wear of the AISI 316 steels is shown to be transitional, changing from mild to severe wear about a transition load. For the AISI 310 steels no such transitional behaviour is observed; a severe mode of wear is encountered for all conditions. High …
-
An experimental investigation of wear behavior of ultra-high molecular weight polyethylene under sliding motion
… cycles. The tests are carried out with the wear specimen lubricated by deionized water. The purpose is to produce delamination, which is the severe wear condition in Ultra-High Molecular Weight Polyethylene (UHMWPE), the material used for the articulating surfaces in orthopedics under …
-
Παραγωγή σύνθετων επικαλύψεων με την τεχνική ηλεκτρικού τόξου και ιδιότητες αυτών: Αυτολιπαινόμενες επικαλύψεις με στερεά λιπαντικά και κεραμικά σωματίδια
… of this study are the fabrication and the anti-wear properties investigation of Metal Matrix Composite coatings on plain steel (St52). Gas Tungsten Arc and Plasma Transferred Arc techniques were used to produce these coatings, whereas ceramic reinforcement particles (TiC, WC, NbC) and solid …
-
Desarrollo de superficies determinísticas inspiradas en piel de serpiente mediante técnicas de texturizado mecánico para aplicaciones tribológicas
… surface with great ease and without suffering severe wear, the skin of this species was evaluated as the organ responsible of these characteristics in order to apply this knowledge to the design of artificial surfaces for high energy consumption and high wear applications. The first part of …
-
Dental Analysis of the Prevalence of Caries and Infection in the Ancient Maya of K’Axob, Belize
… of these remains for caries, infection, and wear, this study aims to analyze the prevalence of these dental pathologies and their correlations to one another among other factors. Caries were found to be present in 80 (76.2%) of the 105 individuals and infection was seen in 16 (15.2%) of the …
-
The wear and thermo-elastohydrodynamic behavior of thrust washer bearings under non-axisymmetric loads
… the thrust washer bearing often distresses severely and unpredictably, causing transmission breakdown and liability issues. A specially designed thrust washer bearing test rig allows for controlled variation of the operational parameters (speed, load, lubrication flow rate, etc.) governing …
-
Φθορά κινητού ένθετου πολυαιθυλενίου σε ολική αρθροπλαστική γόνατος: κλινική και πειραματική μελέτη
We studied the wear of the Rotaglide mobile polyethylene bearings following experimental and clinical use. At 5 million cycles and with the same simulation system, the mobile bearings exhibited up to four times less wear than the fixed IB inserts, which were tested at the same time. We also studied …
-
The Effect of Oil Properties on Engine Oil Pump Failure Mechanisms
… economy is attributed to the high friction and wear of various engine components. Thus, the automotive industry aims to design fuel efficient vehicles in order to reduce the fuel consumption. A Variable Displacement Vane Pump (hereafter denoted VDVP) is an innovative type of oil pump that has a …
-
Avaliação das diferenças entre bolas forjadas e bolas fundidas no processo de moagem
The differences in grinding capacity and wear between cast iron balls and forged steel balls was investigated based on grinding efficiency and wear experiments conducted in a mill with dimensions 0.3048m x 0.3048. The sample utilized, designated as concentrator feed, presented d50 of 210m and …
-
Análise tribológica de conjugados (CrAl)N depositados por PAPVD sobre ferramentas de metal duro com diferentes rugosidades superficiais
… tooling for high hardness materials machining. Wear and its tribological consequences when modifying the initial roughness of the substract is the subject of this paper. Hardmetal (WC 95%-Co 5%) was submitted to three different roughness by grinding and polishing. Sandpaper and polishing were …
-
Modeling the origins of adhesive wear across scales
Friction and wear occur at every interface between solid materials. In the design of mechanical devices, it is desirable to be able to quantify and control the amount of friction and wear, as well as predict their evolution with time. ``Tribology'' is the science looking at interactive surfaces in …
-
Desgaste em recobrimentos duplex e monocamada a base de WC-Co
The abrasive wear of a WC12Co/NiCrAl two layer coating, single layer WC12Co, and single layer 50%(WC12Co)50%(NiCr) on the as deposited and melted conditions was studied. The tests were performed at two different conditions, called mild wearand severe wear. Samples of the substrate material, AISI …
-
Caracterização do comportamento de desgaste de cerâmicas de alumina densa : efeitos de parâmetros do ensaio do tipo pino no disco
Searching for wear resistant materials, attention has been paid to Si3N4, SiC, Al2O3 and ZrO2 ceramics due to their better properties as compared to other materials. Although ceramic are brittleness, improvements on the processing and by the addition of second phases to the ceramic matrix have …
-
Investigation of Glaze Formation in Reciprocating Wear of Superalloys
… and harsh operating conditions lead to wear in aero-engine components such as the disc-blade interface. Under dry sliding conditions, metal-to-metal contact leads to adhesive transfer and wear because of their similar chemical properties. To reduce this, dissimilar material combinations …
-
Desgaste de um rotor de ferro fundido cinzento revestido com camada de metal duro após 1.000 horas de bombeamento de vinhoto operando na condição de cavitação
… The aim of this work was investigate the main wear mechanisms of an impeller and parts of a centrifugal pump after pumping vinasse treated in reactor (pH 8,3±0,7). A tungsten carbide-cobalt (WC10Co4%Cr) film based hard metal of 360±35μm μm was applied on the grey cast iron pump impeller by HVOF …
-
Development of new ceramic nano-composites for the next generation prosthetic devices
… regard, which offer the potential for the lowest wear rate and therefore the longest lifespan. The strength and toughness of ceramic prostheses have been greatly enhanced through the emergence of a zirconia toughened alumina (ZTA) composite. However, there remains a clear drive to reduce fracture …
-
Efeito da fragilização por hidrogênio exsitu no comportamento tribológico dos aços SAE 1045, AISI 304 e AISI 316
… of the coefficient of friction (COF), specific wear rate, 2D profilometry, Vickers microhardness, X-ray diffraction (XRD), optical microscopy, and scanning electron microscopy (SEM). The results demonstrated that the tribological response is strongly influenced by the crystal structure. The SAE …