  1. IMPLEMENTATION OF CRACK-REDUCING TECHNOLOGIES FOR CONCRETE IN BRIDGE DECKS: SYNTHETIC FIBERS, INTERNAL CURING, AND SHRINKAGE-REDUCING ADMIXTURES

    … to reduce cracking in bridge decks, including shrinkage-reducing admixtures (SRAs), shrinkage-compensating admixtures (SCAs), fiber reinforcement, and internal curing (IC), are evaluated based on laboratory tests of concrete mixtures with and without slag cement and silica fume and the cracking …

    ku Repository record for IMPLEMENTATION OF CRACK-REDUCING TECHNOLOGIES FOR CONCRETE IN BRIDGE DECKS: SYNTHETIC FIBERS, INTERNAL CURING, AND SHRINKAGE-REDUCING ADMIXTURES (opens in a new tab)

  2. Controlling Cracks in Bridge Decks

    … oxide-based (CaO) or magnesium oxide-based (MgO) shrinkage compensating admixtures or expansive additives (SCA) with LC-HPC. A modified version of ASTM C157 in which length-change measurements begin 5½ ± ½ hr after casting concrete is developed and used to evaluate swelling and shrinkage including …

    ku Repository record for Controlling Cracks in Bridge Decks (opens in a new tab)

  3. EFFECT OF CRACK-REDUCING TECHNOLOGIES AND SUPPLEMENTARY CEMENTITIOUS MATERIALS ON SETTLEMENT CRACKING OF PLASTIC CONCRETE AND DURABILITY PERFORMANCE OF HARDENED CONCRETE

    … mixtures containing internal curing (IC), a shrinkage reducing admixture (SRA), optimized and non-optimized aggregate gradations, or the supplementary cementitious materials (SCMs) slag cement and silica fume. Some concrete mixtures contained combinations of these technologies, such as …

    ku Repository record for EFFECT OF CRACK-REDUCING TECHNOLOGIES AND SUPPLEMENTARY CEMENTITIOUS MATERIALS ON SETTLEMENT CRACKING OF PLASTIC CONCRETE AND DURABILITY PERFORMANCE OF HARDENED CONCRETE (opens in a new tab)