Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results

Showing 1 to 20 of 45 for “"solidification cracking"”.

  1. Solidification Cracking in Low Alloy Steel Weld Metals

    … variables, particularly speed, on weld metal solidification cracking. This has involved low alloy steels to specifications En24, SAE4130, ASTM A387B, and several aircraft steels. Existing relationships between composition and cracking have been critically examined, and an improved expression, …

    aston Download PDF for Solidification Cracking in Low Alloy Steel Weld Metals (opens in a new tab)

  2. Solidification cracking resistance of high strength aluminum alloys

    … Hence the evaluation of fracture toughness (cracking resistance) at different parts of ingot is very much essential to understand the propagation of cracks in ingots.;The objective of this research was to determine the cracking resistance of Al 2024 (Al-Cu-Mg) and Al 3004 (Al-Mn-Mg) alloys …

    wvu Repository record for Solidification cracking resistance of high strength aluminum alloys (opens in a new tab)

  3. SOLIDIFICATION CRACKING IN ADDITIVELY MANUFACTURED HIGH ENTROPY ALLOY NiCrCoFe WITH V OR W

    … Although the alloy was designed to minimize solidification cracking, cracking was still observed in the alloy. This research seeks to examine the cracking mechanisms in HEA produced with wire additive manufacturing.

    mtu Repository record for SOLIDIFICATION CRACKING IN ADDITIVELY MANUFACTURED HIGH ENTROPY ALLOY NiCrCoFe WITH V OR W (opens in a new tab)

  4. The Effects of Composition on Weld Solidification Cracking in Low Alloy High Tensile Steels

    … of the effects of material composition on weld solidification cracking in the TIG arc welding of thin alloy steel sheet. The main points of this study included the effects of - oxygen, manganese, Mn/S and 0/S ratios on the sulphur induced cracking, and the possibility of predicting crack …

    aston Repository record for The Effects of Composition on Weld Solidification Cracking in Low Alloy High Tensile Steels (opens in a new tab) Download PDF for The Effects of Composition on Weld Solidification Cracking in Low Alloy High Tensile Steels (opens in a new tab)

  5. Solidification Cracking in Binary Al-Cu Alloys Additively Manufactured through Laser Powder Bed Fusion

    … alloys with a high susceptibility to micro-cracking during solidification cannot be feasibly manufactured through LPBF, such as in selected high-strength Al-alloys. The cracking susceptibility (CS) of Al-alloys varies with composition, so modeling CS with respect to composition is crucial in …

    ucf Repository record for Solidification Cracking in Binary Al-Cu Alloys Additively Manufactured through Laser Powder Bed Fusion (opens in a new tab)

  6. Weldability and microstructural analysis of nuclear grade austenitic stainless steels

    … evaluated the hot ductility response, and hot cracking susceptibility (fusion zone solidification cracking and HAZ liquation cracking) of modified nuclear grade and standard austenitic stainless steels. Extensive microstructural characterization using state-of-the art analytical electron …

    utk-theses Repository record for Weldability and microstructural analysis of nuclear grade austenitic stainless steels (opens in a new tab)

  7. Stresses in heavy section electroslag joining

    … reports on the process indicates that although solidification cracking ought to be a problem, apparently it is not routinely observed. Welding conditions which are known to produce solidification cracks in Electroslag Welding with wire electrodes were reported to make crack-free welds using ESJ …

    ubc Repository record for Stresses in heavy section electroslag joining (opens in a new tab) Download PDF for Stresses in heavy section electroslag joining (opens in a new tab)

  8. Microstructure development and weldability of inoculated 6061 processed with gas metal arc directed energy deposition

    … additive manufacturing (AM) due to extensive solidification cracking. Recently, it has been shown that adding nucleation sites, also called inoculants, to high strength aluminum alloys results in grain refinement and elimination of solidification cracking during additive manufacturing. These …

    colo-mines Repository record for Microstructure development and weldability of inoculated 6061 processed with gas metal arc directed energy deposition (opens in a new tab)

  9. Understanding Solidification Behavior of Selected Aluminum and Magnesium Alloys Additively Manufactured by Laser Powder Bed Fusion

    … dense with AM due to the consequence of solidification cracking. Thus, a large knowledge gap remains in assessing already existing, and genesis of new alloys that can be processed dense by AM, without solidification cracking. The present work investigates the AM processing and …

    ucf Repository record for Understanding Solidification Behavior of Selected Aluminum and Magnesium Alloys Additively Manufactured by Laser Powder Bed Fusion (opens in a new tab)

  10. Effect of oxygen on the gas tungsten arc weldability of laser-powder bed fusion fabricated 304L stainless steel, The

    … via laser-powder bed fusion would affect the cracking response during gas tungsten arc welding. Weldability and solidification studies were performed on 304L stainless steel material produced via the laser-powder bed fusion process and compared with the behavior of wrought material. It was …

    colo-mines Repository record for Effect of oxygen on the gas tungsten arc weldability of laser-powder bed fusion fabricated 304L stainless steel, The (opens in a new tab)

  11. Influence of reaction synthesis feedstocks on solidification defect formation and microstructure-property relationships in electron beam freeform fabrication of aluminum metal matrix composites

    … can also minimize the propensity for solidification cracking that certain Al alloys possess as a result of large solidification temperature ranges and high coefficients of thermal expansion. To overcome the limitations of conventional manufacturing processes, additive manufacturing …

    colo-mines Repository record for Influence of reaction synthesis feedstocks on solidification defect formation and microstructure-property relationships in electron beam freeform fabrication of aluminum metal matrix composites (opens in a new tab)

  12. NICKEL SUPERALLOY COMPOSITION AND PROCESS OPTIMIZATION FOR IMPROVED WELDABILITY

    … and elastic modulus values, but with increased solidification cracking susceptibility. The 7Co-3Ti alloy maintained elastic modulus values and room temperature hardness, and had increased strain-age cracking resistance.

    mtu Repository record for NICKEL SUPERALLOY COMPOSITION AND PROCESS OPTIMIZATION FOR IMPROVED WELDABILITY (opens in a new tab)

  13. Towards elucidating the process-structure-performance relationships of lightweight structural alloys

    … are fusion-based, relying on melting and solidification, which can lead to poor mechanical performance due to intense thermal gradients leading to solidification cracking and columnar dendritic grain growth. Additive Friction Stir-Deposition (AFS-D) is a novel technique that implements …

    alabama Repository record for Towards elucidating the process-structure-performance relationships of lightweight structural alloys (opens in a new tab)

  14. Al-Ce-Mn Solidification Phase Selection and Solid-State Phase Transformations

    … are prone to processing related defects such as solidification cracking. The Al-10Si-Mg alloy was initially adopted because of its resistance to solidification cracking. However, the Al-10Si-Mg alloy has reduced tensile properties especially at high temperatures, where the silicon phase coarsens …

    utk-theses Repository record for Al-Ce-Mn Solidification Phase Selection and Solid-State Phase Transformations (opens in a new tab)

  15. Fiber laser weldability of austenitic nickel alloys

    … at laser powers ranging from 400 to 600 Watts. Solidification cracking was observed in cross-sections of the fusion zone of HR-160® alloy and HR-120® alloy. Dendritic solidification was found in all alloys, and partitioning within the dendritic structure compared well with Scheil calculations …

    colo-mines Repository record for Fiber laser weldability of austenitic nickel alloys (opens in a new tab)

  16. NICKEL SUPERALLOY COMPOSITION AND PROCESS OPTIMIZATION FOR WELDABILITY, COST, AND STRENGTH

    … Composition 1 alloy was scaled up to assess weld solidification cracking resistance compared to baseline nickel superalloys. It was found that the Optimized Composition 1 alloy has decreased cost, increased weldability, and comparable strength to Nimonic 263. With further testing, this alloy may …

    mtu Repository record for NICKEL SUPERALLOY COMPOSITION AND PROCESS OPTIMIZATION FOR WELDABILITY, COST, AND STRENGTH (opens in a new tab)

  17. Development of an Aluminum Multi-Material via Sequential Additive Friction Stir Deposition and Wire Arc Additive Manufacturing

    … aluminum alloy 6061, which is prone to solidification cracking. Current AFSD machines are limited to 3-axis deposition, which limits capabilities within the printing process. Robotic WAAM has multi-axis deposition capabilities but must use aluminum filler wire, such as aluminum alloy …

    ut-knoxville Repository record for Development of an Aluminum Multi-Material via Sequential Additive Friction Stir Deposition and Wire Arc Additive Manufacturing (opens in a new tab)

  18. Microstructure and Defects of AA6061 in the Laser Powder Bed Fusion Additive Manufacturing

    … (LPBF) additive manufacturing is restricted by solidification cracking and porosity. This study examines defect formation, microstructural evolution, and precipitate behavior in AA6061 processed under various LPBF conditions, including room temperature and heated substrates (500°C), as well as …

    south-carolina Repository record for Microstructure and Defects of AA6061 in the Laser Powder Bed Fusion Additive Manufacturing (opens in a new tab)

  19. Investigation into the Effects of Heat Treatment and Nanoparticles on the Microstructure and Mechanical Properties of LPBF'ed AlSi10MgAlloy

    … traditional columnar grains, which are prone to solidification cracking, into more equiaxed, strain-tolerant structures. The enhanced strength in as built parts was attributed to grain refinement, dislocation strengthening, and secondary-phase particle strengthening due to the addition of …

    carleton Repository record for Investigation into the Effects of Heat Treatment and Nanoparticles on the Microstructure and Mechanical Properties of LPBF'ed AlSi10MgAlloy (opens in a new tab)

Page 1 of 3