Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results

Showing 1 to 20 of 26 for “"solution annealing"”.

  1. Grain Boundary Engineering of Stainless Steel Via Additive Manufacturing

    … treatment, 0-30% cold-rolling, and a 1150°C solution annealing treatment were systematically applied to 316L stainless steel samples produced by laser powder bed fusion. The resulting microstructures were analyzed, including calculations of the special boundary and triple junction statistics, …

    alabama Repository record for Grain Boundary Engineering of Stainless Steel Via Additive Manufacturing (opens in a new tab)

  2. High-resolution characterisation of strengthening effects in nickel-based superalloy Alloy 718

    … 718 turbine discs involves multi-step forging, solution annealing, and dual ageing. Direct ageing is an alternative process to achieve yield strength increments of > 10 % by omitting solution annealing. However, the detailed processing-microstructure-property relationships during direct ageing …

    unsw Repository record for High-resolution characterisation of strengthening effects in nickel-based superalloy Alloy 718 (opens in a new tab)

  3. The development of qualification standards for cast duplex stainless steel

    … study of the effectiveness of existing foundry solution annealing procedures for producing cast DSS without intermetallic phases were implemented. In the ASTM E562 study, 5 samples were extracted from various cast austenitic and DSS in order to have varying amounts of ferrite. Each sample was …

    ut-knoxville Repository record for The development of qualification standards for cast duplex stainless steel (opens in a new tab)

  4. Efeito de múltiplos ciclos de solubilização sub-solvus delta e envelhecimento na microestrutura e propriedades mecânicas da superliga 718

    … submitted to successive cycles of sub-solvus δ solution annealing (954°C/1h) and aging (760°C/5h + 649°C/1h). Forged and cast samples had its microstructures observed by optical and scanning electron microscopes with the identification of precipitates made by the morphologies. Grain size …

    brazil-uerj Repository record for Efeito de múltiplos ciclos de solubilização sub-solvus delta e envelhecimento na microestrutura e propriedades mecânicas da superliga 718 (opens in a new tab)

  5. Influence of alloying and processing on the degradation behaviour of Mg-Zn based alloys

    … act as cathodes until 24 h immersion. After solution annealing, the more homogeneous microstructure and reduced galvanic couples resulted in a higher corrosion resistance in Mg-Zn-Ca. In contrast, the intrinsic impurities (Fe and Si) started to dominate the corrosion behaviour of Mg-0.5Zn …

    cau-kiel Repository record for Influence of alloying and processing on the degradation behaviour of Mg-Zn based alloys (opens in a new tab)

  6. Atmospheric pitting corrosion of stainless steel

    … direction and plane of the metal surface. Solution annealing of stainless steel resulted in ferrite reduction and formation of faceted pits. Pits can grow with an initial shallow dish, which may propagate via ‘earring’ or small satellite pits. The size and morphology were seen to vary with …

    birmingham Download PDF for Atmospheric pitting corrosion of stainless steel (opens in a new tab)

  7. The Use of Optical In-Situ Data of Tensile Samples to Model Porosity for Part Qualification of AM 316L

    … the ability of hot isostatic pressing (HIP) and solution annealing (SA) to mitigate pore effects and produce a part that achieves acceptable tensile properties. Two control samples with no purposeful porosity included were also built to compare the tensile results within the build to an ideal …

    ut-knoxville Repository record for The Use of Optical In-Situ Data of Tensile Samples to Model Porosity for Part Qualification of AM 316L (opens in a new tab)

  8. A Study on NiTiSn Low-Temperature Shape Memory Alloys and the Processing of NiTiHf High-Temperature Shape Memory Alloys

    … NiTi was examined along with the effects of solution annealing, Ni:Ti ratio adjustments, and precipitation strengthening on the thermomechanical properties of NiTiSn LTSMAs. Second, the thermomechanical processability of NiTiHf high-temperature SMA (HTSMA) wires is presented. The evolution of …

    unt Repository record for A Study on NiTiSn Low-Temperature Shape Memory Alloys and the Processing of NiTiHf High-Temperature Shape Memory Alloys (opens in a new tab)

  9. Additive manufacturing of Ni-rich nitinol for superelastic properties for stent application

    … properties. Heat treatments, including solution annealing and ageing, play a critical role in reducing residual stresses, refining the microstructure, and tuning the phase transformation temperatures which enable setting the superelastic response required for stent applications. …

    dcu Download PDF for Additive manufacturing of Ni-rich nitinol for superelastic properties for stent application (opens in a new tab)

  10. Modeling and characterization of mechanical properties in laser powder bed fusion additive manufactured Inconel 718

    … compression and tensile samples was subjected to solution annealing and double aging heat treatment. Tensile, compressive and hardness properties were measured in as built and heat-treated condition. Compressive properties were also characterized in the machined condition to understand the …

    colo-mines Repository record for Modeling and characterization of mechanical properties in laser powder bed fusion additive manufactured Inconel 718 (opens in a new tab)

  11. Influence of Processing Parameters, Feedstock and Heat Treatment on the Microstructure of PBF-LB 316L Stainless Steel

    … (GA) were subjected to stress relieving (SR) and solution annealing (SA) and a combination of these treatments. Microstructural evolution was characterized primarily using light optical microscopy (LOM) and quantitative image analysis, with selected samples additionally characterized by EBSD. The …

    chalmers Repository record for Influence of Processing Parameters, Feedstock and Heat Treatment on the Microstructure of PBF-LB 316L Stainless Steel (opens in a new tab)

  12. THE EFFECT OF POST PROCESSING ON THE MECHANICAL PROPERTIES AND FRACTURE MECHANISMS OF ALSI10MG PRODUCED THROUGH SELECTIVE LASER MELTING

    … water quenching is not adequate. Currently, annealing for a stress relief treatment is the only post- processing measure that does not involve water quenching. This project studied a novel direct HIP approach, whereby an argon quench is used after solution annealing. Three different cooling …

    mcmaster Repository record for THE EFFECT OF POST PROCESSING ON THE MECHANICAL PROPERTIES AND FRACTURE MECHANISMS OF ALSI10MG PRODUCED THROUGH SELECTIVE LASER MELTING (opens in a new tab)

  13. Analysis of Additively Manufactured 17-4PH Stainless Steel

    … of selective laser melting systems state that solution annealing and precipitation hardening will achieve traditional mechanical properties, thereby removing all retained austenite. Once again, it is not clear, how the recommended solution and precipitation treatments lead to the desired …

    mcmaster Repository record for Analysis of Additively Manufactured 17-4PH Stainless Steel (opens in a new tab)

  14. Improved process procedures for upgrading and repair of high alloy and stainless castings

    … A 494 - 94. Effects of autogenous GTA welding, solution annealing temperature and cooling rate after the solution soak, were also evaluated.</p> <p>Test results show that cast materials generally have lower critical pitting temperatures than their wrought counterparts, but have comparable …

    ut-knoxville Repository record for Improved process procedures for upgrading and repair of high alloy and stainless castings (opens in a new tab)

  15. Processing-Structure-Property Relationships in Directly Aged Alloy 718

    … turbine disks. The direct ageing route where solution annealing after forging is omitted is preferred in the aerospace industry not only for being more economical but also for achieving superior yield strength in comparison to conventional routes. However, to meet increasing demands from the …

    unsw Repository record for Processing-Structure-Property Relationships in Directly Aged Alloy 718 (opens in a new tab)

  16. Very high cycle fatigue behavior of laser beam-powder bed fused Inconel 718 considering the layer orientation and surface finish effects

    … the build plate, and subjected to a post-process solution annealing and aging heat treatment. In addition, specimens were testing in both the as-built and post-process machined condition. Fatigue response of LB-PBF Inconel 718 was compared to that of wrought Inconel 718. Comparison of the …

    unf Repository record for Very high cycle fatigue behavior of laser beam-powder bed fused Inconel 718 considering the layer orientation and surface finish effects (opens in a new tab) Download PDF for Very high cycle fatigue behavior of laser beam-powder bed fused Inconel 718 considering the layer orientation and surface finish effects (opens in a new tab)

  17. Minimization of residual stresses in the closure -weld region of the spent nuclear fuel canisters using induction annealing process

    … highly nonlinear and is best solved in a single solution using a coupled formulation. The results of the two-dimensional axisymmetric model were almost identical to the results of the three-dimensional model. Therefore, the computationally efficient two-dimensional axisymmetric model was used for …

    unlv Repository record for Minimization of residual stresses in the closure -weld region of the spent nuclear fuel canisters using induction annealing process (opens in a new tab) Download PDF for Minimization of residual stresses in the closure -weld region of the spent nuclear fuel canisters using induction annealing process (opens in a new tab)

  18. SHAPE MEMORY BEHAVIOR OF NiTiHf ALLOYS FABRICATED BY LASER POWDER BED FUSION

    … in three conditions: (i) as-fabricated, (ii) solution annealed and (iii) aged (550 oC for 3h), where the transformation temperatures (TTs), shape memory strains and superelasticity were quantified. After solution annealing, TTs and hysteresis were decreased while aging resulted in higher TTs …

    uky-thes Repository record for SHAPE MEMORY BEHAVIOR OF NiTiHf ALLOYS FABRICATED BY LASER POWDER BED FUSION (opens in a new tab)

  19. Zuverlässigkeit von ausscheidungshärtbaren und martensitischen Stählen im additiv gefertigten Zustand unter hochzyklischer mechanischer Beanspruchung

    … similar behavior: Heat treatment in the form of solution annealing and aging results in a comparable microstructure for all material states considered. Irregularities present in the material are not only inhomogeneous in space but also logarithmically normally distributed in size. The …

    qucosa-diss

  20. Polarization and corrosion behavior of 316L stainless steel and alloy AL6X in acid chloride environments

    … on the pitting resistance of AL6X was confirmed. Solution annealing in the range of 2050°F-2450°F did not affect the pitting resistance but when solution annealed at 1950°F, Sigma phase formation along the grain boundary was associated with pit initiation. A series of experiments was conducted to …

    ut-knoxville Repository record for Polarization and corrosion behavior of 316L stainless steel and alloy AL6X in acid chloride environments (opens in a new tab)

Page 1 of 2