Global ETD Search
Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.
Results 1 to 20 of 46 for “"specific wear rate"”
-
Influence of voltage oscillation pulse-off time in a doms on the properties of hard hydrogen-free DLC coatings for the automotive industry.
… previously carried out at CEMMPRE where substrate bias was optimized (-80 V) at 124 µs of oscillation pulse-off time. In this work, DLC coatings were deposited by deep oscillations magnetron sputtering (DOMS), a variant of high power magnetron sputtering (HiPIMS). The main objective is to …
-
Produção por fusão seletiva a laser de revestimentos resistentes ao desgaste utilizando a liga Fe68Cr8Mo4Nb4B16
… and excellent resistance against corrosion and wear. The application of these alloys as protective coatings can increase the service life of engineering components operating in aggressive environments. Besides presenting interesting combinations between physical and chemical properties, these …
-
Wear modelling of diamond-like carbon coatings against steel in deionised water
… coatings used to reduce friction and minimise wear in a wide range of applications. The focus of this work is the use of DLC coatings within Rolls-Royce’s pressurised water reactors. A strong understanding of material behaviour in this environment is compulsory due to the stringent safety …
-
Development of new ceramic nano-composites for the next generation prosthetic devices
… regard, which offer the potential for the lowest wear rate and therefore the longest lifespan. The strength and toughness of ceramic prostheses have been greatly enhanced through the emergence of a zirconia toughened alumina (ZTA) composite. However, there remains a clear drive to reduce fracture …
-
Characterization of Tribological Properties of Ti-6Al-4V Fabricated by Electron Beam Powder Bed Fusion
… tribological performance of EB-PBF Ti-6Al-4V, specifically, wear and erosion behavior, in relation to process-induced variability and powder reuse. While EB-PBF components are adopted in wear-critical structures in aerospace, biomedical, and possibly oil-and-gas industries, limited knowledge of …
-
The efficacy of Hibiscus sabdariffa as a fibre-reinforcement material for denture base acrylic resins
… resins. The flexural strength, impact strength, specific wear rate, hardness and water absorption behaviour were determined in line with ASTM D 790 and D 256, G 99, D 2583 and D 570 methods of testing, respectively. Parametric and non-parametric tests were used to analyse the mean differences (p …
-
Two-body abrasion and synergy in abrasion-corrosion of martensitic and complex phase steel
… from North sea. A significant influence of wear over corrosion was observed however, the influence of corrosion over wear was very negligible. In general, martensitic steel performed slightly better than dual phase steel in all the media except seawater. Additionally, abrasion was studied in …
-
Development and Characterization of PFA-PAEK Polymer Blends as a Melt-Processible Candidate Material for High Temperature, Tribological Applications
… (PFA-PAEK) polymer blends, specifically PFA-polyetheretherketone (PFA-PEEK) and PFA-polyetherketoneketone (PFA-PEKK), as melt-processible alternatives to polytetrafluoroethylene-PEEK (PTFE-PEEK) systems. Specifically formulated PTFE-PEEK offers high temperature usage and …
-
COLD SPRAY ALUMINUM 7075 FUNCTIONALLY GRADED COATING REINFORCED WITH BORON NITRIDE NANOPLATELETS AND VARYING VOLUMETRIC BORON CARBIDE LOADS
… AA7075, which the DoD uses extensively. This specific alloy has been used in many of its aerospace applications due to its excellent specific strength, fatigue resistance, and relative light weight, while being cost efficient. However, AA7075 is susceptible to abrasion due to having low wear …
-
Oxidation and wear behaviour of a work roll grade high speed steel
… mixture of dry air and water vapour flowing at a rate of 0.45 or 1.45 cm'/min respectively, compared to dry air conditions. At 615'C and for the maximum water vapour content, the oxidation behaviour was initially logarithmic followed by linear stage. In contrast, for a water vapour flow rate of …
-
Tribological properties of a tightly woven carbon-carbon composite
… the C/C composite. The friction coefficient and wear rate were determined as functions of applied load, sliding speed, sliding distance and lubrication in ambient laboratory conditions. Mean friction coefficient of the composite was 0.135 æ when tested at ambient atmosphere and 0.113 æ in …
-
Manufatura aditiva por fusão de leito de pó a laser de aço inoxidável 316L com adições de boro: avaliação das propriedades de corrosão e desgaste
Adding boron to stainless steels improves wear resistance through the formation of Cr- and Mo-rich borides but may cause sensitization. Enhancing wear without compromising corrosion resistance requires adjusting the alloy’s global composition. This thesis aims to modify 316L stainless steel, known …
-
Efeitos da microestrutura, direção de construção e formação de defeitos nas propriedades de flexão e desgaste do aço ferramenta H13 processado por fusão em leito de pó a laser
… powder bed fusion behaved during bending and wear tests, correlating this behavior with microstructure, build direction, and formed defects. The microstructure revealed a cellular morphology of martensite surrounded by retained austenite. The bending tests demonstrated a high sensitivity to …
-
Electroplated composite coatings with incorporated nano particles for tribological systems with the focus on water lubrication
… the development of novel materials with better wear or corrosion performance in the adjoining water environment. This applies to broad oceanic applications, for example, marine vessels, conventional power plants, tidal and wave energy systems and other water-lubricated industrial bearings. The …
-
Surface modification of additively manufactured metallic components
… processes. Yet, functional surfaces generated in AM have to be often finish machined because of their relatively inferior roughness. The first phase of this research worked around this limitation by tailoring the topography of an AM surface in-process to entail textures that further …
-
Efeito da fragilização por hidrogênio exsitu no comportamento tribológico dos aços SAE 1045, AISI 304 e AISI 316
… transition drives the use of hydrogen as a strategic vector for industrial decarbonization. However, the interaction of hydrogen with metals results in hydrogen embrittlement (HE), altering their mechanical properties. Although widely studied, there remains a gap in understanding the impacts …
-
Comportamento tribológico de revestimentos do tipo DLC-W depositados por DCMS e HiPIMS
… best tribological behavior, having the lowest specific wear rate of all coatings. tested independently of service conditions, while showing friction coefficient values, and showing wear mechanisms identical to the others.
-
The influence of hydrogen gas exposure and low temperature on the tribological characteristics of ti-6al-4v
… Average friction coefficients and the specific wear rate were calculated from the test data. Also high-resolution digital microscope imaging was used to observe and characterize the wear mechanisms of the four groups of samples. Results show that hydrogen exposure facilitated adhesive …
-
Produção de recobrimentos resistentes ao desgaste através de laser cladding de pós das ligas amorfizáveis fe-co-nb-b-(y)
… can be subjected to a high level of surface wear it necessary to search for new wear-resistant alloys to improve the performance and safety of the components. The objective of this work was to produce laser coatings with high hardness and high wear resistance. Three new vitreous alloys of the …
-
Wear and Friction Modelling of Carbon Fiber Reinforced Epoxy Composites
The wear resistance of unidirectional carbon fiber reinforced epoxy under severe abrasive sliding conditions was studied. It was found that unidirectional laminates tested with the fibers parallel to the sliding direction (UDp) were more wear resistant under the same set of test conditions when …
Page 1 of 3