Development of a gleeble based test for post weld heat treatment cracking in nickel alloys
… to the various forms of postweld heat treatment cracking, including stress-relief cracking and strain-age cracking. Materials evaluated include Waspaloy and Alloy 718. Samples are initially given an elevated temperature thermal exposure that simulates the weld HAZ. Upon cooling from elevated …
-
NICKEL SUPERALLOY COMPOSITION AND PROCESS OPTIMIZATION FOR IMPROVED WELDABILITY
… values, but with increased solidification cracking susceptibility. The 7Co-3Ti alloy maintained elastic modulus values and room temperature hardness, and had increased strain-age cracking resistance.
-
Investigation of hot cracking in additive manufactured nickel-base superalloys
… Ni-base superalloys, are susceptible to cracking during both AM processing and subsequent densification and/or heat treatment. Therefore, to fully utilize the potential that AM offers, it is crucial to optimize the manufacturing process in order to minimize the amount of defects in the …
-
An investigation of reheat cracking in the weld heat affected zone of type 347 stainless steel
Reheat cracking has been a persistent problem for many alloys such as the stabilized stainless steels: Types 321 and 347 and Cr-Mo-V steels as well as Ni-base superalloys termed “strain-age cracking”. Cracking occurs during PWHT at the HAZ. Many investigations have been conducted on the RHC with …
-
Phase Transformation Behavior and Stress Relief Cracking Susceptibility in Creep Resistant Steels
Cracking has been reported in newly constructed water wall panels of fossil power plants during startup testing. Both high hardness (exceeding 350 HV) and high levels of welding residual stress have been reported in welds of waterwall panels made of T23 and T24 steels. Stress-relief cracking (SRC) …
-
Reheat cracking susceptibility in welds of creep resistant alloys for power generation applications
… pressure vessels, and thermal energy storage (TES) tanks may utilize austenitic stainless steel (SS) alloys, e.g. type 347H, 347AP (347LN), and Therma 4910 (316LNB). Higher temperature components(>720°C), such as supercritical CO2 primary heat exchangers (PHX), may require nickel base …