Removal of inclusions from cast superalloy revert
It is known that the recycling of superalloy scrap causes the mechanical properties and the casting performance of reverted alloys to deteriorate. This is due to contamination of the alloy by inclusions. The contaminants affect the microstructure of the casting in terms of modification of MC …
-
Structure-property relations in superalloy single crystals
… is concerned with a single crystal nickel-base superalloy which has been developed for application as a high pressure turbine blade material in jet aircraft engines. The microstructures and mechanical properties of superalloys, including the effects of heat-treatments, have been reviewed.</p> …
-
Deformation studies near hard particles in a superalloy
<p>Superalloys have performed well as blade and disc materials in turbine engines due to their exceptional elevated temperature strength, high resistance to creep, oxidation and corrosion as well as good fracture toughness. This study explores the use of a relatively new technique of strain …
-
Effect of Etchants on Superalloy HIP Oxide Scales
… When manufacturing parts in nickel-based superalloy Inconel 718 oxides can form during hot isostatic pressing. These oxides need to be removed from the part to meet standards. This is done in a two-step etching process, pickling and etching. In this project different pickling solutions are …
-
Heat Treatment Optimization for Nickel-based Cast Superalloy
Nickel-based superalloys are broadly used in the aerospace industry for applications at elevated service temperatures. Haynes 282 is a recently developed, gamma-prime (γ ′ ) strengthened, nickel-based superalloy that can be manufactured in different ways, such as wrought methods, powder methods, …
-
Time-dependend fracture mechanics characterization of HAYNES HR160 superalloy
… the q in the da/dt versus C*(t) relationship for superalloy HR160 and can be used as a reference for q when long-term test results are predicted from short-term tests.</p>
-
Fiber laser welding of nickel-based superalloy Inconel 718
Inconel 718 (IN 718) is widely used in applications, such as aircraft and power turbine components. Recently, fiber laser welding has become an attractive joining technique in industry for fabrication and repair of service-damaged components. However, a major limitation in the laser welding of IN …
-
NICKEL SUPERALLOY COMPOSITION AND PROCESS OPTIMIZATION FOR IMPROVED WELDABILITY
… and high temperature environments. Nickel superalloys are a viable option, but are expensive and are difficult to weld, leading to joint failures. The goal of this project is to experimentally evaluate computationally-designed nickel superalloys for increased weldability and decreased alloy …
-
Development of Multicomponent EAM Potential for Ni-Based Superalloy
… Aluminides and Carbides, key phases in Ni-based Superalloys. The goal is to utilize the MD simulation to understand the deformation dynamics that contribute to the formation of voids and creep initiation. For this purpose, we constructed the raw data from ab-initio (molecular dynamics) MD …
-
Shielding Effectiveness of Superalloy, Aluminum, and Mumetal Shielding Tapes
… 1 GHz. The three shielding tapes used included superalloy, aluminum, and mumetal. Calculations for Shielding Effectiveness involve the computation of Absorption Loss, Reflection Loss, and Re-Reflection Correction Factor. From the outcome of the calculations, it was suitable to conclude that all …
-
Life modeling of notched CM247LC DS nickel-base superalloy
Directionally solidified (DS) nickel-base superalloys are used in high temperature gas turbine engines because of their high yield strength at extreme temperatures and strong low cycle fatigue (LCF) and creep resistance. Costly inspecting, servicing, and replacing of damaged components has …
-
Thermo-mechanical fatigue crack growth of a polycrystalline superalloy
… the fatigue crack growth rate of polycrystalline superalloy IN100. Temperature interaction testing was performed by cycling between 316°C and 649°C in blocks of 1, 10 and 100 cycles. Load interaction testing in the form of single overloads was performed at 316°C and 649°C. After compiling a …
-
Characterization of linear friction welded in-service Inconel 718 superalloy
… process to manufacture or repair of Inconel® 718 superalloy (IN 718) aero engine BLISKs. This was achieved by simulating a LFW joint made of virgin (V) and in-service (IS) (from samples extracted from an actual turbine disk) IN 718 material. An in-depth microstructural characterization of the V …
-
Metal-Mold Reactions in CMSX-4 Single Crystal Superalloy Castings
Metal-mold reaction (MMR) layers are often found on the surface of as-cast CMSX-4 single-crystal alloy parts. These layers cannot be removed prior to solution heat treatment of cast parts because of the sensitivity of the single-crystal castings to recrystallization (RX) defect formation. Removal …
-
Creep and fatigue of a single crystal nickel base superalloy
… led to the development of existing nickel-base superalloys to produce materials with optimum mechanical properties in the single crystal condition. As single crystals are known to be anisotropic, a study is needed to determine the general mechanical properties of these materials, and determine …