Global ETD Search
Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.
Results
Showing 1 to 20 of 426 for “"superalloys"”.
-
Fracture studies in superalloys
<p>This research is concerned with the effects of temperature and frequency on the fatigue crack propagation behaviour. The fatigue behaviour at elevated temperature has been reviewed with emphasis on the mechanisms of propagation proposed to explain the effects of temperature and frequency.</p> …
-
The freckling mechanism of superalloys
… defects which are usually found in nickel-base superalloys or specialty steels and which occur during solidification. They are presently one of the major defects encountered in advanced casting technology of superalloys. Two modified Rayleigh criteria have been suggested which seem best adapted …
-
Banding in nickel-base superalloys and steels
Process irregularities in remelting furnace operation have an impact on the ingot solidification structure which depends on the local thermal conditions and the alloy concerned. In this work, a laboratory investigation into the structures resulting from interruptions in solid growth is presented in …
-
Fatigue life prediction on nickel base superalloys
Neural networks have been used extensively in material science with varying success.It has been demonstrated that they can be very effective at predicting mechanical properties such as yield strength and ultimate tensile strength. These networks require large amounts of input data in order to learn …
-
The spray forming of Ni based superalloys
… <p>Samples of two spray formed Ni superalloys, MAR-M-002 and UDIMET 720, have been re-heated into the solid/liquid region and the fully solid region just below the solidus temperature for a series of times to try and reproduce the situation of grain growth in a spray formed deposit. …
-
Investment Casting of Thin Sections in Superalloys
… complex components through investment casting of superalloys is extremely important for producing turbine blades. Often, the sharp corners in the castings will not fill completely, resulting in unintentionally rounded corner which must be machined to achieve the final, required dimensions. By …
-
Hierarchical multiscale modeling of Ni-base superalloys
Ni-base superalloys are widely used in hot sections of gas turbine engines due to the high resistance to fatigue and creep at elevated temperatures. Due to the demands for improved performance and efficiency in applications of the superalloys, new and improved higher temperature alloy systems are …
-
Fatigue damage accumulation in nickel base superalloys.
Tangentially oriented Waspaloy specimens taken from the bore section of a turbine disc were subjected to low cycle fatigue in the form of cyclic four point bend tests. Substantial differences in grain size and structure occurred across the section of the disc. Fatigue damage occurred primarily as a …
-
Composition effects on macroscopic solidification segregation of superalloys
… macrosegregation, i.e. freckles, in superalloys. First, the freckling mechanism of superalloys is developed using the physical simulation of freckle formation in specially designed model alloys. It is found that freckles originate from dendrite irregularities at the solidification …
-
Direct Laser Metal Deposition Of Nickel Based Superalloys
Nickel-based superalloys are substantially used in the manufacturing of boilers for ultra-supercritical power plants and gas turbine hot-section as this grade of alloys provide higher yield strength with the rise in operating temperature and pressure owing to the presence of γʹ second phase …
-
Isothermal oxidation comparison of three Ni-based superalloys
Ni-based superalloys are used for high-temperature components of gas turbines in both industrial and aerospace applications due to their ability to maintain dimensional stability under conditions of high stress and strain. The oxidation resistance of these alloys often dictates their service …
-
Constitutive modeling of creep of single crystal superalloys
… describe the creep deformation of single crystal superalloys. The con- stitutive model that is developed here is based on the fact that as bodies deform the stress free state that corresponds to the current configuration (referred to as the "natural configuration", i.e., the configuration that the …
-
Microstructural Instabilities in Nickel-based Single Crystal Superalloys
Single crystal superalloys, mostly Nickel-based, have been, so far, the material of choice for high-temperature applications, such as gas turbine blades. Single crystalline turbine blades are usually cast in the direction, providing the best combination of properties. While misorientations up to …
-
Updated Force Model for Milling Nickel-based Superalloys
Nickel-based superalloys are commonly used in applications which require high strength and resistance to creep and oxidation in extreme conditions. All nickel-based superalloys are considered difficult to machine; however, cast gamma-prime-strengthened nickel-based superalloys are more difficult to …
-
Modelling of thermo-mechanical fatigue behavior in superalloys
Thermo-mechanical fatigue (TMF) and isothermal fatigue (IF) behavior of coated and uncoated Mar-M247 and, uncoated Mar-M246 was studied. The Mar-M247 was coated with Alpak-S1. The coating consists of a manganese and Aluminium powder slurry that is applied by painting, dipping, or spraying with an …
-
Laser Powder Bed Fusion of Nickel-based Superalloys
… the manufacturability of nickel-based superalloys, IN625 and IN718, using the laser powder bed fusion (LPBF) process. The study provides a better understanding of the process-structure-property of nickel-based superalloys, their fatigue life, and subsequent post-processing. First, the …
Page 1 of 22