Shear bond strengths of two new self-etching primers
… were bonded with a stainless steel button using Transbond XT composite. The bonding agents were iBOND, G-Bond, Transbond Plus SEP and Transbond XT primer (control). SBS’s immediately, 24hours and 3months were measured with their Adhesive Remnant Index (ARI). Results: Transbond XT primer …
-
An in vivo and in vitro study of a new orthodontic bonding agent
… three groups brackets were bonded with Concise, Transbond XT, or APC Plus and debonded 30 minutes after bonding. In the second three groups, brackets were bonded with Concise, Transbond XT, or Concise and debonded after thermocycling. The in vivo study consisted of 31 patients and a split arch …
-
Resistencia al cizallamiento e índice adhesivo remanente (ARI) utilizando primers hidrofílico e hidrofóbico expuestos a contaminación con agua y saliva
… (ARI) de dos tipos de primers: hidrofílico (Transbond™ MIP) e hidrofóbico (Transbond™ XT Light Cure Adhesive y Rely-a-bond®) sobre esmalte de dientes bovino expuestos a contaminación (agua y saliva) y sin contaminación. Materiales y Métodos: Se utilizaron 99 incisivos permanentes de bovino y …
-
Abrasions- und Adhäsiv-Verhalten fließfähiger Komposite im Rahmen der kieferorthopädischen Langzeitretention
… untersucht. Die Materialien Filtek Supreme XT, Transbond LR, Transbond Supreme LV, Tetric EvoFlow, Venus Diamond Flow, Vertise Flow, Gradia Direct LoFlo sind im ersten Teil auf Volumenverlust und Tiefenverlust sowohl nach 150.000 als auch nach 300.000 Zyklen getestet worden. Durch die …
-
Wear of Orthodontic Bite Turbos and Opposing Enamel
… as bite turbos. 8 specimens (10x8x4 mm) each of Transbond LR (3M), Transbond Plus (3M) and Triad gel (Dentsply) were prepared in silicone molds and light cured for 30 seconds using an Acteon Satelec Blue Ray 3 (420-480 nm, 3,000 mW/cm2 ± 10%). The specimens were wet polished to 2,000 grit SiC …
-
Color Characterization of Color Changing Orthodontic Adhesives
… Color Change by American Orthodontics and Transbond PLUS by 3M Unitek were evaluated. As a non-color changing control, Transbond XT by 3M Unitek was analyzed. A teflonTeflon mold was used to fabricate uniform discs of adhesives (n=10/adhesive). A spectrophotometer was used to analyze the …
-
Bracket Bond Strength Effects of Incorporation of NovaMin into an Orthodontic Bonding Resin
… into a commercially available resin, TransBond LV. Resin discs were immersed in 5 mL of both deionized water and lactic acid (pH~5). Calcium ion concentrations were measured using a calcium-selective electrode. Solutions were replaced every 24 hours for the first week, then remained …
-
Bonding Orthodontic Brackets to Stainless Steel Crowns
… (2): Aluminablasting + Silane Coupling Agent + Transbond; (3): Diamond Bur Abrasion + Metal Primer + Assure; (4): Diamond Bur Abrasion + Silane Coupling Agent + Transbond; (5: control): Acid Etching + Metal Primer + Assure; (6: control): Acid Etching + Silane Coupling Agent + Transbond. Bond …
-
Untersuchungen der Scher-Abschäl-Festigkeit von kieferorthopädischen Brackets nach Kariesinfiltration - in vitro Studie an bovinen Schmelzflächen
… der Kariesinfiltrant Icon® und das Adhäsivsystem Transbond™ XT. Nach individueller Vorbehandlung der gesunden und demineralisierten Schmelzflächen mit und ohne Transbond™ XT Primer, Icon® (eine Versuchsreihe mit anschließendem Thermocycling) oder Kombination beider Materialien, wurden die Brackets …
-
Orthodontic Bond Strength Comparison Between Two Filled Resin Sealants
… or sealant. Group 1, the control group, used Transbond XT Primer (3M Unitek). Groups 2 and 3 were prepared with the sealants L.E.D. Pro Seal (Reliance Orthodontic Products) and Opal Seal (Opal Orthodontics) respectively. Transbond XT Adhesive was applied to a stainless steel bracket and bonded …
-
Evaluation of shear/peel bond strengths of orthodontic attachments to moist and dry enamel
… as 24 hours vs. 6 months and were as follows: Transbond(tm) XT/dry (10.57 +- 2.83 MPa vs 12.23 +- 3.14 MPa), Assure(tm)/dry (6.93 +- 2.2 MPa vs 8.18 +- 1.39 MPa), Smartbond(R)/dry (3.91 +- 1.17 MPa vs 4.11 +- 1.96 MPa), Transbond(tm) XT/moist (0.14 +- 0.31 MPa vs 0 +- 0 MPa), Assure(tm)/moist …
-
Bond Strengths of Three Orthodontic Adhesives for Direct and Indirect Bonding
… this fairly new indirect adhesive with 3M's Transbond XT and Reliance's Rely-A-Bond. Two hundred and seventy freshly extracted bovine teeth were mounted in acrylic resin and divided into 18 groups of 15 teeth each. Nine groups were bonded indirectly and nine groups were bonded directly. The …
-
Effect of Shear Bond Strength with Novel APC™ Flash-Free Brackets and Different Bonding Protocol: An In Vitro Study
… Coated bracket bonded with phosphoric acid etch, Transbond™ MIP, Group 2 ceramic APC™ Flash-Free adhesive bracket with phosphoric acid etch and Transbond™ MIP, Group 3 ceramic APC™ Flash-Free adhesive bracket bonded with Transbond™ plus, Group 4 ceramic APC™ Flash-Free adhesive bracket bonded with …
-
Translucency, stain resistance and hardness of composites used for Invisalign attachments
… and three orthodontic adhesives (L.C.R.™, Transbond™ XT, Phase II® Dual Cure) were used in this in-vitro study. 2.0 mm thick samples of each material were fabricated in silicone molds covered with a flat sheet of Invisalign attachment template material. To evaluate the translucency …
-
Work of Fracture in Ceramic Bracket Bonding Systems
… was then bonded with either Gren Gloo or Transbond XT. After bonding, the specimens were debonded with a newly developed Instron-like machine. Results: Titanium brackets bonded with Gren Gloo exhibit higher displacement, shear bond strength (SBS) and work of fracture than all other bracket …
-
A Comparison of the Failure Rate of Two Orthodontic Light-Curable Adhesives: A Chart Review
… available bracket adhesive systems such as Transbond XT™ (3M™ Company, St. Paul, MN) which is often used as a gold standard to compare other adhesive systems. Comparing Transbond XT™ to BracePaste® and finding favorable results may provide evidence of an effective alternative to the highly …
-
The Influence of Work of Fracture on Six Orthodontic Bonding Systems
… with one of the following adhesives, Gren Gloo, Transbond XT or Glass lonomer. After bonding, the specimens were stored in distilled water at room temperature for 72 hours. The brackets were then debonded with a high-resolution tensile testing device and then assigned an Adhesive Remnant Index …
-
An In Vitro Comparison of Shear Bond Strength Between Two Orthodontic Light-Curable Adhesive Pastes
… BracePaste compared to that of the conventional “Transbond XT” adhesive. Additionally, enamel and bracket interfaces were examined to determine the location of bond failure and the tooth surfaces were visually examined to assess severity of enamel marks and the presence of remaining adhesives on …
-
Effect of a Hydrophilic Bonding Agent on Shear Bond Strength to Water and Saliva Contaminated Enamel
… Recently, a hydrophilic ethanol-based primer (Transbond MIP Moisture Insensitive Primer) has been developed and may show improvements to conventional resin adhesives in moisture contaminated conditions. Sixty extracted human premolar teeth were randomly assigned into four groups of 15. In Group …
-
Vergleich der Scherhaftfestigkeiten von Adhäsiven für kieferorthopädische Befestigungselemente nach DIN 13990-1/ -2
… 2\. die Scherhaftfestigkeit der Adhäsive Transbond XT, Beauty Ortho Bond und Fuji Ortho LC unter unterschiedlichen Ätzbedingungen zu bestimmen Methode Die Schmelzoberfläche wurde im ersten Versuchsteil nach Herstellerangaben konditioniert. Im zweiten Versuchsteil wurde die …