Global ETD Search
Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.
Results 1 to 14 of 14 for “"veneering porcelain"”
-
Influence of surface treatment on veneering porcelain shear bond strength to zirconia after cyclic loading
… to suffer from chipping or cracking of the veneering porcelain (VP) as the most common complication. There is little information in the literature regarding the influence of surface treatment on VP shear bond strength to Y-TZP after cyclic loading. Purpose of this study: The goals of this …
-
Factors Affecting the Fracture Strength and Fatigue Resistance of Molar Crowns Produced Using a Zirconia-based System
… be attributed to either inferior strength of the veneering porcelain or weakness in the zirconia-veneer bond. The aims of this in-vitro project were to analyze some of the factors that can influence the performance of zirconia-based molar crowns and to characterize the zirconia-veneer interface. …
-
Keramische Kronen auf Zähnen und Implantaten
… zirconia single crowns with a sintered veneering cap. In this prospective study 118 patients with a total of 220 single crowns placed on 106 teeth (69 vital teeth, 37 endodontically treated teeth) and 114 implants in molar and premolar regions were examined during a mean observation …
-
Effect of veneering technique, heat rate, holding time and zirconia thickness on the mechanical properties of porcelain veneers
OBJECTIVES: Evaluate the effect of different veneering techniques, Y-TZP core thicknesses, and firing cycles with different heat rates and holding times on the mechanical properties of veneering porcelain. MATERIALS AND METHODS: Biaxial flexural strength and Thermal shock resistance tests were …
-
Interaction between enamel, porcelain and a gold alloy: an in vitro wear study.
… restorative materials such as gold alloy or porcelain have been used for many years to restore excessively worn teeth, the procedures are generally complex and challenging to the dentists as well as costly and time-consuming for the patients. A good restorative material should be aesthetic, …
-
Fracture resistance of three-unit posterior zirconium dioxide fixed partial dentures : an in vitro study
… All frameworks were veneered with VITA VM®9 veneering porcelain. Half of the specimens of each group were loaded in an artificial mouth for 1.2 million cycles to simulate 5 years of clinical function. No fracture occurred during artificial aging. Then, all samples were subjected to the …
-
Mechanical and Microstructural Properties of Monolithic Zirconia
… being used for monolithic crowns without veneering porcelain. However, there is a lack of scientific information regarding whether or not monolithic zirconia crowns can function with sufficient durability, especially in the molar regions. The overall aim of this thesis was to analyze …
-
Wear of ceramics and enamel in a chewing simulator
… comparison was made between different zirconia, veneering porcelain (Ceramco 3) and natural enamel. Additionally, the surface roughness (Ra) of the ceramic surface was measured before and after wear testing to evaluate effect of cyclic loading on the t-m phase transformation. Materials and …
-
Reliability and failure modes of anterior zirconium-oxide crowns dependent on coping design
… Reliasoft). Results: Chipping of the veneering porcelain was the main failure mode in both groups. Nine specimens showed areas of delamination. The mean loads at failure were 313 ± 82 N (n=6) for group S and 367 ± 123 N (n=6) for group A (profile 1). The use level probability Weibull …
-
Effect of surface treatment on porcelain bond strength to titanium
… to evaluate the bond strength of a low fusing veneering porcelain fired on Titanium grade V with different surface treatments. MATERIALS & METHODS: One hundred and twenty bars of Titanium grade V (25±1x 3±0.5x 0.5±0.05mm) were divided randomly into twelve groups: group 1 no surface treatment, …
-
Fatigue Strength of Bi-layered Ceramics Under Cyclic Loading as a Function of Core Veneer Thickness Ratios
… 29, 42, 40, 48, respectively). IPS e.max Ceram veneering porcelain was used as directed. Thicknesses of both un-veneered cores and veneered specimens were controlled by a ceramic machinist (BOMAS Machine Specialties). All specimens were adhesively cemented with Multilink Automix (Ivoclar) to …
-
Comparison of Metal-Ceramic Bond Strengths of Four Noble Alloys using Press-on-Metal (PoM) and Conventional Layering Techniques
… of bond strength tests to the adoption of a porcelain adherence test where bond strengths were not evaluated, and then back to the current bond strength test that has been adopted by the American Dental Association as Standard No. 38, which is a modification of International Organization for …
-
Untersuchung zur lagerbedingten Änderung des Haftverbundes zwischen Titan und verschiedenen Keramiken mit und ohne Bonder
Die Zielsetzung der vorliegenden Untersuchungen war es, den Einfluss unterschiedlicher Lagerungsbedingungen auf den Haftverbund zwischen Titan und Verblendkeramik zu untersuchen, wobei die jeweilige Verblendkeramik mit Bonder und ohne Bonder untersucht wurde. Untersucht wurde die Vita Titankeramik …
-
Klinische Bewährung von Procera® AllCeram Kronen nach einem Zeitraum von 10 Jahren
Procera® AllCeram Kronen werden seit 1997 an der Zahnklinik der Freien Universität in Berlin hergestellt, eingesetzt und evaluiert. Bei insgesamt 36 Patienten wurden 74 Kronen mit diesem Herstellungsverfahren eingegliedert und 2009, nach einem Zeitraum von zwölf Jahren unter Funktion für diese …