Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results 1 to 6 of 6 for “"zinc single crystals"”

  1. The microstructure of zinc single crystals during creep.

    This item was digitized as part of a project to share McGill's intellectual legacy with the public. If you are the copyright holder or a relative of the copyright holder who is deceased, you may request withdrawal by emailing escholarship.library@mcgill.ca. The full policy for eScholarship may be …

    mcgill Repository record for The microstructure of zinc single crystals during creep. (opens in a new tab)

  2. Annealing of deformation twins in zinc single crystals

    Thesis (Ph. D.)--Michigan State University. Department of Metallurgy, Mechanics and Materials Science, 1975

    msu Repository record for Annealing of deformation twins in zinc single crystals (opens in a new tab)

  3. Impurities and the Evaporation Morphology of Zinc Single Crystals

    … investigations of the evaporation morphology of zinc single crystals are presented. Dislocation etch pits developed on (0001) zinc cleavage surfaces. A mechanism is proposed to account for enhanced evaporation at decorated dislocations. The observation of macroledges on pit faces is reported and …

    mcmaster Repository record for Impurities and the Evaporation Morphology of Zinc Single Crystals (opens in a new tab)

  4. Embrittlement of zinc crystals by mercury

    … and modified work hardening characteristics of zinc single crystals coated with mercury. Important results of tensile tests performed under fixed experimental conditions are summarized to be: (1) increase in critical resolved shear stress, and increase of work hardening slope in stage A and …

    ubc Repository record for Embrittlement of zinc crystals by mercury (opens in a new tab)

  5. Pit initiation on passivated metal surfaces: crystallographic orientation and environmental effects

    … susceptibility to pitting corrosion of tin and zinc was found to be dependent on the crystallographic orientation of the surface in chloride solutions. For tin single crystals, the(111) face showed the lowest critical pitting potential among five differently oriented surfaces. The critical …

    ubc Repository record for Pit initiation on passivated metal surfaces: crystallographic orientation and environmental effects (opens in a new tab)