{"id":{"repo_id":"alberta","oai_identifier":"oai:ualberta.scholaris.ca:123456789/60971"},"canonical_url":"https://search.ndltd.org/etd/alberta/oai:ualberta.scholaris.ca:123456789/60971","repository":{"repo_id":"alberta","name":"University of Alberta","base_url":"https://era.library.ualberta.ca/oai"},"display":{"title":"The Role of Sulfur during the Cracking of n-Hexadecane and Cold Lake Bitumen with alpha-Fe2O3 and Steam","abstract":"Coke produced during bitumen upgrading has a high heteroatom content and low economic value. To improve feed efficiency, cracking of hexadecane and bitumen with α-Fe2O3 and water has been studied to decrease coke yield, while increasing sulfur content. Compared to thermal cracking, catalytic cracking of hexadecane with α-Fe2O3 increased the conversion by 11.8% overall. By adding steam, however, the conversion decreased by 5.9%, due to competitive adsorption. The reaction of H2S with α-Fe2O3 was also inhibited by steam that competed for active sites and even oxidized the produced iron sulfides. Conversely, during bitumen cracking, α-Fe2O3 did not affect the coke yield due to fouling of the surface, but did increase the sulfur content of the solid product. On the other hand, the addition of water not only decreased the coke yield by ~3%, but also inhibited the reaction of H2S, indicating that competitive adsorption was still occurring after fouling.","abstract_html":"Coke produced during bitumen upgrading has a high heteroatom content and low economic value. To improve feed efficiency, cracking of hexadecane and bitumen with α-Fe2O3 and water has been studied to decrease coke yield, while increasing sulfur content. Compared to thermal cracking, catalytic cracking of hexadecane with α-Fe2O3 increased the conversion by 11.8% overall. By adding steam, however, the conversion decreased by 5.9%, due to competitive adsorption. The reaction of H2S with α-Fe2O3 was also inhibited by steam that competed for active sites and even oxidized the produced iron sulfides. Conversely, during bitumen cracking, α-Fe2O3 did not affect the coke yield due to fouling of the surface, but did increase the sulfur content of the solid product. On the other hand, the addition of water not only decreased the coke yield by ~3%, but also inhibited the reaction of H2S, indicating that competitive adsorption was still occurring after fouling.","abstract_has_math":false,"creators":["Olson, Blake J"],"institution":"University of Alberta","degree_name":"Master of Science","degree_level":"Master's","degree_discipline":"Chemical Engineering","degree_department":null,"school":null,"contributors":[],"advisors":["McCaffrey, William (Chemical and Materials Engineering)","De Klerk, Arno (Chemical and Materials Engineering)"],"committee_chairs":[],"committee_members":[],"year":2013,"date_issued":"2013-06","date_published":"2013-06","updated_at":"2026-11-26T20:56:00Z","subjects":["Coke","Hexadecane","Steam","Liquid phase cracking","Cold Lake Bitumen","Alpha-Fe2O3"],"languages":["en"],"rights":["This thesis is made available by the University of Alberta Libraries with permission of the copyright owner solely for non-commercial purposes. This thesis, or any portion thereof, may not otherwise be copied or reproduced without the written consent of the copyright owner, except to the extent permitted by Canadian copyright law."],"rights_urls":[],"identifier_entries":[],"person_identifier_entries":[]},"links":{"outbound_url":"https://doi.org/10.7939/R3K352","outbound_label":"DOI","outbound_source":"dc:identifier.doi","record_url":"https://doi.org/10.7939/R3K352","record_label":"Repository record","record_kind":"doi","record_source":"dc:identifier.doi","access_status":null,"embargo_until":null,"access_note":null},"oai_pmh_record":{"url":"https://union.ndltd.org/oai-pmh/?verb=GetRecord&metadataPrefix=oai_dc&identifier=oai%3Aunion.ndltd.org%3Arepo%3Aalberta%3Aoai%3Aualberta.scholaris.ca%3A123456789%2F60971","prefix":"oai_dc"},"source_record":{"url":"https://era.library.ualberta.ca/oai?verb=GetRecord&metadataPrefix=dim&identifier=oai%3Aualberta.scholaris.ca%3A123456789%2F60971","prefix":"dim"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:contributor.advisor","label":"Advisor","values":["McCaffrey, William (Chemical and Materials Engineering)","De Klerk, Arno (Chemical and Materials Engineering)"]},{"key":"dc:contributor.other","label":"Dc Contributor Other","values":["Stryker, Jeffrey (Chemistry)"]},{"key":"dc:creator","label":"Author","values":["Olson, Blake J"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date.accessioned","label":"Dc Date Accessioned","values":["2025-05-06T16:58:28Z"]},{"key":"dc:date.available","label":"Dc Date Available","values":["2025-05-06T16:58:28Z"]},{"key":"dc:date.issued","label":"Date","values":["2013-06"]},{"key":"dc:type","label":"Dc Type","values":["Thesis"]},{"key":"thesis:degree_discipline","label":"Discipline","values":["Chemical Engineering"]},{"key":"thesis:degree_level","label":"Degree Level","values":["Master's"]},{"key":"thesis:degree_name","label":"Degree Name","values":["Master of Science"]},{"key":"thesis:institution_name","label":"Thesis Institution Name","values":["University of Alberta"]}]},{"id":"subjects_keywords","label":"Subjects and Keywords","entries":[{"key":"dc:subject","label":"Dc Subject","values":["Coke","Hexadecane","Steam","Liquid phase cracking","Cold Lake Bitumen","Alpha-Fe2O3"]}]},{"id":"language_rights","label":"Language and Rights","entries":[{"key":"dc:language.iso","label":"Language (ISO)","values":["en"]},{"key":"dc:rights","label":"Dc Rights","values":["This thesis is made available by the University of Alberta Libraries with permission of the copyright owner solely for non-commercial purposes. This thesis, or any portion thereof, may not otherwise be copied or reproduced without the written consent of the copyright owner, except to the extent permitted by Canadian copyright law."]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier.doi","label":"DOI","values":["https://doi.org/10.7939/R3K352"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description.abstract","label":"Abstract","values":["Coke produced during bitumen upgrading has a high heteroatom content and low economic value. To improve feed efficiency, cracking of hexadecane and bitumen with α-Fe2O3 and water has been studied to decrease coke yield, while increasing sulfur content. Compared to thermal cracking, catalytic cracking of hexadecane with α-Fe2O3 increased the conversion by 11.8% overall. By adding steam, however, the conversion decreased by 5.9%, due to competitive adsorption. The reaction of H2S with α-Fe2O3 was also inhibited by steam that competed for active sites and even oxidized the produced iron sulfides. Conversely, during bitumen cracking, α-Fe2O3 did not affect the coke yield due to fouling of the surface, but did increase the sulfur content of the solid product. On the other hand, the addition of water not only decreased the coke yield by ~3%, but also inhibited the reaction of H2S, indicating that competitive adsorption was still occurring after fouling."]},{"key":"dc:title","label":"Title","values":["The Role of Sulfur during the Cracking of n-Hexadecane and Cold Lake Bitumen with alpha-Fe2O3 and Steam"]},{"key":"others:access_status","label":"Others Access Status","values":["open.access"]}]}],"canonical_facts":{"dc:contributor.advisor":["McCaffrey, William (Chemical and Materials Engineering)","De Klerk, Arno (Chemical and Materials Engineering)"],"dc:contributor.other":["Stryker, Jeffrey (Chemistry)"],"dc:creator":["Olson, Blake J"],"dc:date.accessioned":["2025-05-06T16:58:28Z"],"dc:date.available":["2025-05-06T16:58:28Z"],"dc:date.issued":["2013-06"],"dc:description.abstract":["Coke produced during bitumen upgrading has a high heteroatom content and low economic value. To improve feed efficiency, cracking of hexadecane and bitumen with α-Fe2O3 and water has been studied to decrease coke yield, while increasing sulfur content. Compared to thermal cracking, catalytic cracking of hexadecane with α-Fe2O3 increased the conversion by 11.8% overall. By adding steam, however, the conversion decreased by 5.9%, due to competitive adsorption. The reaction of H2S with α-Fe2O3 was also inhibited by steam that competed for active sites and even oxidized the produced iron sulfides. Conversely, during bitumen cracking, α-Fe2O3 did not affect the coke yield due to fouling of the surface, but did increase the sulfur content of the solid product. On the other hand, the addition of water not only decreased the coke yield by ~3%, but also inhibited the reaction of H2S, indicating that competitive adsorption was still occurring after fouling."],"dc:identifier.doi":["https://doi.org/10.7939/R3K352"],"dc:language.iso":["en"],"dc:rights":["This thesis is made available by the University of Alberta Libraries with permission of the copyright owner solely for non-commercial purposes. This thesis, or any portion thereof, may not otherwise be copied or reproduced without the written consent of the copyright owner, except to the extent permitted by Canadian copyright law."],"dc:subject":["Coke","Hexadecane","Steam","Liquid phase cracking","Cold Lake Bitumen","Alpha-Fe2O3"],"dc:title":["The Role of Sulfur during the Cracking of n-Hexadecane and Cold Lake Bitumen with alpha-Fe2O3 and Steam"],"dc:type":["Thesis"],"others:access_status":["open.access"],"thesis:degree_discipline":["Chemical Engineering"],"thesis:degree_level":["Master's"],"thesis:degree_name":["Master of Science"],"thesis:institution_name":["University of Alberta"]},"updated_at":"2026-11-26T20:56:00Z"}