{"id":{"repo_id":"birmingham","oai_identifier":"oai:etheses.bham.ac.uk:4300"},"canonical_url":"https://search.ndltd.org/etd/birmingham/oai:etheses.bham.ac.uk:4300","repository":{"repo_id":"birmingham","name":"University of Birmingham","base_url":"https://etheses.bham.ac.uk/cgi/oai2"},"display":{"title":"Nanocarbon-hydride composites for hydrogen storage","abstract":"Graphite is considered a possible material for solid state hydrogen storage. In this thesis graphite was ball milled for 8hrs under 3 bar H\\(_2\\), followed by the addition of LiBH\\(_4\\) at a ratio of 2:1 (graphite:LiBH\\(_4\\)) and milled for a further 2hrs. Characterization of the as milled material showed the formation of a nanocrsytalline/amorphous mixture of graphite and LiBH\\(_4\\). Decomposition was performed by heating to 500°C at 2°Cmin\\(^{-1}\\). Graphite milled for 8 hrs released a small amount of hydrogen at 350°C, though no reaction was observed using DSC. The graphite+LiBH\\(_4\\) sample, however, exhibited 4 endothermic peaks consistent with a modified LiBH\\(_4\\) decomposition. The application of an over pressure of hydrogen during heating of the graphite+LiBH\\(_4\\) was found to suppress the decomposition of LiBH\\(_4\\). In-situ XRD measurements demonstrated that Li\\(_2\\)C\\(_2\\) was formed. Li\\(_2\\)C\\(_2\\) is known to be a key decomposition product in making a graphite based system reversible. It was not possible to identify the exact decomposition path due to partial oxidation of the sample during the measurement. Partial reversibility was observed at non optimized conditions of 500°C under 100bar H\\(_2\\) for 20 minutes.","abstract_html":"Graphite is considered a possible material for solid state hydrogen storage. In this thesis graphite was ball milled for 8hrs under 3 bar H<span class=\"etd-inline-math\"><sub>2</sub></span>, followed by the addition of LiBH<span class=\"etd-inline-math\"><sub>4</sub></span> at a ratio of 2:1 (graphite:LiBH<span class=\"etd-inline-math\"><sub>4</sub></span>) and milled for a further 2hrs. Characterization of the as milled material showed the formation of a nanocrsytalline/amorphous mixture of graphite and LiBH<span class=\"etd-inline-math\"><sub>4</sub></span>. Decomposition was performed by heating to 500°C at 2°Cmin<span class=\"etd-inline-math\"><sup>-1</sup></span>. Graphite milled for 8 hrs released a small amount of hydrogen at 350°C, though no reaction was observed using DSC. The graphite+LiBH<span class=\"etd-inline-math\"><sub>4</sub></span> sample, however, exhibited 4 endothermic peaks consistent with a modified LiBH<span class=\"etd-inline-math\"><sub>4</sub></span> decomposition. The application of an over pressure of hydrogen during heating of the graphite+LiBH<span class=\"etd-inline-math\"><sub>4</sub></span> was found to suppress the decomposition of LiBH<span class=\"etd-inline-math\"><sub>4</sub></span>. In-situ XRD measurements demonstrated that Li<span class=\"etd-inline-math\"><sub>2</sub></span>C<span class=\"etd-inline-math\"><sub>2</sub></span> was formed. Li<span class=\"etd-inline-math\"><sub>2</sub></span>C<span class=\"etd-inline-math\"><sub>2</sub></span> is known to be a key decomposition product in making a graphite based system reversible. It was not possible to identify the exact decomposition path due to partial oxidation of the sample during the measurement. Partial reversibility was observed at non optimized conditions of 500°C under 100bar H<span class=\"etd-inline-math\"><sub>2</sub></span> for 20 minutes.","abstract_has_math":true,"creators":["Vines, Joshua Edwin"],"institution":"University of Birmingham","degree_name":"m_rs","degree_level":"m_rs","degree_discipline":null,"degree_department":null,"school":null,"contributors":[],"advisors":[],"committee_chairs":[],"committee_members":[],"year":2013,"date_issued":"2013-07","date_published":"2013-07","updated_at":"2026-11-19T09:27:39Z","subjects":["QC Physics","QD Chemistry","TA Engineering (General). Civil engineering (General)"],"languages":["eng"],"rights":[],"rights_urls":[],"identifier_entries":[],"person_identifier_entries":[]},"links":{"outbound_url":null,"outbound_label":null,"outbound_source":null,"record_url":null,"record_label":null,"record_kind":null,"record_source":null,"download_url":"http://etheses.bham.ac.uk//id/eprint/4300/1/VinesJ13MRes.pdf","download_label":"Download PDF","download_source":"dc:identifier.uri","access_status":null,"embargo_until":null,"access_note":null},"source_record":{"url":"https://etheses.bham.ac.uk/cgi/oai2?verb=GetRecord&metadataPrefix=uketd_dc&identifier=oai%3Aetheses.bham.ac.uk%3A4300","prefix":"uketd_dc"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:contributor.sponsor","label":"Sponsor","values":["epsrc"]},{"key":"dc:creator","label":"Author","values":["Vines, Joshua Edwin"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date","label":"Dc Date","values":["2013-07"]},{"key":"dc:date.issued","label":"Date","values":["2013-07"]},{"key":"dc:publisher.department","label":"Dc Publisher Department","values":["College of Engineering & Physical Sciences","School of Metallurgy and Materials"]},{"key":"dc:publisher.institution","label":"Dc Publisher Institution","values":["University of Birmingham"]},{"key":"dc:relation.isreferencedby","label":"Dc Relation Isreferencedby","values":["http://etheses.bham.ac.uk//id/eprint/4300/"]},{"key":"dc:type","label":"Dc Type","values":["Thesis"]},{"key":"dc:type.qualificationlevel","label":"Dc Type Qualificationlevel","values":["m_rs"]},{"key":"dc:type.qualificationname","label":"Dc Type Qualificationname","values":["m_rs"]}]},{"id":"subjects_keywords","label":"Subjects and Keywords","entries":[{"key":"dc:subject","label":"Dc Subject","values":["QC Physics","QD Chemistry","TA Engineering (General). Civil engineering (General)"]}]},{"id":"language_rights","label":"Language and Rights","entries":[{"key":"dc:language.dcterms_iso639_2","label":"Language (ISO 639-2)","values":["eng"]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier.uri","label":"Identifier URI","values":["http://etheses.bham.ac.uk//id/eprint/4300/1/VinesJ13MRes.pdf","http://etheses.bham.ac.uk//id/eprint/4300/2/Decl_IS_Vines13MRes.pdf"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description.abstract","label":"Abstract","values":["Graphite is considered a possible material for solid state hydrogen storage. In this thesis graphite was ball milled for 8hrs under 3 bar H\\(_2\\), followed by the addition of LiBH\\(_4\\) at a ratio of 2:1 (graphite:LiBH\\(_4\\)) and milled for a further 2hrs. Characterization of the as milled material showed the formation of a nanocrsytalline/amorphous mixture of graphite and LiBH\\(_4\\). Decomposition was performed by heating to 500°C at 2°Cmin\\(^{-1}\\). Graphite milled for 8 hrs released a small amount of hydrogen at 350°C, though no reaction was observed using DSC. The graphite+LiBH\\(_4\\) sample, however, exhibited 4 endothermic peaks consistent with a modified LiBH\\(_4\\) decomposition. The application of an over pressure of hydrogen during heating of the graphite+LiBH\\(_4\\) was found to suppress the decomposition of LiBH\\(_4\\). In-situ XRD measurements demonstrated that Li\\(_2\\)C\\(_2\\) was formed. Li\\(_2\\)C\\(_2\\) is known to be a key decomposition product in making a graphite based system reversible. It was not possible to identify the exact decomposition path due to partial oxidation of the sample during the measurement. Partial reversibility was observed at non optimized conditions of 500°C under 100bar H\\(_2\\) for 20 minutes."]},{"key":"dc:format","label":"Dc Format","values":["application/pdf"]},{"key":"dcterms:accessrights","label":"Dcterms Accessrights","values":["public","staffonly"]},{"key":"dc:title","label":"Title","values":["Nanocarbon-hydride composites for hydrogen storage"]}]}],"canonical_facts":{"dc:contributor.sponsor":["epsrc"],"dc:creator":["Vines, Joshua Edwin"],"dc:date":["2013-07"],"dc:date.issued":["2013-07"],"dc:description.abstract":["Graphite is considered a possible material for solid state hydrogen storage. In this thesis graphite was ball milled for 8hrs under 3 bar H\\(_2\\), followed by the addition of LiBH\\(_4\\) at a ratio of 2:1 (graphite:LiBH\\(_4\\)) and milled for a further 2hrs. Characterization of the as milled material showed the formation of a nanocrsytalline/amorphous mixture of graphite and LiBH\\(_4\\). Decomposition was performed by heating to 500°C at 2°Cmin\\(^{-1}\\). Graphite milled for 8 hrs released a small amount of hydrogen at 350°C, though no reaction was observed using DSC. The graphite+LiBH\\(_4\\) sample, however, exhibited 4 endothermic peaks consistent with a modified LiBH\\(_4\\) decomposition. The application of an over pressure of hydrogen during heating of the graphite+LiBH\\(_4\\) was found to suppress the decomposition of LiBH\\(_4\\). In-situ XRD measurements demonstrated that Li\\(_2\\)C\\(_2\\) was formed. Li\\(_2\\)C\\(_2\\) is known to be a key decomposition product in making a graphite based system reversible. It was not possible to identify the exact decomposition path due to partial oxidation of the sample during the measurement. Partial reversibility was observed at non optimized conditions of 500°C under 100bar H\\(_2\\) for 20 minutes."],"dc:format":["application/pdf"],"dc:identifier.uri":["http://etheses.bham.ac.uk//id/eprint/4300/1/VinesJ13MRes.pdf","http://etheses.bham.ac.uk//id/eprint/4300/2/Decl_IS_Vines13MRes.pdf"],"dc:language.dcterms_iso639_2":["eng"],"dc:publisher.department":["College of Engineering & Physical Sciences","School of Metallurgy and Materials"],"dc:publisher.institution":["University of Birmingham"],"dc:relation.isreferencedby":["http://etheses.bham.ac.uk//id/eprint/4300/"],"dc:subject":["QC Physics","QD Chemistry","TA Engineering (General). Civil engineering (General)"],"dcterms:accessrights":["public","staffonly"],"dc:title":["Nanocarbon-hydride composites for hydrogen storage"],"dc:type":["Thesis"],"dc:type.qualificationlevel":["m_rs"],"dc:type.qualificationname":["m_rs"]},"updated_at":"2026-11-19T09:27:39Z"}