{"id":{"repo_id":"carleton","oai_identifier":"oai:carleton.scholaris.ca:20.500.14718/38492"},"canonical_url":"https://search.ndltd.org/etd/carleton/oai:carleton.scholaris.ca:20.500.14718/38492","repository":{"repo_id":"carleton","name":"Carleton University","base_url":"https://carleton.scholaris.ca/server/oai/request"},"display":{"title":"Vapour Deposition: Thermal Characterization and Application of Metal Oxide Thin Films","abstract":"Three precursors of group 11 metals, gold(I) 1,3-diisopropyl-imidazolidin-2-ylidene hexamethyldisilazide, gold(I) tert-butyl-imino-2,2-dimethylpyrrolidinate, silver(I) tertbutyl-imino-2,2-dimethylpyrrolidinate were subjected to solution based NMR thermolysis studies. Rates of decomposition and order of reactivity were gathered. Two novel antimony compounds, trimethyl phosphine antimony (III) chloride and bistrimethyl phosphine antimony (III) chloride were subjected to thermal characterization by TGA and CVD experiments in attempt to produce antimony or antimony oxide films. Few experiments gave varying depositions but reproducible coatings were not achieved. Protective coatings of alumina and bilayers of alumina and titania were deposited on bronze test tokens as well as on numismatic silver coins. Multiple tests examined the efficacy of such films against physical and chemical wear. Silver coins were compared to a traditional lacquer coating. The ALD coatings on tokens provided improved wear and chemical protection vs. unprotected coins. Final numismatic coatings of alumina gave greatest adhesion, but did reveal small areas of chemical penetration.","abstract_html":"Three precursors of group 11 metals, gold(I) 1,3-diisopropyl-imidazolidin-2-ylidene hexamethyldisilazide, gold(I) tert-butyl-imino-2,2-dimethylpyrrolidinate, silver(I) tertbutyl-imino-2,2-dimethylpyrrolidinate were subjected to solution based NMR thermolysis studies. Rates of decomposition and order of reactivity were gathered. Two novel antimony compounds, trimethyl phosphine antimony (III) chloride and bistrimethyl phosphine antimony (III) chloride were subjected to thermal characterization by TGA and CVD experiments in attempt to produce antimony or antimony oxide films. Few experiments gave varying depositions but reproducible coatings were not achieved. Protective coatings of alumina and bilayers of alumina and titania were deposited on bronze test tokens as well as on numismatic silver coins. Multiple tests examined the efficacy of such films against physical and chemical wear. Silver coins were compared to a traditional lacquer coating. The ALD coatings on tokens provided improved wear and chemical protection vs. unprotected coins. Final numismatic coatings of alumina gave greatest adhesion, but did reveal small areas of chemical penetration.","abstract_has_math":false,"creators":["Wells, Adam"],"institution":"Carleton University","degree_name":"Master of Science (M.Sc.)","degree_level":"Master's","degree_discipline":"Chemistry","degree_department":null,"school":null,"contributors":[],"advisors":[],"committee_chairs":[],"committee_members":[],"year":2014,"date_issued":"2014","date_published":"2014","updated_at":"2026-11-19T07:04:44Z","subjects":["Chemistry, Inorganic"],"languages":["en"],"rights":["Copyright © 2014 the author(s). Theses may be used for non-commercial research, educational, or related academic purposes only. Such uses include personal study, research, scholarship, and teaching. Theses may only be shared by linking to Carleton University Institutional Repository and no part may be used without proper attribution to the author. No part may be used for commercial purposes directly or indirectly via a for-profit platform; no adaptation or derivative works are permitted without consent from the copyright owner."],"rights_urls":[],"identifier_entries":[{"key":"dc:identifier.doi","label":"DOI","values":["10.22215/etd/2014-10343"],"render_values":[{"text":"10.22215/etd/2014-10343","href":"https://doi.org/10.22215/etd/2014-10343","code":true}]}],"person_identifier_entries":[]},"links":{"outbound_url":"https://hdl.handle.net/20.500.14718/38492","outbound_label":"Handle","outbound_source":"dc:identifier.uri","record_url":"https://hdl.handle.net/20.500.14718/38492","record_label":"Repository record","record_kind":"handle","record_source":"dc:identifier.uri","download_url":null,"download_label":null,"download_source":null,"access_status":null,"embargo_until":null,"access_note":null},"source_record":{"url":"https://carleton.scholaris.ca/server/oai/request?verb=GetRecord&metadataPrefix=dim&identifier=oai%3Acarleton.scholaris.ca%3A20.500.14718%2F38492","prefix":"dim"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:creator","label":"Author","values":["Wells, Adam"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date.accessioned","label":"Dc Date Accessioned","values":["2025-04-08T19:24:31Z"]},{"key":"dc:date.available","label":"Dc Date Available","values":["2025-04-08T19:24:31Z"]},{"key":"dc:date.issued","label":"Date","values":["2014"]},{"key":"dc:publisher","label":"Institution","values":["Carleton University"]},{"key":"dc:type","label":"Dc Type","values":["thesis"]},{"key":"thesis:degree_discipline","label":"Discipline","values":["Chemistry"]},{"key":"thesis:degree_level","label":"Degree Level","values":["Master's"]},{"key":"thesis:degree_name","label":"Degree Name","values":["Master of Science (M.Sc.)"]}]},{"id":"subjects_keywords","label":"Subjects and Keywords","entries":[{"key":"dc:subject.lcsh","label":"Dc Subject Lcsh","values":["Chemistry, Inorganic"]}]},{"id":"language_rights","label":"Language and Rights","entries":[{"key":"dc:language.iso","label":"Language (ISO)","values":["en"]},{"key":"dc:rights","label":"Dc Rights","values":["Copyright © 2014 the author(s). Theses may be used for non-commercial research, educational, or related academic purposes only. Such uses include personal study, research, scholarship, and teaching. Theses may only be shared by linking to Carleton University Institutional Repository and no part may be used without proper attribution to the author. No part may be used for commercial purposes directly or indirectly via a for-profit platform; no adaptation or derivative works are permitted without consent from the copyright owner."]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier.doi","label":"DOI","values":["10.22215/etd/2014-10343"]},{"key":"dc:identifier.uri","label":"Identifier URI","values":["https://hdl.handle.net/20.500.14718/38492"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description.abstract","label":"Abstract","values":["Three precursors of group 11 metals, gold(I) 1,3-diisopropyl-imidazolidin-2-ylidene hexamethyldisilazide, gold(I) tert-butyl-imino-2,2-dimethylpyrrolidinate, silver(I) tertbutyl-imino-2,2-dimethylpyrrolidinate were subjected to solution based NMR thermolysis studies. Rates of decomposition and order of reactivity were gathered. Two novel antimony compounds, trimethyl phosphine antimony (III) chloride and bistrimethyl phosphine antimony (III) chloride were subjected to thermal characterization by TGA and CVD experiments in attempt to produce antimony or antimony oxide films. Few experiments gave varying depositions but reproducible coatings were not achieved. Protective coatings of alumina and bilayers of alumina and titania were deposited on bronze test tokens as well as on numismatic silver coins. Multiple tests examined the efficacy of such films against physical and chemical wear. Silver coins were compared to a traditional lacquer coating. The ALD coatings on tokens provided improved wear and chemical protection vs. unprotected coins. Final numismatic coatings of alumina gave greatest adhesion, but did reveal small areas of chemical penetration."]},{"key":"dc:title","label":"Title","values":["Vapour Deposition: Thermal Characterization and Application of Metal Oxide Thin Films"]},{"key":"local:lac.licence","label":"Local Lac Licence","values":["true"]},{"key":"others:access_status","label":"Others Access Status","values":["open.access"]}]}],"canonical_facts":{"dc:creator":["Wells, Adam"],"dc:date.accessioned":["2025-04-08T19:24:31Z"],"dc:date.available":["2025-04-08T19:24:31Z"],"dc:date.issued":["2014"],"dc:description.abstract":["Three precursors of group 11 metals, gold(I) 1,3-diisopropyl-imidazolidin-2-ylidene hexamethyldisilazide, gold(I) tert-butyl-imino-2,2-dimethylpyrrolidinate, silver(I) tertbutyl-imino-2,2-dimethylpyrrolidinate were subjected to solution based NMR thermolysis studies. Rates of decomposition and order of reactivity were gathered. Two novel antimony compounds, trimethyl phosphine antimony (III) chloride and bistrimethyl phosphine antimony (III) chloride were subjected to thermal characterization by TGA and CVD experiments in attempt to produce antimony or antimony oxide films. Few experiments gave varying depositions but reproducible coatings were not achieved. Protective coatings of alumina and bilayers of alumina and titania were deposited on bronze test tokens as well as on numismatic silver coins. Multiple tests examined the efficacy of such films against physical and chemical wear. Silver coins were compared to a traditional lacquer coating. The ALD coatings on tokens provided improved wear and chemical protection vs. unprotected coins. Final numismatic coatings of alumina gave greatest adhesion, but did reveal small areas of chemical penetration."],"dc:identifier.doi":["10.22215/etd/2014-10343"],"dc:identifier.uri":["https://hdl.handle.net/20.500.14718/38492"],"dc:language.iso":["en"],"dc:publisher":["Carleton University"],"dc:rights":["Copyright © 2014 the author(s). Theses may be used for non-commercial research, educational, or related academic purposes only. Such uses include personal study, research, scholarship, and teaching. Theses may only be shared by linking to Carleton University Institutional Repository and no part may be used without proper attribution to the author. No part may be used for commercial purposes directly or indirectly via a for-profit platform; no adaptation or derivative works are permitted without consent from the copyright owner."],"dc:subject.lcsh":["Chemistry, Inorganic"],"dc:title":["Vapour Deposition: Thermal Characterization and Application of Metal Oxide Thin Films"],"dc:type":["thesis"],"local:lac.licence":["true"],"others:access_status":["open.access"],"thesis:degree_discipline":["Chemistry"],"thesis:degree_level":["Master's"],"thesis:degree_name":["Master of Science (M.Sc.)"]},"updated_at":"2026-11-19T07:04:44Z"}