{"id":{"repo_id":"clemson","oai_identifier":"oai:open.clemson.edu:all_theses-5122"},"canonical_url":"https://search.ndltd.org/etd/clemson/oai:open.clemson.edu:all_theses-5122","repository":{"repo_id":"clemson","name":"Clemson University","base_url":"https://open.clemson.edu/do/oai/"},"display":{"title":"Experimental Investigation of the Long-Term Bending Deflection and Creep Performance of Cross-Laminated Timber (CLT)","abstract":"Rising popularity in mass timber construction for residential and commercial projects has escalated the need to develop and increase understanding of mass timber products both from a strength and serviceability perspective. For cross-laminated timber (CLT) there is a significant lack of research on the creep characteristics also known as long-term deflection behavior. Creep is particularly important for products such as CLT that are used for floors with longer spans. Full-scale creep testing was conducted using 5-ply CLT panels over the course of 6 months in a controlled environment under dry service condition. Testing resulted in average final deflections 1.73 times the initial elastic deflections. This data was fitted to a power model to provide an accurate estimation of a creep factor for CLT products used in designs under the NDS. Current models show an average increase in deflection of 1.95 times the initial instantaneous deflections after 2.5 years supporting a 2.0 creep factor (Kcr) for the prediction of long-term deflections in the design of CLT members according to the National Design Specification for Wood Construction.","abstract_html":"Rising popularity in mass timber construction for residential and commercial projects has escalated the need to develop and increase understanding of mass timber products both from a strength and serviceability perspective. For cross-laminated timber (CLT) there is a significant lack of research on the creep characteristics also known as long-term deflection behavior. Creep is particularly important for products such as CLT that are used for floors with longer spans. Full-scale creep testing was conducted using 5-ply CLT panels over the course of 6 months in a controlled environment under dry service condition. Testing resulted in average final deflections 1.73 times the initial elastic deflections. This data was fitted to a power model to provide an accurate estimation of a creep factor for CLT products used in designs under the NDS. Current models show an average increase in deflection of 1.95 times the initial instantaneous deflections after 2.5 years supporting a 2.0 creep factor (Kcr) for the prediction of long-term deflections in the design of CLT members according to the National Design Specification for Wood Construction.","abstract_has_math":false,"creators":["DeSantis, Aaron"],"institution":null,"degree_name":"Master of Civil Engineering (MCE)","degree_level":"Thesis","degree_discipline":"Civil Engineering","degree_department":null,"school":null,"contributors":["Dr. Weichiang Pang","Dr. Michael Stoner","Dr. Brandon Ross"],"advisors":[],"committee_chairs":[],"committee_members":[],"year":null,"date_issued":"","date_published":null,"updated_at":"2026-11-19T07:31:04Z","subjects":["Creep","Cross-laminated Timber","CLT","Mass timber","wood design","structural engineering","creep factor"],"languages":[],"rights":[],"rights_urls":[],"identifier_entries":[],"person_identifier_entries":[]},"links":{"outbound_url":"https://open.clemson.edu/all_theses/4106","outbound_label":"Repository record","outbound_source":"dc:identifier","record_url":"https://open.clemson.edu/all_theses/4106","record_label":"Repository record","record_kind":"record","record_source":"dc:identifier","download_url":null,"download_label":null,"download_source":null,"access_status":null,"embargo_until":null,"access_note":null},"source_record":{"url":"https://open.clemson.edu/do/oai/?verb=GetRecord&metadataPrefix=oai_etdms&identifier=oai%3Aopen.clemson.edu%3Aall_theses-5122","prefix":"oai_etdms"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:contributor","label":"Contributor","values":["Dr. Weichiang Pang","Dr. Michael Stoner","Dr. Brandon Ross"]},{"key":"dc:creator","label":"Author","values":["DeSantis, Aaron"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date.available","label":"Dc Date Available","values":["2023-07-19T07:00:00Z"]},{"key":"dc:date.created","label":"Dc Date Created","values":["2023-08-01T07:00:00Z"]},{"key":"thesis:degree_discipline","label":"Discipline","values":["Civil Engineering"]},{"key":"thesis:degree_level","label":"Degree Level","values":["Thesis"]},{"key":"thesis:degree_name","label":"Degree Name","values":["Master of Civil Engineering (MCE)"]}]},{"id":"subjects_keywords","label":"Subjects and Keywords","entries":[{"key":"dc:subject","label":"Dc Subject","values":["Creep","Cross-laminated Timber","CLT","Mass timber","wood design","structural engineering","creep factor"]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier","label":"Identifier","values":["https://open.clemson.edu/all_theses/4106"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description.abstract","label":"Abstract","values":["Rising popularity in mass timber construction for residential and commercial projects has escalated the need to develop and increase understanding of mass timber products both from a strength and serviceability perspective. For cross-laminated timber (CLT) there is a significant lack of research on the creep characteristics also known as long-term deflection behavior. Creep is particularly important for products such as CLT that are used for floors with longer spans. Full-scale creep testing was conducted using 5-ply CLT panels over the course of 6 months in a controlled environment under dry service condition. Testing resulted in average final deflections 1.73 times the initial elastic deflections. This data was fitted to a power model to provide an accurate estimation of a creep factor for CLT products used in designs under the NDS. Current models show an average increase in deflection of 1.95 times the initial instantaneous deflections after 2.5 years supporting a 2.0 creep factor (Kcr) for the prediction of long-term deflections in the design of CLT members according to the National Design Specification for Wood Construction."]},{"key":"dc:title","label":"Title","values":["Experimental Investigation of the Long-Term Bending Deflection and Creep Performance of Cross-Laminated Timber (CLT)"]}]}],"canonical_facts":{"dc:contributor":["Dr. Weichiang Pang","Dr. Michael Stoner","Dr. Brandon Ross"],"dc:creator":["DeSantis, Aaron"],"dc:date.available":["2023-07-19T07:00:00Z"],"dc:date.created":["2023-08-01T07:00:00Z"],"dc:description.abstract":["Rising popularity in mass timber construction for residential and commercial projects has escalated the need to develop and increase understanding of mass timber products both from a strength and serviceability perspective. For cross-laminated timber (CLT) there is a significant lack of research on the creep characteristics also known as long-term deflection behavior. Creep is particularly important for products such as CLT that are used for floors with longer spans. Full-scale creep testing was conducted using 5-ply CLT panels over the course of 6 months in a controlled environment under dry service condition. Testing resulted in average final deflections 1.73 times the initial elastic deflections. This data was fitted to a power model to provide an accurate estimation of a creep factor for CLT products used in designs under the NDS. Current models show an average increase in deflection of 1.95 times the initial instantaneous deflections after 2.5 years supporting a 2.0 creep factor (Kcr) for the prediction of long-term deflections in the design of CLT members according to the National Design Specification for Wood Construction."],"dc:identifier":["https://open.clemson.edu/all_theses/4106"],"dc:subject":["Creep","Cross-laminated Timber","CLT","Mass timber","wood design","structural engineering","creep factor"],"dc:title":["Experimental Investigation of the Long-Term Bending Deflection and Creep Performance of Cross-Laminated Timber (CLT)"],"thesis:degree_discipline":["Civil Engineering"],"thesis:degree_level":["Thesis"],"thesis:degree_name":["Master of Civil Engineering (MCE)"]},"updated_at":"2026-11-19T07:31:04Z"}