{"id":{"repo_id":"colostate","oai_identifier":"oai:mountainscholar.org:10217/243076"},"canonical_url":"https://search.ndltd.org/etd/colostate/oai:mountainscholar.org:10217/243076","repository":{"repo_id":"colostate","name":"Colorado State University","base_url":"https://api.mountainscholar.org/server/oai/request"},"display":{"title":"Nucleation and growth studies of polycrystalline covalent materials","abstract":"The chemical vapor deposition of different covalent polycrystalline materials—including diamond, silicon carbide, and carbon nitride—in stagnation flow reactors was rigorously simulated to determine the nucleation and growth mechanism s of these materials. Kinetic models were used to predict the rates of gas-phase and surface chemistry, the temperature and velocity profiles, potential gaseous film growth precursors, the time evolution of nucleation and intermediate layer formation, and the morphological evolution of continuous polycrystalline films. Numerical studies were also carried out to determine the dependence of the kinetics of nucleation and subsequent polycrystalline film growth on operating conditions. The calculated results for carbon nitride deposition indicate that the experimentally measured bond types in the carbon nitride films must result from chemical bond rearrangement occurring on the deposition surface or in the bulk phase once gaseous film growth precursors, including C, CH2, CH3, C2H2, N, NH, NH2, HCN, and H2CN, are adsorbed. Of these precursors, C and CH3 dominate the carbon contribution to carbon nitride film growth, and atomic nitrogen is the principal nitrogen bearing species. When the evolution rates of a silicon carbide intermediate layer and diamond clusters are calculated by accounting for gas-phase and surface reactions, surface and bulk diffusion, the mechanism for intermediate layer formation, and heterogeneous diamond nucleation kinetics, it is predicted that higher adsorption energies, in the range of 3.7 to 4.5 eV, lead to larger surface adatom densities, lower saturated nucleation densities, and larger silicon carbide intermediate layer thicknesses. The intermediate layer thickness becomes saturated while the growing diamond nuclei still cover a very small fraction of the silicon carbide. Reports of heteroepitaxial diamond nucleation without silicon carbide intermediate layer formation may be readily explained by a significant decrease in the intermediate layer thickness at lower substrate temperatures and at higher diamond nucleation densities. Further, the results of the morphology evolution model reveal that the crystallographic texture and surface morphology—surface roughness, film texture, and grain size—of polycrystalline silicon carbide films, as well as diamond films deposited on the silicon carbide layer, are strongly dependent upon the saturated nucleation density, the deposition condition, and film thickness.","abstract_html":"The chemical vapor deposition of different covalent polycrystalline materials—including diamond, silicon carbide, and carbon nitride—in stagnation flow reactors was rigorously simulated to determine the nucleation and growth mechanism s of these materials. Kinetic models were used to predict the rates of gas-phase and surface chemistry, the temperature and velocity profiles, potential gaseous film growth precursors, the time evolution of nucleation and intermediate layer formation, and the morphological evolution of continuous polycrystalline films. Numerical studies were also carried out to determine the dependence of the kinetics of nucleation and subsequent polycrystalline film growth on operating conditions. The calculated results for carbon nitride deposition indicate that the experimentally measured bond types in the carbon nitride films must result from chemical bond rearrangement occurring on the deposition surface or in the bulk phase once gaseous film growth precursors, including C, CH2, CH3, C2H2, N, NH, NH2, HCN, and H2CN, are adsorbed. Of these precursors, C and CH3 dominate the carbon contribution to carbon nitride film growth, and atomic nitrogen is the principal nitrogen bearing species. When the evolution rates of a silicon carbide intermediate layer and diamond clusters are calculated by accounting for gas-phase and surface reactions, surface and bulk diffusion, the mechanism for intermediate layer formation, and heterogeneous diamond nucleation kinetics, it is predicted that higher adsorption energies, in the range of 3.7 to 4.5 eV, lead to larger surface adatom densities, lower saturated nucleation densities, and larger silicon carbide intermediate layer thicknesses. The intermediate layer thickness becomes saturated while the growing diamond nuclei still cover a very small fraction of the silicon carbide. Reports of heteroepitaxial diamond nucleation without silicon carbide intermediate layer formation may be readily explained by a significant decrease in the intermediate layer thickness at lower substrate temperatures and at higher diamond nucleation densities. Further, the results of the morphology evolution model reveal that the crystallographic texture and surface morphology—surface roughness, film texture, and grain size—of polycrystalline silicon carbide films, as well as diamond films deposited on the silicon carbide layer, are strongly dependent upon the saturated nucleation density, the deposition condition, and film thickness.","abstract_has_math":false,"creators":["Yun, Jungheum, author","Dandy, David S., advisor","Watson, A. Ted, committee member","Parkinson, Bruce, committee member","Belfiore, Laurence, committee member"],"institution":"Colorado State University. Libraries","degree_name":"Doctor of Philosophy (Ph.D.)","degree_level":"Doctoral","degree_discipline":"Chemical Engineering","degree_department":null,"school":null,"contributors":[],"advisors":[],"committee_chairs":[],"committee_members":[],"year":2003,"date_issued":"2003","date_published":"2003","updated_at":"2026-11-19T07:18:04Z","subjects":["chemical engineering","materials science"],"languages":["eng","English"],"rights":["Copyright and other restrictions may apply. User is responsible for compliance with all applicable laws. For information about copyright law, please see https://libguides.colostate.edu/copyright.","This Item is protected by copyright and/or related rights (https://rightsstatements.org/vocab/InC/1.0/). You are free to use this Item in any way that is permitted by the copyright and related rights legislation that applies to your use. For other uses you need to obtain permission from the rights-holder(s)."],"rights_urls":[],"identifier_entries":[{"key":"dc:identifier.uri","label":"Identifier URI","values":["https://hdl.handle.net/10217/243076"],"render_values":[{"text":"https://hdl.handle.net/10217/243076","href":"https://hdl.handle.net/10217/243076","code":true}]}],"person_identifier_entries":[]},"links":{"outbound_url":"https://doi.org/10.25675/3.025932","outbound_label":"DOI","outbound_source":"dc:identifier.uri","record_url":"https://doi.org/10.25675/3.025932","record_label":"Repository record","record_kind":"doi","record_source":"dc:identifier.uri","access_status":null,"embargo_until":null,"access_note":null},"oai_pmh_record":{"url":"https://union.ndltd.org/oai-pmh/?verb=GetRecord&metadataPrefix=oai_dc&identifier=oai%3Aunion.ndltd.org%3Arepo%3Acolostate%3Aoai%3Amountainscholar.org%3A10217%2F243076","prefix":"oai_dc"},"source_record":{"url":"https://api.mountainscholar.org/server/oai/request?verb=GetRecord&metadataPrefix=dim&identifier=oai%3Amountainscholar.org%3A10217%2F243076","prefix":"dim"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:creator","label":"Author","values":["Yun, Jungheum, author","Dandy, David S., advisor","Watson, A. Ted, committee member","Parkinson, Bruce, committee member","Belfiore, Laurence, committee member"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date.accessioned","label":"Dc Date Accessioned","values":["2026-01-29T19:37:19Z"]},{"key":"dc:date.issued","label":"Date","values":["2003"]},{"key":"dc:publisher","label":"Institution","values":["Colorado State University. Libraries"]},{"key":"dc:relation.ispartof","label":"Dc Relation Ispartof","values":["2000-2019"]},{"key":"dc:type","label":"Dc Type","values":["Text"]},{"key":"thesis:degree_discipline","label":"Discipline","values":["Chemical Engineering"]},{"key":"thesis:degree_level","label":"Degree Level","values":["Doctoral"]},{"key":"thesis:degree_name","label":"Degree Name","values":["Doctor of Philosophy (Ph.D.)"]},{"key":"thesis:institution_name","label":"Thesis Institution Name","values":["Colorado State University"]}]},{"id":"subjects_keywords","label":"Subjects and Keywords","entries":[{"key":"dc:subject","label":"Dc Subject","values":["chemical engineering","materials science"]}]},{"id":"language_rights","label":"Language and Rights","entries":[{"key":"dc:language","label":"Dc Language","values":["English"]},{"key":"dc:language.iso","label":"Language (ISO)","values":["eng"]},{"key":"dc:rights","label":"Dc Rights","values":["Copyright and other restrictions may apply. User is responsible for compliance with all applicable laws. For information about copyright law, please see https://libguides.colostate.edu/copyright.","This Item is protected by copyright and/or related rights (https://rightsstatements.org/vocab/InC/1.0/). You are free to use this Item in any way that is permitted by the copyright and related rights legislation that applies to your use. For other uses you need to obtain permission from the rights-holder(s)."]},{"key":"dc:rights.license","label":"Dc Rights License","values":["Per the terms of a contractual agreement, all use of this item is limited to the non-commercial use of Colorado State University and its authorized users."]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier.uri","label":"Identifier URI","values":["https://hdl.handle.net/10217/243076","https://doi.org/10.25675/3.025932"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description","label":"Description","values":["Not digitized by CSUL Digital Services."]},{"key":"dc:description.abstract","label":"Abstract","values":["The chemical vapor deposition of different covalent polycrystalline materials—including diamond, silicon carbide, and carbon nitride—in stagnation flow reactors was rigorously simulated to determine the nucleation and growth mechanism s of these materials. Kinetic models were used to predict the rates of gas-phase and surface chemistry, the temperature and velocity profiles, potential gaseous film growth precursors, the time evolution of nucleation and intermediate layer formation, and the morphological evolution of continuous polycrystalline films. Numerical studies were also carried out to determine the dependence of the kinetics of nucleation and subsequent polycrystalline film growth on operating conditions. The calculated results for carbon nitride deposition indicate that the experimentally measured bond types in the carbon nitride films must result from chemical bond rearrangement occurring on the deposition surface or in the bulk phase once gaseous film growth precursors, including C, CH2, CH3, C2H2, N, NH, NH2, HCN, and H2CN, are adsorbed. Of these precursors, C and CH3 dominate the carbon contribution to carbon nitride film growth, and atomic nitrogen is the principal nitrogen bearing species. When the evolution rates of a silicon carbide intermediate layer and diamond clusters are calculated by accounting for gas-phase and surface reactions, surface and bulk diffusion, the mechanism for intermediate layer formation, and heterogeneous diamond nucleation kinetics, it is predicted that higher adsorption energies, in the range of 3.7 to 4.5 eV, lead to larger surface adatom densities, lower saturated nucleation densities, and larger silicon carbide intermediate layer thicknesses. The intermediate layer thickness becomes saturated while the growing diamond nuclei still cover a very small fraction of the silicon carbide. Reports of heteroepitaxial diamond nucleation without silicon carbide intermediate layer formation may be readily explained by a significant decrease in the intermediate layer thickness at lower substrate temperatures and at higher diamond nucleation densities. Further, the results of the morphology evolution model reveal that the crystallographic texture and surface morphology—surface roughness, film texture, and grain size—of polycrystalline silicon carbide films, as well as diamond films deposited on the silicon carbide layer, are strongly dependent upon the saturated nucleation density, the deposition condition, and film thickness."]},{"key":"dc:format.medium","label":"Dc Format Medium","values":["doctoral dissertations"]},{"key":"dc:title","label":"Title","values":["Nucleation and growth studies of polycrystalline covalent materials"]},{"key":"others:access_status","label":"Others Access Status","values":["open.access"]}]}],"canonical_facts":{"dc:creator":["Yun, Jungheum, author","Dandy, David S., advisor","Watson, A. Ted, committee member","Parkinson, Bruce, committee member","Belfiore, Laurence, committee member"],"dc:date.accessioned":["2026-01-29T19:37:19Z"],"dc:date.issued":["2003"],"dc:description":["Not digitized by CSUL Digital Services."],"dc:description.abstract":["The chemical vapor deposition of different covalent polycrystalline materials—including diamond, silicon carbide, and carbon nitride—in stagnation flow reactors was rigorously simulated to determine the nucleation and growth mechanism s of these materials. Kinetic models were used to predict the rates of gas-phase and surface chemistry, the temperature and velocity profiles, potential gaseous film growth precursors, the time evolution of nucleation and intermediate layer formation, and the morphological evolution of continuous polycrystalline films. Numerical studies were also carried out to determine the dependence of the kinetics of nucleation and subsequent polycrystalline film growth on operating conditions. The calculated results for carbon nitride deposition indicate that the experimentally measured bond types in the carbon nitride films must result from chemical bond rearrangement occurring on the deposition surface or in the bulk phase once gaseous film growth precursors, including C, CH2, CH3, C2H2, N, NH, NH2, HCN, and H2CN, are adsorbed. Of these precursors, C and CH3 dominate the carbon contribution to carbon nitride film growth, and atomic nitrogen is the principal nitrogen bearing species. When the evolution rates of a silicon carbide intermediate layer and diamond clusters are calculated by accounting for gas-phase and surface reactions, surface and bulk diffusion, the mechanism for intermediate layer formation, and heterogeneous diamond nucleation kinetics, it is predicted that higher adsorption energies, in the range of 3.7 to 4.5 eV, lead to larger surface adatom densities, lower saturated nucleation densities, and larger silicon carbide intermediate layer thicknesses. The intermediate layer thickness becomes saturated while the growing diamond nuclei still cover a very small fraction of the silicon carbide. Reports of heteroepitaxial diamond nucleation without silicon carbide intermediate layer formation may be readily explained by a significant decrease in the intermediate layer thickness at lower substrate temperatures and at higher diamond nucleation densities. Further, the results of the morphology evolution model reveal that the crystallographic texture and surface morphology—surface roughness, film texture, and grain size—of polycrystalline silicon carbide films, as well as diamond films deposited on the silicon carbide layer, are strongly dependent upon the saturated nucleation density, the deposition condition, and film thickness."],"dc:format.medium":["doctoral dissertations"],"dc:identifier.uri":["https://hdl.handle.net/10217/243076","https://doi.org/10.25675/3.025932"],"dc:language":["English"],"dc:language.iso":["eng"],"dc:publisher":["Colorado State University. Libraries"],"dc:relation.ispartof":["2000-2019"],"dc:rights":["Copyright and other restrictions may apply. User is responsible for compliance with all applicable laws. For information about copyright law, please see https://libguides.colostate.edu/copyright.","This Item is protected by copyright and/or related rights (https://rightsstatements.org/vocab/InC/1.0/). You are free to use this Item in any way that is permitted by the copyright and related rights legislation that applies to your use. For other uses you need to obtain permission from the rights-holder(s)."],"dc:rights.license":["Per the terms of a contractual agreement, all use of this item is limited to the non-commercial use of Colorado State University and its authorized users."],"dc:subject":["chemical engineering","materials science"],"dc:title":["Nucleation and growth studies of polycrystalline covalent materials"],"dc:type":["Text"],"others:access_status":["open.access"],"thesis:degree_discipline":["Chemical Engineering"],"thesis:degree_level":["Doctoral"],"thesis:degree_name":["Doctor of Philosophy (Ph.D.)"],"thesis:institution_name":["Colorado State University"]},"updated_at":"2026-11-19T07:18:04Z"}