{"id":{"repo_id":"fau","oai_identifier":"oai:digitalcommons.fau.edu:etd_general_3-1551"},"canonical_url":"https://search.ndltd.org/etd/fau/oai:digitalcommons.fau.edu:etd_general_3-1551","repository":{"repo_id":"fau","name":"title=\"Search in OATD\">Florida Atlantic University","base_url":"https://digitalcommons.fau.edu/do/oai/"},"display":{"title":"INFLUENCE OF TEMPERATURE ON CALCAREOUS DEPOSIT DEPOSITION UPON CATHODICALLY POLARIZED STEEL IN SEA WATER","abstract":"Experiments have been performed where cylindrical 1018 steel specimens were polarized to -0.900 V.(SCE) in natural sea water at 24 and 3C and with rotation speeds of 0 and 0.83 Hz. The nature of the calcareous deposits which formed was characterized, first, by monitoring current density during the experiments and, second, by post-test SEM investigation of deposit morphology and thickness and by EEDS analysis of deposit composition. The dependence of cathodic current density and film composition upon temperature and exposure time has been established, and the observed trends have been interpreted in terms of (1) the temperature dependence of the solubility limit and relative nucleation and growth rates for Ca and Mg rich phases and (2) possible electrical conductive behavior on the part of Mg rich deposits.","abstract_html":"Experiments have been performed where cylindrical 1018 steel specimens were polarized to -0.900 V.(SCE) in natural sea water at 24 and 3C and with rotation speeds of 0 and 0.83 Hz. The nature of the calcareous deposits which formed was characterized, first, by monitoring current density during the experiments and, second, by post-test SEM investigation of deposit morphology and thickness and by EEDS analysis of deposit composition. The dependence of cathodic current density and film composition upon temperature and exposure time has been established, and the observed trends have been interpreted in terms of (1) the temperature dependence of the solubility limit and relative nucleation and growth rates for Ca and Mg rich phases and (2) possible electrical conductive behavior on the part of Mg rich deposits.","abstract_has_math":false,"creators":["KUNJAPUR, MADANA MOHAN"],"institution":null,"degree_name":null,"degree_level":"Thesis","degree_discipline":null,"degree_department":null,"school":null,"contributors":[],"advisors":[],"committee_chairs":[],"committee_members":[],"year":null,"date_issued":"","date_published":null,"updated_at":"2026-11-26T13:51:09Z","subjects":["Steel--Cathodic protection","Calcium--Effect of temperature on","Seawater"],"languages":[],"rights":[],"rights_urls":[],"identifier_entries":[],"person_identifier_entries":[]},"links":{"outbound_url":"https://digitalcommons.fau.edu/etd_general_3/552","outbound_label":"Repository record","outbound_source":"dc:identifier","record_url":"https://digitalcommons.fau.edu/etd_general_3/552","record_label":"Repository record","record_kind":"record","record_source":"dc:identifier","access_status":null,"embargo_until":null,"access_note":null},"oai_pmh_record":{"url":"https://union.ndltd.org/oai-pmh/?verb=GetRecord&metadataPrefix=oai_dc&identifier=oai%3Aunion.ndltd.org%3Arepo%3Afau%3Aoai%3Adigitalcommons.fau.edu%3Aetd_general_3-1551","prefix":"oai_dc"},"source_record":{"url":"https://digitalcommons.fau.edu/do/oai/?verb=GetRecord&metadataPrefix=oai_etdms&identifier=oai%3Adigitalcommons.fau.edu%3Aetd_general_3-1551","prefix":"oai_etdms"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:creator","label":"Author","values":["KUNJAPUR, MADANA MOHAN"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date.created","label":"Dc Date Created","values":["1987-01-01T08:00:00Z"]},{"key":"thesis:degree_level","label":"Degree Level","values":["Thesis"]}]},{"id":"subjects_keywords","label":"Subjects and Keywords","entries":[{"key":"dc:subject","label":"Dc Subject","values":["Steel--Cathodic protection","Calcium--Effect of temperature on","Seawater"]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier","label":"Identifier","values":["https://digitalcommons.fau.edu/etd_general_3/552"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description.abstract","label":"Abstract","values":["Experiments have been performed where cylindrical 1018 steel specimens were polarized to -0.900 V.(SCE) in natural sea water at 24 and 3C and with rotation speeds of 0 and 0.83 Hz. The nature of the calcareous deposits which formed was characterized, first, by monitoring current density during the experiments and, second, by post-test SEM investigation of deposit morphology and thickness and by EEDS analysis of deposit composition. The dependence of cathodic current density and film composition upon temperature and exposure time has been established, and the observed trends have been interpreted in terms of (1) the temperature dependence of the solubility limit and relative nucleation and growth rates for Ca and Mg rich phases and (2) possible electrical conductive behavior on the part of Mg rich deposits."]},{"key":"dc:description.note","label":"Dc Description Note","values":["College of Engineering and Computer Science|Thesis (M.S.)--Florida Atlantic University, 1987.|FAU Electronic Theses and Dissertations Collection|College of Engineering and Computer Science"]},{"key":"dc:title","label":"Title","values":["INFLUENCE OF TEMPERATURE ON CALCAREOUS DEPOSIT DEPOSITION UPON CATHODICALLY POLARIZED STEEL IN SEA WATER"]}]}],"canonical_facts":{"dc:creator":["KUNJAPUR, MADANA MOHAN"],"dc:date.created":["1987-01-01T08:00:00Z"],"dc:description.abstract":["Experiments have been performed where cylindrical 1018 steel specimens were polarized to -0.900 V.(SCE) in natural sea water at 24 and 3C and with rotation speeds of 0 and 0.83 Hz. The nature of the calcareous deposits which formed was characterized, first, by monitoring current density during the experiments and, second, by post-test SEM investigation of deposit morphology and thickness and by EEDS analysis of deposit composition. The dependence of cathodic current density and film composition upon temperature and exposure time has been established, and the observed trends have been interpreted in terms of (1) the temperature dependence of the solubility limit and relative nucleation and growth rates for Ca and Mg rich phases and (2) possible electrical conductive behavior on the part of Mg rich deposits."],"dc:description.note":["College of Engineering and Computer Science|Thesis (M.S.)--Florida Atlantic University, 1987.|FAU Electronic Theses and Dissertations Collection|College of Engineering and Computer Science"],"dc:identifier":["https://digitalcommons.fau.edu/etd_general_3/552"],"dc:subject":["Steel--Cathodic protection","Calcium--Effect of temperature on","Seawater"],"dc:title":["INFLUENCE OF TEMPERATURE ON CALCAREOUS DEPOSIT DEPOSITION UPON CATHODICALLY POLARIZED STEEL IN SEA WATER"],"thesis:degree_level":["Thesis"]},"updated_at":"2026-11-26T13:51:09Z"}