{"id":{"repo_id":"fau","oai_identifier":"oai:digitalcommons.fau.edu:etd_general_4-1075"},"canonical_url":"https://search.ndltd.org/etd/fau/oai:digitalcommons.fau.edu:etd_general_4-1075","repository":{"repo_id":"fau","name":"title=\"Search in OATD\">Florida Atlantic University","base_url":"https://digitalcommons.fau.edu/do/oai/"},"display":{"title":"Mode II interlaminar fracture toughness of interleaved composite materials","abstract":"Interlaminar mode II fracture toughness, GIIC, of thermoset and thermoplastic interleaved (TSI and TPI) composites were investigated over a wide range of interleaf thickness. TPI specimens had four to about seven times larger GIIC than those without an interleaf. Poor adhesion observed for some TPI specimens were likely to be due to contaminated film materials. Thermoset interleaves were less effective in enhancing the mode II fracture toughness. However, even 0.043 mm thermoset interleaves gave three times larger G$\\sb{\\rm IIC}$ than those without an interleaf. Estimates of the volume of the yielded material around the crack tip based on a quasi-elastic finite element approach and Irwin's model showed that the yield zone height reaches a peak value for increasing interleaf thickness for both TSI and TPI specimens. Furthermore, fracture toughness data correlates well with yield zone heights.","abstract_html":"Interlaminar mode II fracture toughness, GIIC, of thermoset and thermoplastic interleaved (TSI and TPI) composites were investigated over a wide range of interleaf thickness. TPI specimens had four to about seven times larger GIIC than those without an interleaf. Poor adhesion observed for some TPI specimens were likely to be due to contaminated film materials. Thermoset interleaves were less effective in enhancing the mode II fracture toughness. However, even 0.043 mm thermoset interleaves gave three times larger G$\\sb{\\rm IIC}$ than those without an interleaf. Estimates of the volume of the yielded material around the crack tip based on a quasi-elastic finite element approach and Irwin&#x27;s model showed that the yield zone height reaches a peak value for increasing interleaf thickness for both TSI and TPI specimens. Furthermore, fracture toughness data correlates well with yield zone heights.","abstract_has_math":true,"creators":["Aksoy, Adnan."],"institution":null,"degree_name":null,"degree_level":"Thesis","degree_discipline":null,"degree_department":null,"school":null,"contributors":[],"advisors":[],"committee_chairs":[],"committee_members":[],"year":null,"date_issued":"","date_published":null,"updated_at":"2026-11-26T13:53:33Z","subjects":["Composite materials--Cracking","Fracture mechanics","Composite materials--Testing"],"languages":[],"rights":[],"rights_urls":[],"identifier_entries":[],"person_identifier_entries":[]},"links":{"outbound_url":"https://digitalcommons.fau.edu/etd_general_4/76","outbound_label":"Repository record","outbound_source":"dc:identifier","record_url":"https://digitalcommons.fau.edu/etd_general_4/76","record_label":"Repository record","record_kind":"record","record_source":"dc:identifier","access_status":null,"embargo_until":null,"access_note":null},"oai_pmh_record":{"url":"https://union.ndltd.org/oai-pmh/?verb=GetRecord&metadataPrefix=oai_dc&identifier=oai%3Aunion.ndltd.org%3Arepo%3Afau%3Aoai%3Adigitalcommons.fau.edu%3Aetd_general_4-1075","prefix":"oai_dc"},"source_record":{"url":"https://digitalcommons.fau.edu/do/oai/?verb=GetRecord&metadataPrefix=oai_etdms&identifier=oai%3Adigitalcommons.fau.edu%3Aetd_general_4-1075","prefix":"oai_etdms"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:creator","label":"Author","values":["Aksoy, Adnan."]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date.created","label":"Dc Date Created","values":["1990-01-01T08:00:00Z"]},{"key":"thesis:degree_level","label":"Degree Level","values":["Thesis"]}]},{"id":"subjects_keywords","label":"Subjects and Keywords","entries":[{"key":"dc:subject","label":"Dc Subject","values":["Composite materials--Cracking","Fracture mechanics","Composite materials--Testing"]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier","label":"Identifier","values":["https://digitalcommons.fau.edu/etd_general_4/76"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description.abstract","label":"Abstract","values":["Interlaminar mode II fracture toughness, GIIC, of thermoset and thermoplastic interleaved (TSI and TPI) composites were investigated over a wide range of interleaf thickness. TPI specimens had four to about seven times larger GIIC than those without an interleaf. Poor adhesion observed for some TPI specimens were likely to be due to contaminated film materials. Thermoset interleaves were less effective in enhancing the mode II fracture toughness. However, even 0.043 mm thermoset interleaves gave three times larger G$\\sb{\\rm IIC}$ than those without an interleaf. Estimates of the volume of the yielded material around the crack tip based on a quasi-elastic finite element approach and Irwin's model showed that the yield zone height reaches a peak value for increasing interleaf thickness for both TSI and TPI specimens. Furthermore, fracture toughness data correlates well with yield zone heights."]},{"key":"dc:description.note","label":"Dc Description Note","values":["College of Engineering and Computer Science|FAU Electronic Theses and Dissertations Collection|Thesis (M.S.E.)--Florida Atlantic University, 1990.|College of Engineering and Computer Science"]},{"key":"dc:title","label":"Title","values":["Mode II interlaminar fracture toughness of interleaved composite materials"]}]}],"canonical_facts":{"dc:creator":["Aksoy, Adnan."],"dc:date.created":["1990-01-01T08:00:00Z"],"dc:description.abstract":["Interlaminar mode II fracture toughness, GIIC, of thermoset and thermoplastic interleaved (TSI and TPI) composites were investigated over a wide range of interleaf thickness. TPI specimens had four to about seven times larger GIIC than those without an interleaf. Poor adhesion observed for some TPI specimens were likely to be due to contaminated film materials. Thermoset interleaves were less effective in enhancing the mode II fracture toughness. However, even 0.043 mm thermoset interleaves gave three times larger G$\\sb{\\rm IIC}$ than those without an interleaf. Estimates of the volume of the yielded material around the crack tip based on a quasi-elastic finite element approach and Irwin's model showed that the yield zone height reaches a peak value for increasing interleaf thickness for both TSI and TPI specimens. Furthermore, fracture toughness data correlates well with yield zone heights."],"dc:description.note":["College of Engineering and Computer Science|FAU Electronic Theses and Dissertations Collection|Thesis (M.S.E.)--Florida Atlantic University, 1990.|College of Engineering and Computer Science"],"dc:identifier":["https://digitalcommons.fau.edu/etd_general_4/76"],"dc:subject":["Composite materials--Cracking","Fracture mechanics","Composite materials--Testing"],"dc:title":["Mode II interlaminar fracture toughness of interleaved composite materials"],"thesis:degree_level":["Thesis"]},"updated_at":"2026-11-26T13:53:33Z"}