{"id":{"repo_id":"gatech","oai_identifier":"oai:repository.gatech.edu:1853/47742"},"canonical_url":"https://search.ndltd.org/etd/gatech/oai:repository.gatech.edu:1853/47742","repository":{"repo_id":"gatech","name":"Georgia Tech","base_url":"https://repository.gatech.edu/server/oai/request"},"display":{"title":"Recovery boiler superheater corrosion - solubility of metal oxides in molten salt","abstract":"The recovery boiler in a pulp and paper mill plays a dual role of recovering pulping chemicals and generating steam for either chemical processes or producing electricity. The efficiency of producing steam in the recovery boiler is limited by the first melting temperature of ash deposits that accumulate on the superheater tubes. Above the first melting temperature, the molten salt reacts with the protective oxide film that develops and dissolves it. The most protective oxide is determined by evaluating how little it dissolves and how its solubility changes in the molten salt. Solubility tests were done on several protective oxides in a known salt composition from a recovery boiler that burns hardwood derived fuel. ICP-OES was used to measure concentration of dissolved metal in the exposure tests while EDS and XRD were used to verify chemical compositions in exposure tests. NiO was found to be the least soluble oxide while Cr₂O₃ and Al₂O₃ had similar solubility with Fe₂O₃ being less soluble than Cr₂O₃ but more soluble than NiO. Exposure tests with pure metals and selected alloys indicated that even though Fe₂O₃ has little solubility, it is not a protective oxide and causes severe corrosion in stainless steels. The change in performance of iron based alloys was due to the development of a negative solubility gradient for Fe₂O₃ where Fe₂O₃ precipitated out of solution and created a continuous leaching of oxide. Manganese was found to be beneficial in stainless steels but its role is still unknown. Nickel based alloys were found to be least corroded due to nickel's low solubility and because it did not form a negative solubility gradient.","abstract_html":"The recovery boiler in a pulp and paper mill plays a dual role of recovering pulping chemicals and generating steam for either chemical processes or producing electricity. The efficiency of producing steam in the recovery boiler is limited by the first melting temperature of ash deposits that accumulate on the superheater tubes. Above the first melting temperature, the molten salt reacts with the protective oxide film that develops and dissolves it. The most protective oxide is determined by evaluating how little it dissolves and how its solubility changes in the molten salt. Solubility tests were done on several protective oxides in a known salt composition from a recovery boiler that burns hardwood derived fuel. ICP-OES was used to measure concentration of dissolved metal in the exposure tests while EDS and XRD were used to verify chemical compositions in exposure tests. NiO was found to be the least soluble oxide while Cr₂O₃ and Al₂O₃ had similar solubility with Fe₂O₃ being less soluble than Cr₂O₃ but more soluble than NiO. Exposure tests with pure metals and selected alloys indicated that even though Fe₂O₃ has little solubility, it is not a protective oxide and causes severe corrosion in stainless steels. The change in performance of iron based alloys was due to the development of a negative solubility gradient for Fe₂O₃ where Fe₂O₃ precipitated out of solution and created a continuous leaching of oxide. Manganese was found to be beneficial in stainless steels but its role is still unknown. Nickel based alloys were found to be least corroded due to nickel&#x27;s low solubility and because it did not form a negative solubility gradient.","abstract_has_math":false,"creators":["Meyer, Joseph Freeman"],"institution":"Georgia Institute of Technology","degree_name":null,"degree_level":null,"degree_discipline":null,"degree_department":"Materials Science and Engineering","school":null,"contributors":[],"advisors":["Singh, Preet M."],"committee_chairs":[],"committee_members":["Gokhale, Arun","Keiser, James"],"year":2013,"date_issued":"2013-04-15","date_published":"2013-04-15","updated_at":"2026-11-19T05:17:50Z","subjects":["SEM","Pulp and paper","ICP","XRD","EDS","Recovery boiler","Corrosion","Molten salt corrosion","Biomass stoves","Corrosion and anti-corrosives","Boilers Corrosion"],"languages":[],"rights":[],"rights_urls":[],"identifier_entries":[],"person_identifier_entries":[]},"links":{"outbound_url":"http://hdl.handle.net/1853/47742","outbound_label":"Handle","outbound_source":"dc:identifier.uri","record_url":"http://hdl.handle.net/1853/47742","record_label":"Repository record","record_kind":"handle","record_source":"dc:identifier.uri","download_url":null,"download_label":null,"download_source":null,"access_status":null,"embargo_until":null,"access_note":null},"source_record":{"url":"https://repository.gatech.edu/server/oai/request?verb=GetRecord&metadataPrefix=dim&identifier=oai%3Arepository.gatech.edu%3A1853%2F47742","prefix":"dim"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:contributor.advisor","label":"Advisor","values":["Singh, Preet M."]},{"key":"dc:contributor.committeemember","label":"Committee Member","values":["Gokhale, Arun","Keiser, James"]},{"key":"dc:contributor.department","label":"Department","values":["Materials Science and Engineering"]},{"key":"dc:contributor.other","label":"Dc Contributor Other","values":["School of Materials Science and Engineering","College of Engineering"]},{"key":"dc:creator","label":"Author","values":["Meyer, Joseph Freeman"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date.accessioned","label":"Dc Date Accessioned","values":["2013-06-15T02:59:32Z"]},{"key":"dc:date.available","label":"Dc Date Available","values":["2013-06-15T02:59:32Z"]},{"key":"dc:date.issued","label":"Date","values":["2013-04-15"]},{"key":"dc:publisher","label":"Institution","values":["Georgia Institute of Technology"]},{"key":"dc:relation.advisorentity","label":"Dc Relation Advisorentity","values":["436052a4-5726-4887-bdbf-e726647a6d26"]},{"key":"dc:relation.ispartofseries","label":"Dc Relation Ispartofseries","values":["Master of Science in Materials Science and Engineering"]},{"key":"dc:relation.orgunit","label":"Dc Relation Orgunit","values":["21b5a45b-0b8a-4b69-a36b-6556f8426a35","7c022d60-21d5-497c-b552-95e489a06569"]},{"key":"dc:relation.seriesentity","label":"Dc Relation Seriesentity","values":["68bad012-6751-4d30-ad95-62d356993b35"]},{"key":"dc:type","label":"Dc Type","values":["Text","Thesis"]}]},{"id":"subjects_keywords","label":"Subjects and Keywords","entries":[{"key":"dc:subject","label":"Dc Subject","values":["SEM","Pulp and paper","ICP","XRD","EDS","Recovery boiler","Corrosion","Molten salt corrosion"]},{"key":"dc:subject.lcsh","label":"Dc Subject Lcsh","values":["Biomass stoves","Corrosion and anti-corrosives","Boilers Corrosion"]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier.uri","label":"Identifier URI","values":["http://hdl.handle.net/1853/47742"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description.abstract","label":"Abstract","values":["The recovery boiler in a pulp and paper mill plays a dual role of recovering pulping chemicals and generating steam for either chemical processes or producing electricity. The efficiency of producing steam in the recovery boiler is limited by the first melting temperature of ash deposits that accumulate on the superheater tubes. Above the first melting temperature, the molten salt reacts with the protective oxide film that develops and dissolves it. The most protective oxide is determined by evaluating how little it dissolves and how its solubility changes in the molten salt. Solubility tests were done on several protective oxides in a known salt composition from a recovery boiler that burns hardwood derived fuel. ICP-OES was used to measure concentration of dissolved metal in the exposure tests while EDS and XRD were used to verify chemical compositions in exposure tests. NiO was found to be the least soluble oxide while Cr₂O₃ and Al₂O₃ had similar solubility with Fe₂O₃ being less soluble than Cr₂O₃ but more soluble than NiO. Exposure tests with pure metals and selected alloys indicated that even though Fe₂O₃ has little solubility, it is not a protective oxide and causes severe corrosion in stainless steels. The change in performance of iron based alloys was due to the development of a negative solubility gradient for Fe₂O₃ where Fe₂O₃ precipitated out of solution and created a continuous leaching of oxide. Manganese was found to be beneficial in stainless steels but its role is still unknown. Nickel based alloys were found to be least corroded due to nickel's low solubility and because it did not form a negative solubility gradient."]},{"key":"dc:description.degree","label":"Dc Description Degree","values":["MS"]},{"key":"dc:title","label":"Title","values":["Recovery boiler superheater corrosion - solubility of metal oxides in molten salt"]},{"key":"dspace:entity.type","label":"Dspace Entity Type","values":["Publication"]}]}],"canonical_facts":{"dc:contributor.advisor":["Singh, Preet M."],"dc:contributor.committeemember":["Gokhale, Arun","Keiser, James"],"dc:contributor.department":["Materials Science and Engineering"],"dc:contributor.other":["School of Materials Science and Engineering","College of Engineering"],"dc:creator":["Meyer, Joseph Freeman"],"dc:date.accessioned":["2013-06-15T02:59:32Z"],"dc:date.available":["2013-06-15T02:59:32Z"],"dc:date.issued":["2013-04-15"],"dc:description.abstract":["The recovery boiler in a pulp and paper mill plays a dual role of recovering pulping chemicals and generating steam for either chemical processes or producing electricity. The efficiency of producing steam in the recovery boiler is limited by the first melting temperature of ash deposits that accumulate on the superheater tubes. Above the first melting temperature, the molten salt reacts with the protective oxide film that develops and dissolves it. The most protective oxide is determined by evaluating how little it dissolves and how its solubility changes in the molten salt. Solubility tests were done on several protective oxides in a known salt composition from a recovery boiler that burns hardwood derived fuel. ICP-OES was used to measure concentration of dissolved metal in the exposure tests while EDS and XRD were used to verify chemical compositions in exposure tests. NiO was found to be the least soluble oxide while Cr₂O₃ and Al₂O₃ had similar solubility with Fe₂O₃ being less soluble than Cr₂O₃ but more soluble than NiO. Exposure tests with pure metals and selected alloys indicated that even though Fe₂O₃ has little solubility, it is not a protective oxide and causes severe corrosion in stainless steels. The change in performance of iron based alloys was due to the development of a negative solubility gradient for Fe₂O₃ where Fe₂O₃ precipitated out of solution and created a continuous leaching of oxide. Manganese was found to be beneficial in stainless steels but its role is still unknown. Nickel based alloys were found to be least corroded due to nickel's low solubility and because it did not form a negative solubility gradient."],"dc:description.degree":["MS"],"dc:identifier.uri":["http://hdl.handle.net/1853/47742"],"dc:publisher":["Georgia Institute of Technology"],"dc:relation.advisorentity":["436052a4-5726-4887-bdbf-e726647a6d26"],"dc:relation.ispartofseries":["Master of Science in Materials Science and Engineering"],"dc:relation.orgunit":["21b5a45b-0b8a-4b69-a36b-6556f8426a35","7c022d60-21d5-497c-b552-95e489a06569"],"dc:relation.seriesentity":["68bad012-6751-4d30-ad95-62d356993b35"],"dc:subject":["SEM","Pulp and paper","ICP","XRD","EDS","Recovery boiler","Corrosion","Molten salt corrosion"],"dc:subject.lcsh":["Biomass stoves","Corrosion and anti-corrosives","Boilers Corrosion"],"dc:title":["Recovery boiler superheater corrosion - solubility of metal oxides in molten salt"],"dc:type":["Text","Thesis"],"dspace:entity.type":["Publication"]},"updated_at":"2026-11-19T05:17:50Z"}