{"id":{"repo_id":"gatech","oai_identifier":"oai:repository.gatech.edu:1853/5114"},"canonical_url":"https://search.ndltd.org/etd/gatech/oai:repository.gatech.edu:1853/5114","repository":{"repo_id":"gatech","name":"Georgia Tech","base_url":"https://repository.gatech.edu/server/oai/request"},"display":{"title":"High Curie Temperature Bismuth- and Indium- Substituted Lead Titanate","abstract":"The extent of BiInO3 substitution in the perovskite system xBiInO3-(1-x)PbTiO3 and the corresponding raise in the Curie temperature were investigated using thermal analysis, X-ray diffraction and electron microscopy. Maximum tetragonal perovskite distortion (c/a = 1.082) was obtained for x=0.20, with a corresponding Curie temperature of 582C. Phase-pure tetragonal perovskite was obtained for x less than 0.25. Compound formation after calcining mixed oxide powders resulted in agglomerated cube-shaped tetragonal perovskite particles, which could be fired to 94.7% of theoretical density (TD) by crushing after calcining, dry pressing and firing. Sol-gel fabrication resulted in nano-sized tetragonal or pseudo-cubic perovskite particles, which after two-step firing, resulted in a tetragonal perovskite microstructure at as high as (x=0.25) 98.2% of TD.","abstract_html":"The extent of BiInO3 substitution in the perovskite system xBiInO3-(1-x)PbTiO3 and the corresponding raise in the Curie temperature were investigated using thermal analysis, X-ray diffraction and electron microscopy. Maximum tetragonal perovskite distortion (c/a = 1.082) was obtained for x=0.20, with a corresponding Curie temperature of 582C. Phase-pure tetragonal perovskite was obtained for x less than 0.25. Compound formation after calcining mixed oxide powders resulted in agglomerated cube-shaped tetragonal perovskite particles, which could be fired to 94.7% of theoretical density (TD) by crushing after calcining, dry pressing and firing. Sol-gel fabrication resulted in nano-sized tetragonal or pseudo-cubic perovskite particles, which after two-step firing, resulted in a tetragonal perovskite microstructure at as high as (x=0.25) 98.2% of TD.","abstract_has_math":false,"creators":["Duan, Runrun"],"institution":"Georgia Institute of Technology","degree_name":null,"degree_level":null,"degree_discipline":null,"degree_department":"Materials Science and Engineering","school":null,"contributors":[],"advisors":["Speyer, Robert F."],"committee_chairs":[],"committee_members":["Shrout, Thomas","Snyder, Robert"],"year":2004,"date_issued":"2004-06-10","date_published":"2004-06-10","updated_at":"2026-11-19T04:05:29Z","subjects":["Lead titanate Curie piezoelectrics"],"languages":["en_US"],"rights":[],"rights_urls":[],"identifier_entries":[],"person_identifier_entries":[]},"links":{"outbound_url":"http://hdl.handle.net/1853/5114","outbound_label":"Handle","outbound_source":"dc:identifier.uri","record_url":"http://hdl.handle.net/1853/5114","record_label":"Repository record","record_kind":"handle","record_source":"dc:identifier.uri","download_url":null,"download_label":null,"download_source":null,"access_status":null,"embargo_until":null,"access_note":null},"source_record":{"url":"https://repository.gatech.edu/server/oai/request?verb=GetRecord&metadataPrefix=dim&identifier=oai%3Arepository.gatech.edu%3A1853%2F5114","prefix":"dim"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:contributor.advisor","label":"Advisor","values":["Speyer, Robert F."]},{"key":"dc:contributor.committeemember","label":"Committee Member","values":["Shrout, Thomas","Snyder, Robert"]},{"key":"dc:contributor.department","label":"Department","values":["Materials Science and Engineering"]},{"key":"dc:contributor.other","label":"Dc Contributor Other","values":["School of Materials Science and Engineering","College of Engineering"]},{"key":"dc:creator","label":"Author","values":["Duan, Runrun"]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date.accessioned","label":"Dc Date Accessioned","values":["2005-03-03T17:39:03Z"]},{"key":"dc:date.available","label":"Dc Date Available","values":["2005-03-03T17:39:03Z"]},{"key":"dc:date.issued","label":"Date","values":["2004-06-10"]},{"key":"dc:publisher","label":"Institution","values":["Georgia Institute of Technology"]},{"key":"dc:relation.advisorentity","label":"Dc Relation Advisorentity","values":["ca7f4d7a-1308-47c2-8dd0-67775f5e3d5a"]},{"key":"dc:relation.orgunit","label":"Dc Relation Orgunit","values":["21b5a45b-0b8a-4b69-a36b-6556f8426a35","7c022d60-21d5-497c-b552-95e489a06569"]},{"key":"dc:type","label":"Dc Type","values":["Text","Thesis"]}]},{"id":"subjects_keywords","label":"Subjects and Keywords","entries":[{"key":"dc:subject","label":"Dc Subject","values":["Lead titanate Curie piezoelectrics"]}]},{"id":"language_rights","label":"Language and Rights","entries":[{"key":"dc:language.iso","label":"Language (ISO)","values":["en_US"]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier.uri","label":"Identifier URI","values":["http://hdl.handle.net/1853/5114"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description.abstract","label":"Abstract","values":["The extent of BiInO3 substitution in the perovskite system xBiInO3-(1-x)PbTiO3 and the corresponding raise in the Curie temperature were investigated using thermal analysis, X-ray diffraction and electron microscopy. Maximum tetragonal perovskite distortion (c/a = 1.082) was obtained for x=0.20, with a corresponding Curie temperature of 582C. Phase-pure tetragonal perovskite was obtained for x less than 0.25. Compound formation after calcining mixed oxide powders resulted in agglomerated cube-shaped tetragonal perovskite particles, which could be fired to 94.7% of theoretical density (TD) by crushing after calcining, dry pressing and firing. Sol-gel fabrication resulted in nano-sized tetragonal or pseudo-cubic perovskite particles, which after two-step firing, resulted in a tetragonal perovskite microstructure at as high as (x=0.25) 98.2% of TD."]},{"key":"dc:description.degree","label":"Dc Description Degree","values":["M.S."]},{"key":"dc:format.extent","label":"Dc Format Extent","values":["2712123 bytes"]},{"key":"dc:format.mimetype","label":"Dc Format Mimetype","values":["application/pdf"]},{"key":"dc:title","label":"Title","values":["High Curie Temperature Bismuth- and Indium- Substituted Lead Titanate"]},{"key":"dspace:entity.type","label":"Dspace Entity Type","values":["Publication"]}]}],"canonical_facts":{"dc:contributor.advisor":["Speyer, Robert F."],"dc:contributor.committeemember":["Shrout, Thomas","Snyder, Robert"],"dc:contributor.department":["Materials Science and Engineering"],"dc:contributor.other":["School of Materials Science and Engineering","College of Engineering"],"dc:creator":["Duan, Runrun"],"dc:date.accessioned":["2005-03-03T17:39:03Z"],"dc:date.available":["2005-03-03T17:39:03Z"],"dc:date.issued":["2004-06-10"],"dc:description.abstract":["The extent of BiInO3 substitution in the perovskite system xBiInO3-(1-x)PbTiO3 and the corresponding raise in the Curie temperature were investigated using thermal analysis, X-ray diffraction and electron microscopy. Maximum tetragonal perovskite distortion (c/a = 1.082) was obtained for x=0.20, with a corresponding Curie temperature of 582C. Phase-pure tetragonal perovskite was obtained for x less than 0.25. Compound formation after calcining mixed oxide powders resulted in agglomerated cube-shaped tetragonal perovskite particles, which could be fired to 94.7% of theoretical density (TD) by crushing after calcining, dry pressing and firing. Sol-gel fabrication resulted in nano-sized tetragonal or pseudo-cubic perovskite particles, which after two-step firing, resulted in a tetragonal perovskite microstructure at as high as (x=0.25) 98.2% of TD."],"dc:description.degree":["M.S."],"dc:format.extent":["2712123 bytes"],"dc:format.mimetype":["application/pdf"],"dc:identifier.uri":["http://hdl.handle.net/1853/5114"],"dc:language.iso":["en_US"],"dc:publisher":["Georgia Institute of Technology"],"dc:relation.advisorentity":["ca7f4d7a-1308-47c2-8dd0-67775f5e3d5a"],"dc:relation.orgunit":["21b5a45b-0b8a-4b69-a36b-6556f8426a35","7c022d60-21d5-497c-b552-95e489a06569"],"dc:subject":["Lead titanate Curie piezoelectrics"],"dc:title":["High Curie Temperature Bismuth- and Indium- Substituted Lead Titanate"],"dc:type":["Text","Thesis"],"dspace:entity.type":["Publication"]},"updated_at":"2026-11-19T04:05:29Z"}