{"id":{"repo_id":"gatech","oai_identifier":"oai:repository.gatech.edu:1853/52225"},"canonical_url":"https://search.ndltd.org/etd/gatech/oai:repository.gatech.edu:1853/52225","repository":{"repo_id":"gatech","name":"Georgia Tech","base_url":"https://repository.gatech.edu/server/oai/request"},"display":{"title":"On-chip dielectric cohesive fracture characterization and mitigation investigation through off-chip carbon nanotube interconnects","abstract":"The cohesive fracture of thin films is a concern for the reliability of many devices in microelectronics, MEMS, photovoltaics, and other applications. In microelectronic packaging the cohesive fracture toughness has become a concern with new low-k dielectric materials currently being used. To obtain the low-k values needed to meet electrical performance goals, the mechanical strength of the material has decreased. This has resulted in cohesive cracks occurring in the Back End of Line (BEoL) dielectric layers of the microelectronic packages. These cracks lead to electronic failures and occur after thermal loading (due to CTE mismatch of materials) and mechanical loading. To prevent these cohesive cracks, it is necessary to measure the cohesive fracture resistance of these thin films to implement during the design and analysis process. Many of the current tests to measure the cohesive fracture resistance of thin films are based on methods developed for larger scale specimens. These methods can be difficult to apply to thin films due to their size and require mechanical fixturing, physical contact near the crack tip, and complicated stress fields. Therefore, a fixtureless cohesive fracture resistance measurement technique has been developed that utilizes photolithography fabrication processes. This technique uses a superlayer thin film with a high intrinsic stress deposited on top of the desired test material to drive cohesive fracture through the thickness of test material. In addition to developing a technique to measure the fracture resistance of dielectric thin films, the use of carbon nanotube (CNT) forests as off-chip interconnects is investigated as a potential method to mitigate the fracture of these materials. The compressive and tensile modulus of CNT forests is characterized, and it is seen that the modulus is several orders of magnitude less than that of a single straight CNT. The low-modulus CNT forest will help mechanically decouple the chip from the board and reduce stress occurring in the dielectric layers as compared to the current technology of solder ball interconnects and therefore improve reliability. The mechanical performance of these CNT interconnects is investigated by creating a finite-element model of a flip chip electronic package utilizing CNT interconnects and comparing the chip stresses to a traditional solder ball interconnect scenario. Additionally, flip chips are fabricated with CNT forest interconnects, assembled to an FR4 substrate, and subjected to accelerated thermomechanical testing to experimentally investigate their performance.","abstract_html":"The cohesive fracture of thin films is a concern for the reliability of many devices in microelectronics, MEMS, photovoltaics, and other applications. In microelectronic packaging the cohesive fracture toughness has become a concern with new low-k dielectric materials currently being used. To obtain the low-k values needed to meet electrical performance goals, the mechanical strength of the material has decreased. This has resulted in cohesive cracks occurring in the Back End of Line (BEoL) dielectric layers of the microelectronic packages. These cracks lead to electronic failures and occur after thermal loading (due to CTE mismatch of materials) and mechanical loading. To prevent these cohesive cracks, it is necessary to measure the cohesive fracture resistance of these thin films to implement during the design and analysis process. Many of the current tests to measure the cohesive fracture resistance of thin films are based on methods developed for larger scale specimens. These methods can be difficult to apply to thin films due to their size and require mechanical fixturing, physical contact near the crack tip, and complicated stress fields. Therefore, a fixtureless cohesive fracture resistance measurement technique has been developed that utilizes photolithography fabrication processes. This technique uses a superlayer thin film with a high intrinsic stress deposited on top of the desired test material to drive cohesive fracture through the thickness of test material. In addition to developing a technique to measure the fracture resistance of dielectric thin films, the use of carbon nanotube (CNT) forests as off-chip interconnects is investigated as a potential method to mitigate the fracture of these materials. The compressive and tensile modulus of CNT forests is characterized, and it is seen that the modulus is several orders of magnitude less than that of a single straight CNT. The low-modulus CNT forest will help mechanically decouple the chip from the board and reduce stress occurring in the dielectric layers as compared to the current technology of solder ball interconnects and therefore improve reliability. The mechanical performance of these CNT interconnects is investigated by creating a finite-element model of a flip chip electronic package utilizing CNT interconnects and comparing the chip stresses to a traditional solder ball interconnect scenario. Additionally, flip chips are fabricated with CNT forest interconnects, assembled to an FR4 substrate, and subjected to accelerated thermomechanical testing to experimentally investigate their performance.","abstract_has_math":false,"creators":["Ginga, Nicholas J."],"institution":"Georgia Institute of Technology","degree_name":null,"degree_level":"Doctoral","degree_discipline":null,"degree_department":"Mechanical Engineering","school":null,"contributors":[],"advisors":["Sitaraman, Suresh K."],"committee_chairs":[],"committee_members":["Kalaitzidou, Kyriaki","Neu, Richard W.","Ready, W. Jud","Wang, Zhong Lin"],"year":2014,"date_issued":"2014-05-13","date_published":"2014-05-13","updated_at":"2026-11-19T05:57:00Z","subjects":["Thin film","MEMs","CNT","Fracture","Photolithography","Material characterization","Modulus","Carbon nanotubes","Microelectronics","Reliability","Finite element analysis","Interconnects"],"languages":["en_US"],"rights":[],"rights_urls":[],"identifier_entries":[],"person_identifier_entries":[]},"links":{"outbound_url":"http://hdl.handle.net/1853/52225","outbound_label":"Handle","outbound_source":"dc:identifier.uri","record_url":"http://hdl.handle.net/1853/52225","record_label":"Repository record","record_kind":"handle","record_source":"dc:identifier.uri","download_url":null,"download_label":null,"download_source":null,"access_status":null,"embargo_until":null,"access_note":null},"source_record":{"url":"https://repository.gatech.edu/server/oai/request?verb=GetRecord&metadataPrefix=dim&identifier=oai%3Arepository.gatech.edu%3A1853%2F52225","prefix":"dim"},"metadata_groups":[{"id":"people","label":"People","entries":[{"key":"dc:contributor.advisor","label":"Advisor","values":["Sitaraman, Suresh K."]},{"key":"dc:contributor.committeemember","label":"Committee Member","values":["Kalaitzidou, Kyriaki","Neu, Richard W.","Ready, W. Jud","Wang, Zhong Lin"]},{"key":"dc:contributor.department","label":"Department","values":["Mechanical Engineering"]},{"key":"dc:contributor.other","label":"Dc Contributor Other","values":["George W. Woodruff School of Mechanical Engineering","College of Engineering"]},{"key":"dc:creator","label":"Author","values":["Ginga, Nicholas J."]}]},{"id":"academic_context","label":"Academic Context","entries":[{"key":"dc:date.accessioned","label":"Dc Date Accessioned","values":["2014-08-27T13:37:00Z"]},{"key":"dc:date.available","label":"Dc Date Available","values":["2014-08-27T13:37:00Z"]},{"key":"dc:date.created","label":"Dc Date Created","values":["2014-08"]},{"key":"dc:date.issued","label":"Date","values":["2014-05-13"]},{"key":"dc:date.submitted","label":"Dc Date Submitted","values":["August 2014"]},{"key":"dc:date.updated","label":"Dc Date Updated","values":["2014-08-27T13:37:00Z"]},{"key":"dc:publisher","label":"Institution","values":["Georgia Institute of Technology"]},{"key":"dc:relation.advisorentity","label":"Dc Relation Advisorentity","values":["86701d63-9ca5-4060-89f8-aca6e0b267f6"]},{"key":"dc:relation.orgunit","label":"Dc Relation Orgunit","values":["c01ff908-c25f-439b-bf10-a074ed886bb7","7c022d60-21d5-497c-b552-95e489a06569"]},{"key":"dc:type","label":"Dc Type","values":["Text","Dissertation"]},{"key":"thesis:degree_level","label":"Degree Level","values":["Doctoral"]}]},{"id":"subjects_keywords","label":"Subjects and Keywords","entries":[{"key":"dc:subject","label":"Dc Subject","values":["Thin film","MEMs","CNT","Fracture","Photolithography","Material characterization","Modulus","Carbon nanotubes","Microelectronics","Reliability","Finite element analysis","Interconnects"]}]},{"id":"language_rights","label":"Language and Rights","entries":[{"key":"dc:language.iso","label":"Language (ISO)","values":["en_US"]}]},{"id":"identifiers","label":"Identifiers","entries":[{"key":"dc:identifier.uri","label":"Identifier URI","values":["http://hdl.handle.net/1853/52225"]}]},{"id":"additional","label":"Additional Metadata","entries":[{"key":"dc:description.abstract","label":"Abstract","values":["The cohesive fracture of thin films is a concern for the reliability of many devices in microelectronics, MEMS, photovoltaics, and other applications. In microelectronic packaging the cohesive fracture toughness has become a concern with new low-k dielectric materials currently being used. To obtain the low-k values needed to meet electrical performance goals, the mechanical strength of the material has decreased. This has resulted in cohesive cracks occurring in the Back End of Line (BEoL) dielectric layers of the microelectronic packages. These cracks lead to electronic failures and occur after thermal loading (due to CTE mismatch of materials) and mechanical loading. To prevent these cohesive cracks, it is necessary to measure the cohesive fracture resistance of these thin films to implement during the design and analysis process. Many of the current tests to measure the cohesive fracture resistance of thin films are based on methods developed for larger scale specimens. These methods can be difficult to apply to thin films due to their size and require mechanical fixturing, physical contact near the crack tip, and complicated stress fields. Therefore, a fixtureless cohesive fracture resistance measurement technique has been developed that utilizes photolithography fabrication processes. This technique uses a superlayer thin film with a high intrinsic stress deposited on top of the desired test material to drive cohesive fracture through the thickness of test material. In addition to developing a technique to measure the fracture resistance of dielectric thin films, the use of carbon nanotube (CNT) forests as off-chip interconnects is investigated as a potential method to mitigate the fracture of these materials. The compressive and tensile modulus of CNT forests is characterized, and it is seen that the modulus is several orders of magnitude less than that of a single straight CNT. The low-modulus CNT forest will help mechanically decouple the chip from the board and reduce stress occurring in the dielectric layers as compared to the current technology of solder ball interconnects and therefore improve reliability. The mechanical performance of these CNT interconnects is investigated by creating a finite-element model of a flip chip electronic package utilizing CNT interconnects and comparing the chip stresses to a traditional solder ball interconnect scenario. Additionally, flip chips are fabricated with CNT forest interconnects, assembled to an FR4 substrate, and subjected to accelerated thermomechanical testing to experimentally investigate their performance."]},{"key":"dc:description.degree","label":"Dc Description Degree","values":["Ph.D."]},{"key":"dc:format.mimetype","label":"Dc Format Mimetype","values":["application/pdf"]},{"key":"dc:title","label":"Title","values":["On-chip dielectric cohesive fracture characterization and mitigation investigation through off-chip carbon nanotube interconnects"]},{"key":"dspace:entity.type","label":"Dspace Entity Type","values":["Publication"]}]}],"canonical_facts":{"dc:contributor.advisor":["Sitaraman, Suresh K."],"dc:contributor.committeemember":["Kalaitzidou, Kyriaki","Neu, Richard W.","Ready, W. Jud","Wang, Zhong Lin"],"dc:contributor.department":["Mechanical Engineering"],"dc:contributor.other":["George W. Woodruff School of Mechanical Engineering","College of Engineering"],"dc:creator":["Ginga, Nicholas J."],"dc:date.accessioned":["2014-08-27T13:37:00Z"],"dc:date.available":["2014-08-27T13:37:00Z"],"dc:date.created":["2014-08"],"dc:date.issued":["2014-05-13"],"dc:date.submitted":["August 2014"],"dc:date.updated":["2014-08-27T13:37:00Z"],"dc:description.abstract":["The cohesive fracture of thin films is a concern for the reliability of many devices in microelectronics, MEMS, photovoltaics, and other applications. In microelectronic packaging the cohesive fracture toughness has become a concern with new low-k dielectric materials currently being used. To obtain the low-k values needed to meet electrical performance goals, the mechanical strength of the material has decreased. This has resulted in cohesive cracks occurring in the Back End of Line (BEoL) dielectric layers of the microelectronic packages. These cracks lead to electronic failures and occur after thermal loading (due to CTE mismatch of materials) and mechanical loading. To prevent these cohesive cracks, it is necessary to measure the cohesive fracture resistance of these thin films to implement during the design and analysis process. Many of the current tests to measure the cohesive fracture resistance of thin films are based on methods developed for larger scale specimens. These methods can be difficult to apply to thin films due to their size and require mechanical fixturing, physical contact near the crack tip, and complicated stress fields. Therefore, a fixtureless cohesive fracture resistance measurement technique has been developed that utilizes photolithography fabrication processes. This technique uses a superlayer thin film with a high intrinsic stress deposited on top of the desired test material to drive cohesive fracture through the thickness of test material. In addition to developing a technique to measure the fracture resistance of dielectric thin films, the use of carbon nanotube (CNT) forests as off-chip interconnects is investigated as a potential method to mitigate the fracture of these materials. The compressive and tensile modulus of CNT forests is characterized, and it is seen that the modulus is several orders of magnitude less than that of a single straight CNT. The low-modulus CNT forest will help mechanically decouple the chip from the board and reduce stress occurring in the dielectric layers as compared to the current technology of solder ball interconnects and therefore improve reliability. The mechanical performance of these CNT interconnects is investigated by creating a finite-element model of a flip chip electronic package utilizing CNT interconnects and comparing the chip stresses to a traditional solder ball interconnect scenario. Additionally, flip chips are fabricated with CNT forest interconnects, assembled to an FR4 substrate, and subjected to accelerated thermomechanical testing to experimentally investigate their performance."],"dc:description.degree":["Ph.D."],"dc:format.mimetype":["application/pdf"],"dc:identifier.uri":["http://hdl.handle.net/1853/52225"],"dc:language.iso":["en_US"],"dc:publisher":["Georgia Institute of Technology"],"dc:relation.advisorentity":["86701d63-9ca5-4060-89f8-aca6e0b267f6"],"dc:relation.orgunit":["c01ff908-c25f-439b-bf10-a074ed886bb7","7c022d60-21d5-497c-b552-95e489a06569"],"dc:subject":["Thin film","MEMs","CNT","Fracture","Photolithography","Material characterization","Modulus","Carbon nanotubes","Microelectronics","Reliability","Finite element analysis","Interconnects"],"dc:title":["On-chip dielectric cohesive fracture characterization and mitigation investigation through off-chip carbon nanotube interconnects"],"dc:type":["Text","Dissertation"],"dspace:entity.type":["Publication"],"thesis:degree_level":["Doctoral"]},"updated_at":"2026-11-19T05:57:00Z"}